Patent number: 4239645
Abstract: A phosphate base laser glass comprising 55-70% P.sub.2 O.sub.5, 1-15% Al.sub.2 O.sub.3, 0-25% Li.sub.2 O, 0-25% Na.sub.2 O, 0-8% K.sub.2 O, the total proportion of Li.sub.2 O, Na.sub.2 O, and K.sub.2 O being 10-25%, 0-15% BaO, 0-15% ZnO, 0-15% CaO, 0-15%, SrO, 0-15% MgO, the total proportion of BaO, ZnO, CaO, SrO, and MgO being 5-15%, 0-5% Y.sub.2 O.sub.3, 0-5% La.sub.2 O.sub.3, 0-5% GeO.sub.2, 0-5% CeO.sub.2, 0-3% Nb.sub.2 O.sub.5, 0-3% MnO.sub.2, 0-2% Ta.sub.2 O.sub.5, 0-1% Sb.sub.2 O.sub.3, and 0.01-5% Nd.sub.2 O.sub.3, all % being mole %.The phosphate base laser glass of this invention has a high induced emission cross section, a low non-linear refractive index coefficient, and excellent acid resistance and divitrification resistance. By replacing partially or wholely one or more of LiO.sub.2, Na.sub.2 O, K.sub.2 O, BaO, ZnO, CaO, SrO, MgO or Al.sub.2 O.sub.3 by LiF, NaF, KF, BaF.sub.2 ZnF.sub.2, CaF.sub.2, SrF.sub.2, MgF.sub.2 or AlF.sub.
Type:
Grant
Filed:
March 17, 1976
Date of Patent:
December 16, 1980
Assignee:
Hoya Glass Works, Ltd.
Inventors:
Tetsuro Izumitani, Michitaka Tsuru