Patents by Inventor Mikie Kanai

Mikie Kanai has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 7407902
    Abstract: A Bismuth glass composition including 0.5 to 14 wt % of SiO2, 3 to 15 wt % of B2O3, 4 to 22 wt % of ZnO, 55 to 90 wt % of Bi2O3 and 4 wt % or less of Al2O3, and further including 5 wt % or less of an oxide of Group A, 12 wt % or less of an oxide of Group B and 0.1 to 10 wt % of an oxide of Group C, wherein the oxide of Group A is at least one selected from the group consisting of Li2O, Na2O and K2O, the oxide of Group B is at least one selected from the group consisting of MgO, CaO, SrO and BaO, and the oxide of Group C is at least one selected from the group consisting of Sc2O3, Y2O3, La2O3, CeO2, Pr2O3, Nd2O3, Sm2O3, Eu2O3, Gd2O3, Tb2O3, Dy2O3, Ho2O3, Er2O3, Tm2O3, Yb2O3 and Lu2O3.
    Type: Grant
    Filed: March 28, 2003
    Date of Patent: August 5, 2008
    Assignee: Matsushita Electric Industrial Co., Ltd.
    Inventors: Shinya Hasegawa, Hiroshi Onishi, Mikie Kanai, Tetsuya Kamimoto
  • Patent number: 7012783
    Abstract: A magnetic head for a magnetic recording/reproducing device to conform to high-density recording, wherein a metal magnetic film with a high saturation flux density is employed and the mechanical strength of the sealing glass for magnetic heads, is improved thereby achieving a high reliability, high performance magnetic head. Also, this is provided a magnetic recording/reproducing device utilizing the magnetic head. Sealing glass for magnetic heads comprising, by oxide conversion, 17.2 to 25 wt % of SiO2, 1 to 10 wt % of B2O3, 58 to 75 wt % of PbO, 0.2 to 7 wt % of at least one of Al2O3 and ZnO, and 0.2 to 5 wt % of at least one of Na2O and K2O, and a magnetic head and magnetic recording/reproducing device which utilize the sealing glass.
    Type: Grant
    Filed: March 5, 2002
    Date of Patent: March 14, 2006
    Inventors: Shinya Hasegawa, Mikie Kanai, Tetsuya Kamimoto, Hideo Torii
  • Publication number: 20050181927
    Abstract: A Bismuth glass composition including 0.5 to 14 wt % of SiO2, 3 to 15 wt % of B2O3, 4 to 22 wt % of ZnO, 55 to 90 wt % of Bi2O3 and 4 wt % or less of Al2O3, and further including 5 wt % or less of an oxide of Group A, 12 wt % or less of an oxide of Group B and 0.1 to 10 wt % of an oxide of Group C, wherein the oxide of Group A is at least one selected from the group consisting of Li2O, Na2O and K2O, the oxide of Group B is at least one selected from the group consisting of MgO, CaO, SrO and BaO, and the oxide of Group C is at least one selected from the group consisting of Sc2O3, Y2O3, La2O3, CeO2, Pr2O3, Nd2O3, Sm2O3, Eu2O3, Gd2O3, Tb2O3, Dy2O3, Ho2O3, Er2O3, Tm2O3, Yb2O3 and Lu2O3.
    Type: Application
    Filed: March 28, 2003
    Publication date: August 18, 2005
    Applicant: Matsushita Electric Industrial Co., Ltd
    Inventors: Shinya Hasegawa, Hiroshi Onishi, Mikie Kanai, Tetsuya Kamimoto
  • Patent number: 6778355
    Abstract: In order to provide a practically lead-free glass composition having a low softening point and an excellent water resistance for use in various parts of electronic equipment and a magnetic head using the same, a glass composition is provided, which contains 0.5 to 14 wt % of SiO2, 3 to 15 wt % of B2O3, 4 to 22 wt % of ZnO, 55 to 90 wt % of Bi2O3, 0 to 4 wt % of Al2O3, 0 to 5 wt % of at least one selected from the group consisting of Li2O, Na2O and K2O, and 0 to 15 wt % of at least one selected from the group consisting of MgO, CaO, SrO and BaO.
    Type: Grant
    Filed: January 8, 2002
    Date of Patent: August 17, 2004
    Assignee: Matsushita Electric Industrial Co., Ltd.
    Inventors: Shinya Hasegawa, Mikie Kanai, Hideo Torii, Tetsuya Kamimoto
  • Publication number: 20040012883
    Abstract: To provide a magnetic head for a magnetic recording/reproducing device to conform to high-density recording, wherein a metal magnetic film with a high saturation flux density is employed and the mechanical strength of the sealing glass for magnetic heads, is improved thereby achieving a high reliability, high performance magnetic head, also to provide a magnetic recording/reproducing device utilizing the magnetic head.
    Type: Application
    Filed: July 15, 2003
    Publication date: January 22, 2004
    Inventors: Shinya Hasegawa, Mikie Kanai, Tetsuya Kamimoto, Hideo Torii
  • Publication number: 20030048580
    Abstract: In order to provide a practically lead-free glass composition having a low softening point and an excellent water resistance for use in various parts of electronic equipment and a magnetic head using the same, a glass composition is provided, which contains 0.5 to 14 wt % of SiO2, 3 to 15 wt % of B2O3, 4 to 22 wt % of ZnO, 55 to 90 wt % of Bi2O3, 0 to 4 wt % of Al2O3, 0 to 5 wt % of at least one selected from the group consisting of Li2O, Na2O and K2O, and 0 to 15 wt % of at least one selected from the group consisting of MgO, CaO, SrO and BaO.
    Type: Application
    Filed: January 8, 2002
    Publication date: March 13, 2003
    Inventors: Shinya Hasegawa, Mikie Kanai, Hideo Torii, Tetsuya Kamimoto