  • Publication number: 20230250268
    Abstract: An elastomeric composition suitable for use in layered articles like hoses and belts may include: 5 phr to 80 phr of a PEDM terpolymer comprising 55 wt % to 95 wt % propylene, 2.5 wt % to 40 wt % ?-olefin, and 0.05 wt % to 25 wt % diene and having Mooney viscosity (ML(1+4)) of 5 MU to 90 MU; 20 phr to 95 phr of an ethylene-based copolymer selected from: (a) a crystalline ethylene-based copolymer comprising 60 wt % to 95 wt % ethylene, 0 wt % to 10 wt % of one or more dienes, and 5 wt % to 40 wt % C3 to C12 ?-olefin, (b) an amorphous ethylene-based comprising 40 wt % to 59 wt % ethylene, 0 wt % to 10 wt % of one or more dienes, and 40 wt % to 60 wt % C3 to C12 ?-olefin, and (c) a combination of (a) and (b); and 10 phr to 200 phr of a process oil.
    Type: Application
    Filed: July 16, 2021
    Publication date: August 10, 2023
    Inventors: Scott H. Loyd, Milind Balwant Joshi, Xiao Bo Peng, Felix Manuel Zacarias, Narayanaswami Dharmarajan, Rainer Kolb, David William Abmayr, Zhifeng Bai
  • Patent number: 11390734
    Abstract: Disclosed herein is a composition comprising from 5 to 20 parts by weight per hundred parts by weight rubber (phr) of a propylene-?-olefin-diene (PEDM) terpolymer comprising 1 to 10 wt % diene, 5 to 40 wt % ?-olefin, and 15 to 85 wt % propylene, said wt % based on the weight of the PEDM terpolymer; and from 80 to 95 phr of an ethylene-based copolymer comprising ethylene, one or more C3 to C12 ?-olefins, and, optionally, one or more dienes; wherein the amount of ethylene content of the ethylene-based copolymer (in wt % on the basis of total weight of the ethylene-based copolymer) is greater than the amount of ?-olefin content of the PEDM terpolymer (in wt % on the basis of total weight of the PEDM terpolymer).
    Type: Grant
    Filed: November 5, 2018
    Date of Patent: July 19, 2022
    Assignee: ExxonMobil Chemical Patents Inc.
    Inventors: Narayanaswami Dharmarajan, Scott H. Loyd, Milind Balwant Joshi
  • Publication number: 20210371634
    Abstract: Disclosed herein is a composition comprising from 5 to 20 parts by weight per hundred parts by weight rubber (phr) of a propylene-?-olefin-diene (PEDM) terpolymer comprising 1 to 10 wt % diene, 5 to 40 wt % ?-olefin, and 15 to 85 wt % propylene, said wt % based on the weight of the PEDM terpolymer; and from 80 to 95 phr of an ethylene-based copolymer comprising ethylene, one or more C3 to C12 ?-olefins, and, optionally, one or more dienes; wherein the amount of ethylene content of the ethylene-based copolymer (in wt % on the basis of total weight of the ethylene-based copolymer) is greater than the amount of ?-olefin content of the PEDM terpolymer (in wt % on the basis of total weight of the PEDM terpolymer).
    Type: Application
    Filed: November 5, 2018
    Publication date: December 2, 2021
    Inventors: Narayanaswami Dharmarajan, Scott H. Loyd, Milind Balwant Joshi
  • Patent number: 8609760
    Abstract: Natural rubber blends, methods for making the same, and articles made therefrom are provided. The natural rubber blend includes at least one propylene copolymer containing ethylene derived units. The natural rubber blend can further include one or more reinforcing fillers, such as carbon black. The presence of the propylene copolymer significantly improves the ozone resistance and ageing properties of the natural rubber gum stock.
    Type: Grant
    Filed: November 18, 2009
    Date of Patent: December 17, 2013
    Assignee: ExxonMobil Chemical Patents Inc.
    Inventors: Hyun-Dae Jung, Khee Sio Yeo, Milind Balwant Joshi, Pradeep Pandurang Patki, Bharat Bhushan Sharma, Manjunatha Hanumanthappa
  • Publication number: 20110118404
    Abstract: Natural rubber blends, methods for making the same, and articles made therefrom are provided. The natural rubber blend includes at least one propylene copolymer containing ethylene derived units. The natural rubber blend can further include one or more reinforcing fillers, such as carbon black. The presence of the propylene copolymer significantly improves the ozone resistance and ageing properties of the natural rubber gum stock.
    Type: Application
    Filed: November 18, 2009
    Publication date: May 19, 2011
    Inventors: Hyun-Dae Jung, Khee Sio Yeo, Milind Balwant Joshi, Pradeep Pandurang Patki, Bharat Bhushan Sharma, Manjunatha Hanumanthappa