Patents by Inventor Myoung Ruoul Lee

Myoung Ruoul Lee has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Publication number: 20140039149
    Abstract: The present invention relates to a copolymer polyester resin and a molded product using the same, and more specifically to a copolymer polyester resin that contains 10˜80 mol % of 1,4-cyclohexane dimethanol, 0.1˜50 mol % of a diol compound expressed as HO—(CH2)n—CO—(CH2)b—OH (where a and b are integers in the range 1˜5), and ethylene glycol or other diols so that the sum of its entire diol composition is 100 mol % based on dicarboxylic acid. The copolymer polyester resin of the present invention enables reduction of cycle time, improvement of product processability and prevention of PET bottle deformation during mold processing with a heat-shrinking label by complementing low temperature shrinkage, maintaining a high shrinkage rate, and reducing shrinkage stress.
    Type: Application
    Filed: October 11, 2013
    Publication date: February 6, 2014
    Applicant: SK CHEMICALS CO., LTD.
    Inventors: Myoung Ruoul Lee, Jong Ryang Kim
  • Publication number: 20140018497
    Abstract: The present invention relates to a copolymer polyester resin and a molded product using the same and more specifically to a copolymer polyester resin that contains 10˜80 mol % of 1,4-cyclohexane dimethanol, 0.1˜30 mol % of a cyclohexane dimethanol compound expressed as HOH2C—[C6H12]m—[C6H12]—CH2OH (where m is an integer from 1˜10), and ethylene glycol as the remainder so that the sum of the entire diol composition may be 100 mol % based on an aromatic dicarboxylic acid. The copolymer polyester of the present invention enables superior products to be provided that reduce cycle time and enhance product processability during mold processing using a heat-shrinking label by complementing low temperature shrinkage properties that may be exhibited by the polyester resin of the prior art copolymerized with 1,4-cyclohexane dimethanol.
    Type: Application
    Filed: September 19, 2013
    Publication date: January 16, 2014
    Applicant: SK Chemicals Co., Ltd.
    Inventors: Myoung Ruoul Lee, Jong Ryang Kim, Nam Jung Kim
  • Patent number: 8580898
    Abstract: The present invention relates to a copolymer polyester resin and a molded product using the same, and more specifically to a copolymer polyester resin that contains 10˜80 mol % of 1,4-cyclohexane dimethanol, 0.1˜50 mol % of a diol compound expressed as HO—(CH2)a—CO—(CH2)b—OH (where a and b are integers in the range 1˜5), and ethylene glycol or other diols so that the sum of its entire diol composition is 100 mol % based on dicarboxylic acid. The copolymer polyester resin of the present invention enables reduction of cycle time, improvement of product processability and prevention of PET bottle deformation during mold processing with a heat-shrinking label by complementing low temperature shrinkage, maintaining a high shrinkage rate, and reducing shrinkage stress.
    Type: Grant
    Filed: November 20, 2009
    Date of Patent: November 12, 2013
    Assignee: SK Chemicals Co., Ltd.
    Inventors: Myoung Ruoul Lee, Jong Ryang Kim
  • Patent number: 8557951
    Abstract: The present invention relates to a copolymer polyester resin and a molded product using the same and more specifically to a copolymer polyester resin that contains 10˜80 mol % of 1,4-cyclohexane dimethanol, 0.1˜30 mol % of a cyclohexane dimethanol compound expressed as HOH2C—[C6H12]m—[C6H12]—CH2OH (where m is an integer from 1˜10), and ethylene glycol as the remainder so that the sum of the entire diol composition may be 100 mol % based on an aromatic dicarboxylic acid. The copolymer polyester of the present invention enables superior products to be provided that reduce cycle time and enhance product processability during mold processing using a heat-shrinking label by complementing low temperature shrinkage properties that may be exhibited by the polyester resin of the prior art copolymerized with 1,4-cyclohexane dimethanol.
    Type: Grant
    Filed: November 20, 2009
    Date of Patent: October 15, 2013
    Assignee: SK Chemicals Co., Ltd.
    Inventors: Myoung Ruoul Lee, Jong Ryang Kim, Nam Jung Kim
  • Publication number: 20110230634
    Abstract: The present invention relates to a copolymer polyester resin and a molded product using the same and more specifically to a copolymer polyester resin that contains 10˜80 mol % of 1,4-cyclohexane dimethanol, 0.1˜30 mol % of a cyclohexane dimethanol compound expressed as HOH2C—[C6H12]m—[C6H12]—CH2OH (where m is an integer from 1˜10), and ethylene glycol as the remainder so that the sum of the entire diol composition may be 100 mol % based on an aromatic dicarboxylic acid. The copolymer polyester of the present invention enables superior products to be provided that reduce cycle time and enhance product processability during mold processing using a heat-shrinking label by complementing low temperature shrinkage properties that may be exhibited by the polyester resin of the prior art copolymerized with 1,4-cyclohexane dimethanol.
    Type: Application
    Filed: November 20, 2009
    Publication date: September 22, 2011
    Applicant: SK Chemicals Co., Ltd.
    Inventors: Myoung Ruoul Lee, Jong Ryang Kim, Nam Jung Kim
  • Publication number: 20110230635
    Abstract: The present invention relates to a copolymer polyester resin and a molded product using the same and more specifically to a copolymer polyester resin that contains 10˜80 mol % of 1,4-cyclohexane dimethanol, 0.1˜50 mol % of a diol compound expressed as HO—R6CR7—R4R1R5—COHR2R3 (where R1 is an alkyl group with a carbon number of 0˜10, and R2˜R7 are hydrogen or an alkyl group with a carbon number of 1˜10), and ethylene glycol as the remainder so that the sum of the entire diol composition is 100 mol % based on aromatic dicarboxylic acid. The copolymer polyester resin of the present invention enables reduction of cycle time and improvement of product processability and prevention of PET bottle deformation during mold processing with a heat-shrinking label by complementing low temperature shrinkage, maintaining a high shrinkage rate, and reducing shrinkage stress.
    Type: Application
    Filed: November 20, 2009
    Publication date: September 22, 2011
    Applicant: SK CHEMICALS CO., LTD.
    Inventors: Myoung Ruoul Lee, Jong Ryang Kim
  • Publication number: 20110224400
    Abstract: The present invention relates to a copolymer polyester resin and a molded product using the same, and more specifically to a copolymer polyester resin that contains 10˜80 mol % of 1,4-cyclohexane dimethanol, 0.1˜50 mol % of a diol compound expressed as HO—(CH2)a—CO—(CH2)b—OH (where a and b are integers in the range 1˜5), and ethylene glycol or other diols so that the sum of its entire diol composition is 100 mol % based on dicarboxylic acid. The copolymer polyester resin of the present invention enables reduction of cycle time, improvement of product processability and prevention of PET bottle deformation during mold processing with a heat-shrinking label by complementing low temperature shrinkage, maintaining a high shrinkage rate, and reducing shrinkage stress.
    Type: Application
    Filed: November 20, 2009
    Publication date: September 15, 2011
    Applicant: SK CHEMICALS CO., LTD.
    Inventors: Myoung Ruoul Lee, Jong Ryang Kim