  • Patent number: 10669391
    Abstract: The compressible sealing element (1) comprises at least one piece made of a resilient foam (17). This foam has an open-cell content of at least 50% and has such a hardness that it requires a force of less than 2000 N to compress the sealing element (1) per meter length thereof to such an extent that the volume of a rectangular cuboid circumscribing the sealing element is reduced by 40%. The sealing element comprises a water-impermeable cover layer (18) which extends at least over its top surface. The sealing element is intended for filling at least partially the gaps between the stock rails (13) and the switch rails (12) in a railway switch to prevent the switch from being blocked in particular by snow. Advantages of the new sealing element is that it can easier be inserted in these gaps and that it has a smaller effect on the force required to close the switch so that it can also be applied closer to the free extremity of the switch rail (12).
    Type: Grant
    Filed: October 30, 2015
    Date of Patent: June 2, 2020
    Assignee: RECTICEL
    Inventors: Dieter Van Damme, Philippe Vander Schelden, Peter De Wilde, Mario Genetello, Rudi Mortelmans
  • Patent number: 10486407
    Abstract: The present invention relates to a method for manufacturing a flexible skin which has at least one insert adhered thereto. In a first step, the skin is molded on a mold surface. In order to adhere the insert to the skin, an opening is first made in the skin giving access to the back face of the insert. The insert is positioned with its back face against the front face of the skin and an adhering layer is provided which is adhesively connected to the back face of the skin layer which surrounds the opening in the skin layer and, through this opening, to the back face of the insert. The adhering layer is preferably produced by applying a layer of a hardenable material, in particular a curable polyurethane composition. Since the back face of the insert engages the front side of the skin penetration of hardenable material to the front face of the insert is avoided.
    Type: Grant
    Filed: June 27, 2013
    Date of Patent: November 26, 2019
    Assignee: RECTICEL AUTOMOBILSYSTEME GMBH
    Inventors: Peter De Wilde, Jean-Christophe Bouckaert, Filip De Swaef, Frank Dierens
  • Publication number: 20150165750
    Abstract: The present invention relates to a method for manufacturing a flexible skin which has at least one insert adhered thereto. In a first step, the skin is moulded on a mould surface. In order to adhere the insert to the skin, an opening is first made in the skin giving access to the back face of the insert. The insert is positioned with its back face against the front face of the skin and an adhering layer is provided which is adhesively connected to the back face of the skin layer which surrounds the opening in the skin layer and, through this opening, to the back face of the insert. The adhering layer is preferably produced by applying a layer of a hardenable material, in particular a curable polyurethane composition. Since the back face of the insert engages the front side of the skin penetration of hardenable material to the front face of the insert is avoided.
    Type: Application
    Filed: June 27, 2013
    Publication date: June 18, 2015
    Applicant: RECTICEL AUTOMOBILSYSTEME GMBH
    Inventors: Peter De Wilde, Jean-Christophe Bouckaert, Filip De Swaef, Frank Dierens
  • Publication number: 20120219722
    Abstract: The present invention relates to a method for producing a flexible elastomeric composite polyurethane skin wherein a polyurethane reaction mixture is sprayed onto a mould surface and the polyurethane reaction mixture is allowed to cure to produce the skin layer. The polyurethane reaction mixture is composed of components comprising at least an isocyanate component, isocyanate-reactive components and a catalyst component and the isocyanate component is composed of at least one isocyanate having at least two NCO-groups which are not directly attached to an aromatic group. The catalyst component is substantially free of lead, which leads to a lower flexibility. In accordance with the invention, the flexibility of the polyurethane skin is increased by means of at least one flexibiliser which reduces the flexural modulus of the skin and which comprises at least one isocyanate-reactive group. The flexibiliser is preferably a monofunctional flexibiliser which comprises only one isocyanate-reactive group.
    Type: Application
    Filed: May 7, 2012
    Publication date: August 30, 2012
    Applicant: RECTICEL AUTOMOBILSYSTEME GMBH
    Inventors: Kristof Benoit, Peter De Wilde, Geert Van Houcke, Koen Vanlandschoot, Yvan Vanluchene, Hugo De Winter
  • Patent number: 8197939
    Abstract: The present invention relates to a method for producing a flexible elastomeric composite polyurethane skin comprising a first and a second flexible polyurethane layer obtained by spraying a first and a second polyurethane reaction mixture onto one another. The first reaction mixture is an aliphatic polyurethane reaction mixture which is free of lead and formulated to produce a polyurethane elastomer having a flexural modulus smaller than 35 MPa. The second reaction mixture is an aromatic polyurethane reaction mixture producing a polyurethane elastomer having a smaller flexural modulus. The thickness of the aliphatic polyurethane layer could be made so small with respect to the thickness of the aromatic polyurethane layer that the composite skin has an average flexural modulus smaller than 30 MPa.
    Type: Grant
    Filed: May 30, 2006
    Date of Patent: June 12, 2012
    Assignee: Recticel Automobilsysteme GmbH
    Inventors: Kristof Benoit, Peter De Wilde, Geert Van Houcke, Koen Vanlandschoot, Yvan Vanluchene, Hugo De Winter
  • Publication number: 20090324941
    Abstract: The present invention relates to a method for producing a flexible elastomeric composite polyurethane skin comprising a first and a second flexible polyurethane layer obtained by spraying a first and a second polyurethane reaction mixture onto one another. The first reaction mixture is an aliphatic polyurethane reaction mixture which is free of lead and formulated to produce a polyurethane elastomer having a flexural modulus smaller than 35 MPa. The second reaction mixture is an aromatic polyurethane reaction mixture producing a polyurethane elastomer having a smaller flexural modulus. The thickness of the aliphatic polyurethane layer could be made so small with respect to the thickness of the aromatic polyurethane layer that the composite skin has an average flexural modulus smaller than 30 MPa.
    Type: Application
    Filed: May 30, 2006
    Publication date: December 31, 2009
    Applicant: RECTICEL AUTOMOBIL SYSTEME GMBH
    Inventors: Kristof Benoit, Peter De Wilde, Geert Van Houcke, Koen Vanlandschoot, Yvan Vanluchene, Hugo De Winter