  • Patent number: 7867607
    Abstract: A polyolefin fiber includes 0.2 to 5.0 wt % of hydrophilic additive, and 0.05 to 3.00 wt % of titanium dioxide (TiO2). The polyolefin fiber may further include 0.2 to 1.0 wt % of spin finish provided on a surface thereof. The polyolefin fiber is spun to have a circular section, a modified cross-section including an X-shaped section, a Y-shaped section, a deltaic section, an oval section, a diamond section, a bladebone-shaped section, and a combined section thereof, or a combined section of the circular section and the modified cross-section. A method of producing a polyolefin fiber includes (a) melt extruding a composition which contains 93 to 99 wt % of polyolefin resin, 0.2 to 5.0 wt % of hydrophilic additive, and 0.05 to 3.00 wt % of any one titanium dioxide (TiO2) of rutile titanium dioxide, anatase titanium dioxide, and brookite titanium dioxide at 240 to 300° C. and performing winding at a spin speed of 500 to 2,000 mpm to produce a undrawn yarn, and (b) drawing the undrawn yarn at a draw ratio of 1.
    Type: Grant
    Filed: December 5, 2007
    Date of Patent: January 11, 2011
    Assignee: Kolonglotech, Inc.
    Inventors: Pyung-Youl Park, Dong-Hun Kwak
  • Publication number: 20090093180
    Abstract: A polyolefin fiber includes 0.2 to 5.0 wt % of hydrophilic additive, and 0.05 to 3.00 wt % of titanium dioxide (TiO2). The polyolefin fiber may further include 0.2 to 1.0 wt % of spin finish provided on a surface thereof. The polyolefin fiber is spun to have a circular section, a modified cross-section including an X-shaped section, a Y-shaped section, a deltaic section, an oval section, a diamond section, a bladebone-shaped section, and a combined section thereof, or a combined section of the circular section and the modified cross-section. A method of producing a polyolefin fiber includes (a) melt extruding a composition which contains 93 to 99 wt % of polyolefin resin, 0.2 to 5.0 wt % of hydrophilic additive, and 0.05 to 3.00 wt % of any one titanium dioxide (TiO2) of rutile titanium dioxide, anatase titanium dioxide, and brookite titanium dioxide at 240 to 300° C. and performing winding at a spin speed of 500 to 2,000 mpm to produce a undrawn yarn, and (b) drawing the undrawn yarn at a draw ratio of 1.
    Type: Application
    Filed: December 5, 2007
    Publication date: April 9, 2009
    Applicant: KolonGlotech, Inc.
    Inventors: Pyung-Youl Park, Dong-Hun Kwak