  • Patent number: 6451944
    Abstract: A continuous, solvent-free process for obtaining solvent-free, fine white powders of high molecular weight alternating copolymers of maleic anhydride and a C1-C4 alkyl vinyl ether, without odor or taste, having the molecular structure (A—B)n, where A is maleic anhydride, B is an alkyl vinyl ether and n is an integer indicative of the molecular weight of the copolymer, which comprises feeding alkyl vinyl ether as reactant and solvent in excess over the desired 1:1 mole ratio of A:B in the copolymer, molten maleic anhydride and a free radical initiator, continuously at predetermined feeding rates into a reactor heated at a reaction temperature of about 50° to 100° C.
    Type: Grant
    Filed: May 18, 2001
    Date of Patent: September 17, 2002
    Assignee: ISP Investments Inc.
    Inventors: Russell Biss, Jeffrey Cohen, John Zamora, Krystyna Plochocka, Jeffrey A. Lynn
  • Patent number: 6365691
    Abstract: A continuous, solvent-free process for obtaining solvent-free, fine white powders of high molecular weight alternating terpolymers of maleic anhydride, a C1-C4 alkyl vinyl ether and isobutylene, without odor or taste.
    Type: Grant
    Filed: July 6, 2000
    Date of Patent: April 2, 2002
    Assignee: ISP Investments Inc.
    Inventors: Russell Biss, Jeffrey Cohen, John Zamora, Krystyna Plochocka, Jeffrey A. Lynn
  • Publication number: 20010053829
    Abstract: A continuous, solvent-free process for obtaining solvent-free, fine white powders of high molecular weight alternating copolymers of maleic anhydride and a C1-C4 alkyl vinyl ether, without odor or taste, having the molecular structure (A-B)n, where A is maleic anhydride, B is an alkyl vinyl ether and n is an integer indicative of the molecular weight of the copolymer, which comprises feeding alkyl vinyl ether as reactant and solvent in excess over the desired 1:1 mole ratio of A:B in the copolymer, molten maleic anhydride and a free radical initiator, continuously at predetermined feeding rates into a reactor heated at a reaction temperature of about 50° to 100° C.
    Type: Application
    Filed: May 18, 2001
    Publication date: December 20, 2001
    Applicant: ISP INVESTMENTS INC.
    Inventors: Russell Biss, Jeffrey Cohen, John Zamora, Krystyna Plochocka, Jeffrey A. Lynn