Patents by Inventor Ryo Satake
Ryo Satake has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).
-
Publication number: 20240309176Abstract: An aluminum crosslinking agent for dip molding has a sufficient stability enabling use in mass production of gloves and the like, and makes it possible to provide a molded body obtained using the aluminum crosslinking agent, which has sufficient tensile strength and fatigue durability and is soft and elongating; a dip molding composition gloves, and a method for producing gloves are provided. These are an aluminum crosslinking agent for dip molding, including a polynuclear aluminum lactate compound, which has a polynuclear aluminum structure and at least one lactic acid residue. The polynuclear aluminum structure has a structure where a plurality of aluminum atoms are polymerized through one oxygen atom, and has a degree of polymerization of 2 to 20, and lactic acid residues or hydroxyl groups are bonded to remaining valences of the aluminum atom.Type: ApplicationFiled: February 1, 2022Publication date: September 19, 2024Applicant: MIDORI ANZEN CO., LTD.Inventors: Norihide ENOMOTO, Shoya SATAKE, Taku TSUNEISHI, Ryo MAEDA, Shun ISHIHARA
-
Patent number: 11630342Abstract: An image display device which suppresses destruction of an image display panel due to static electricity carried by a phase difference film, and has excellent adhesiveness between the phase difference film and the image display panel even in a moisture-heat environment, and a circularly polarizing plate with a photosensitive adhesive. The image display device includes a circularly polarizing plate having a linear polarizer and a phase difference film, and an image display panel in this order from a viewing side, in which the phase difference film and the image display panel are bonded by a pressure-sensitive adhesive, the phase difference film has an optically anisotropic layer obtained by polymerizing a polymerizable liquid crystal composition containing at least one kind of polymerizable liquid crystal compound having a predetermined structure, and the pressure-sensitive adhesive contains a polymer having an acid value of 1 to 30 mgKOH/g and an antistatic agent.Type: GrantFiled: August 7, 2020Date of Patent: April 18, 2023Assignee: FUJIFILM CorporationInventors: Mayumi Nojiri, Satoshi Shimamura, Ryo Satake, Aiko Yoshida
-
Patent number: 11535761Abstract: A quantum dot-containing composition includes a quantum dot, a ligand having coordinating groups, which coordinates to the surface of the quantum dots, and the ligand is represented by Formula I. In Formula I, A is an organic group including one or more coordinating groups selected from an amino group, a carboxy group, a mercapto group, a phosphine group, and a phosphine oxide group, Z is an (n+m+l)-valent organic linking group, R is a group including an alkyl group, an alkenyl group, or an alkynyl group each of which may have a substituent, Y is a group having a polymer chain which has a degree of polymerization of 3 or greater and which includes a polyacrylate skeleton or the like. n and m are each independently 1 or greater, l is 0 or greater, and n+m+l is integer 3 or greater. At least two coordinating groups are included in a molecule.Type: GrantFiled: January 15, 2019Date of Patent: December 27, 2022Assignee: FUJIFILM CorporationInventors: Naoyoshi Yamada, Ryo Satake, Natsuru Chikushi, Kyohei Arayama
-
Patent number: 11370970Abstract: Provided are an optically anisotropic film which has excellent moisture-heat resistance and can have a reduction in the thickness, an optical film, a polarizing plate, and an image display device. The optically anisotropic film is obtained by polymerizing a polymerizable liquid crystal composition, in which the polymerizable liquid crystal composition contains a polymerizable liquid crystal compound represented by Formula (1): L1-SP1-(E3-A1)m-E1-G1-D1-Ar1-D2-G2-E2-(A2-E4)n-SP2-L2 and a polymerizable liquid crystal compound represented by Formula (2): L1-SP1-(E3-A1)m-E1-G1-D1-Ar2-D2-G2-E2-(A2-E4)n-SP2-L2, and the optically anisotropic film satisfies Formula (3): Re(450)/Re(550)<1 or Formula (4): Rth(450)/Rth(550)<1, and has a degree of alignment as measured by Raman spectroscopy of 0.4 or more.Type: GrantFiled: August 12, 2020Date of Patent: June 28, 2022Assignee: FUJIFILM CorporationInventors: Ayako Muramatsu, Ryo Satake, Mayumi Nojiri, Aiko Yoshida, Keita Takahashi
-
Patent number: 11139458Abstract: An organic EL display device is provided in which a change in tint is reduced in a bent portion. This organic EL display device is an organic electroluminescent display device including, from a viewing side, a circularly polarizing plate, a first adhesion layer, and a bendable organic electroluminescent display panel, in which the circularly polarizing plate includes, from the viewing side, a linear polarizer, a second adhesion layer, and a phase difference layer functioning as a ?/4 plate, a complex modulus of elasticity of the first adhesion layer is 2.50×105 Pa or less, the first adhesion layer is thicker than the second adhesion layer, and an absorption axis of the linear polarizer is positioned at an angle of 0°±30° or 90°±30° with respect to an extension direction of a ridge line formed in a case where the organic electroluminescent display device is bent.Type: GrantFiled: January 23, 2020Date of Patent: October 5, 2021Assignee: FUJIFILM CorporationInventors: Toshihiro Konishi, Kenta Yamazaki, Shinpei Yoshida, Ryo Satake, Hiroyuki Okusa
-
Patent number: 10989849Abstract: An optical laminate includes a wavelength selective reflective element, and an absolute phase adjustment layer which is provided on at least one surface side of the wavelength selective reflective element and has optical isotropy, and in which a first region having a first optical path length and a second region having a second optical path length different from the first optical path length are arranged in a pattern with a diffraction grating-like period. The optical laminate reflects light in the specific reflection wavelength region by the wavelength selective reflective element, of light incident from the absolute phase adjustment layer side. In the optical laminate, light which enters the first region of the absolute phase adjustment layer and is reflected by the wavelength selective reflective element and light which enters the second region and is reflected by the wavelength selective reflective element interfere with each other.Type: GrantFiled: January 21, 2019Date of Patent: April 27, 2021Assignee: FUJIFILM CORPORATIONInventors: Ryo Satake, Yukito Saitoh, Daisuke Kashiwagi
-
Patent number: 10982135Abstract: A phosphor-containing film capable of suppressing deterioration of phosphor and capable of suppressing generation of luminescent spots and the reduction in luminance due to a defect of the resin layer. The film includes: a phosphor-containing layer having a resin layer which has impermeability to oxygen and is provided with a plurality of discretely arranged concave portions, and a plurality of fluorescent regions, each of which is arranged in the concave portion of the resin layer and contains a phosphor that deteriorates through a reaction with oxygen when exposed to oxygen; and a first substrate film and a second substrate film, which are respectively laminated on one main surface and the other main surface of the phosphor-containing layer, in which the fluorescent regions contain a binder and quantum dots serving as the phosphor.Type: GrantFiled: February 28, 2019Date of Patent: April 20, 2021Assignee: FUJIFILM CorporationInventors: Tatsuya Oba, Natsuru Chikushi, Kenichi Kakishita, Masayuki Kusumoto, Ryo Satake, Megumi Sekiguchi
-
Publication number: 20200369960Abstract: An object of the present invention is to provide an optically anisotropic film which has excellent moisture-heat resistance and can have a reduction in the thickness, an optical film, a polarizing plate, and an image display device. The optically anisotropic film of the embodiment of the present invention is an optically anisotropic film obtained by polymerizing a polymerizable liquid crystal composition, in which the polymerizable liquid crystal composition contains a polymerizable liquid crystal compound represented by Formula (1) and a polymerizable liquid crystal compound represented by Formula (2), and the optically anisotropic film satisfies Formula (3) or (4), and has a degree of alignment as measured by Raman spectroscopy of 0.4 or more.Type: ApplicationFiled: August 12, 2020Publication date: November 26, 2020Applicant: FUJIFILM CorporationInventors: Ayako MURAMATSU, Ryo SATAKE, Mayumi NOJIRI, Aiko YOSHIDA, Keita TAKAHASHI
-
Publication number: 20200369961Abstract: Provided is an optical film having an excellent film contrast and improved moisture-heat resistance, a polarizing plate, and an image display device. The optical film has an optically anisotropic film obtained by polymerizing a polymerizable liquid crystal composition, and a photo-alignment film, in which the polymerizable liquid crystal composition contains a polymerizable liquid crystal compound represented by Formula (1): L1-SP1-E1-Cy2-Cy1-D1-Ar1-D2-Cy3-Cy4-E2-SP2-L2 and the optically anisotropic film satisfies Formula (I): Re(450)/Re(550)<1 or Formula (II): Rth(450)/Rth(550)<1 and exhibits a diffraction peak derived from a periodic structure in X-ray diffraction measurement.Type: ApplicationFiled: August 12, 2020Publication date: November 26, 2020Applicant: FUJIFILM CorporationInventors: Ayako MURAMATSU, Ryo SATAKE, Mayumi NOJIRI, Aiko YOSHIDA, Keita TAKAHASHI, Toshikazu SUMI
-
Publication number: 20200362244Abstract: A polymerizable liquid crystal composition used for formation of an optically anisotropic film retaining good reciprocal wavelength dispersibility and having an excellent surface condition, an optically anisotropic film, an optical film, a polarizing plate, and an image display device. The polymerizable liquid crystal composition contains a polymerizable liquid crystal compound represented by Formula (I): L1-SP1-A1-D3-G1-D1-Ar-D2-G2-D4-A2-SP2-L2 and a polymerizable compound represented by Formula (II): L5-SP5-D9-C(?O)-Cy1-Cy2-C(?O)-D7-A5-D8-(A6-D10)n-SP6-L6 and not corresponding to Formula (I).Type: ApplicationFiled: August 5, 2020Publication date: November 19, 2020Applicant: FUJIFILM CorporationInventors: Satoshi SHIMAMURA, Aiko YOSHIDA, Keita TAKAHASHI, Ryo SATAKE, Mayumi NOJIRI
-
Publication number: 20200363682Abstract: An image display device which suppresses destruction of an image display panel due to static electricity carried by a phase difference film, and has excellent adhesiveness between the phase difference film and the image display panel even in a moisture-heat environment, and a circularly polarizing plate with a photosensitive adhesive. The image display device includes a circularly polarizing plate having a linear polarizer and a phase difference film, and an image display panel in this order from a viewing side, in which the phase difference film and the image display panel are bonded by a pressure-sensitive adhesive, the phase difference film has an optically anisotropic layer obtained by polymerizing a polymerizable liquid crystal composition containing at least one kind of polymerizable liquid crystal compound having a predetermined structure, and the pressure-sensitive adhesive contains a polymer having an acid value of 1 to 30 mgKOH/g and an antistatic agent.Type: ApplicationFiled: August 7, 2020Publication date: November 19, 2020Applicant: FUJIFILM CorporationInventors: Mayumi NOJIRI, Satoshi SHIMAMURA, Ryo SATAKE, Aiko YOSHIDA
-
Publication number: 20200161589Abstract: An organic EL display device is provided in which a change in tint is reduced in a bent portion. This organic EL display device is an organic electroluminescent display device including, from a viewing side, a circularly polarizing plate, a first adhesion layer, and a bendable organic electroluminescent display panel, in which the circularly polarizing plate includes, from the viewing side, a linear polarizer, a second adhesion layer, and a phase difference layer functioning as a ?/4 plate, a complex modulus of elasticity of the first adhesion layer is 2.50×105 Pa or less, the first adhesion layer is thicker than the second adhesion layer, and an absorption axis of the linear polarizer is positioned at an angle of 0°±30° or 90°±30° with respect to an extension direction of a ridge line formed in a case where the organic electroluminescent display device is bent.Type: ApplicationFiled: January 23, 2020Publication date: May 21, 2020Applicant: FUJIFILM CorporationInventors: Toshihiro KONISHI, Kenta YAMAZAKI, Shinpei YOSHIDA, Ryo SATAKE, Hiroyuki OKUSA
-
Publication number: 20200013835Abstract: The present invention provides an organic electroluminescent display device in which reflection of external light is suppressed and a change in tint in a case of being viewed in an oblique direction is further suppressed, a phase difference film, and a circular polarization plate. This organic electroluminescent display device according to the present invention includes an organic electroluminescence display panel and a circular polarization plate arranged on the organic electroluminescence display panel, in which the circular polarization plate includes a polarizer and a phase difference film, the phase difference film includes a positive A-plate and a positive C-plate, and the positive A-plate and the positive C-plate satisfy prescribed requirements.Type: ApplicationFiled: September 19, 2019Publication date: January 9, 2020Applicant: FUJIFILM CorporationInventors: Ayako MURAMATSU, Kunihiro ATSUMI, Ryo SATAKE, Mayumi NOJIRI
-
Patent number: 10513655Abstract: Provided is a wavelength conversion member including: a wavelength conversion layer including at least one kind of quantum dots that are excited by excitation light to emit fluorescence and are dispersed in an organic matrix; and a barrier layer that is provided adjacent to at least one main surface of the wavelength conversion layer and includes silicon nitride and/or silicon oxynitride as a major component, in which the organic matrix is obtained by curing a curable composition including at least an alicyclic epoxy compound and includes a chemical structure A which is bonded to silicon nitride and/or silicon oxynitride as a major component of the barrier layer.Type: GrantFiled: July 26, 2017Date of Patent: December 24, 2019Assignee: FUJIFILM CorporationInventors: Ryo Satake, Makoto Kamo, Naoyoshi Yamada, Tatsuya Oba
-
Publication number: 20190194531Abstract: A phosphor-containing film capable of suppressing deterioration of phosphor and capable of suppressing generation of luminescent spots and the reduction in luminance due to a defect of the resin layer. The film includes: a phosphor-containing layer having a resin layer which has impermeability to oxygen and is provided with a plurality of discretely arranged concave portions, and a plurality of fluorescent regions, each of which is arranged in the concave portion of the resin layer and contains a phosphor that deteriorates through a reaction with oxygen when exposed to oxygen; and a first substrate film and a second substrate film, which are respectively laminated on one main surface and the other main surface of the phosphor-containing layer, in which the fluorescent regions contain a binder and quantum dots serving as the phosphor.Type: ApplicationFiled: February 28, 2019Publication date: June 27, 2019Applicant: FUJIFILM CorporationInventors: Tatsuya OBA, Natsuru CHIKUSHI, Kenichi KAKISHITA, Masayuki KUSUMOTO, Ryo SATAKE, Megumi SEKIGUCHI
-
Publication number: 20190154895Abstract: An optical laminate includes a wavelength selective reflective element, and an absolute phase adjustment layer which is provided on at least one surface side of the wavelength selective reflective element and has optical isotropy, and in which a first region having a first optical path length and a second region having a second optical path length different from the first optical path length are arranged in a pattern with a diffraction grating-like period. The optical laminate reflects light in the specific reflection wavelength region by the wavelength selective reflective element, of light incident from the absolute phase adjustment layer side. In the optical laminate, light which enters the first region of the absolute phase adjustment layer and is reflected by the wavelength selective reflective element and light which enters the second region and is reflected by the wavelength selective reflective element interfere with each other.Type: ApplicationFiled: January 21, 2019Publication date: May 23, 2019Inventors: Ryo SATAKE, Yukito SAITOH, Daisuke KASHIWAGI
-
Publication number: 20190144689Abstract: A quantum dot-containing composition includes a quantum dot, a ligand having coordinating groups, which coordinates to the surface of the quantum dots, and the ligand is represented by Formula I. In Formula I, A is an organic group including one or more coordinating groups selected from an amino group, a carboxy group, a mercapto group, a phosphine group, and a phosphine oxide group, Z is an (n+m+l)-valent organic linking group, R is a group including an alkyl group, an alkenyl group, or an alkynyl group each of which may have a substituent, Y is a group having a polymer chain which has a degree of polymerization of 3 or greater and which includes a polyacrylate skeleton or the like. n and m are each independently 1 or greater, l is 0 or greater, and n+m+l is integer 3 or greater. At least two coordinating groups are included in a molecule.Type: ApplicationFiled: January 15, 2019Publication date: May 16, 2019Applicant: FUJIFILM CorporationInventors: Naoyoshi YAMADA, Ryo SATAKE, Natsuru CHIKUSHI, Kyohei ARAYAMA
-
Patent number: 10273408Abstract: A wavelength conversion member is provided. The wavelength conversion member includes: a wavelength conversion layer including at least one kind of quantum dots that are excited by excitation light to emit fluorescence and an antioxidant; at least one interposing layer that is formed to be adjacent to the wavelength conversion layer; and a barrier layer that is formed on at least one surface of the wavelength conversion layer, in which at least one layer of the interposing layers is an antioxidant-containing interposing layer including the antioxidant.Type: GrantFiled: November 20, 2017Date of Patent: April 30, 2019Assignee: FUJIFILM CorporationInventors: Ryo Satake, Tatsuya Oba, Hideaki Ito, Hiroyuki Yoneyama
-
Publication number: 20180314102Abstract: There is provided a lighting device using a wavelength conversion sheet used in a liquid crystal display or the like, and an object of the invention is to provide a lighting device having satisfactory durability. The object is achieved by a lighting device including: a point light source; a wavelength conversion sheet; and a light intensity reduction member arranged between the point light source and the wavelength conversion layer, in which the light intensity reduction member reduces peak illuminance of light that is applied by the point light source on a light incident surface of a wavelength conversion sheet by 10% to 80%, and absorbance of light having a wavelength of 450 nm measured by using an integrating sphere is less than 5%.Type: ApplicationFiled: June 19, 2018Publication date: November 1, 2018Applicant: FUJIFILM CorporationInventors: Hirofumi TOYAMA, Ryo SATAKE, Takashi YONEMOTO, Tatsuya OBA, Natsuru CHIKUSHI
-
Patent number: 9989675Abstract: A polarizing plate includes, in the following order, a pressure sensitive adhesive layer, a polarizer, and an outer side layer provided on a visible side rather than the polarizer side, the thickness of the outer side layer is >3 ?m and ?45 ?m, the storage elastic modulus of the adhesive layer after lamination is 0.1 MPa to 2.0 MPa, and a hardness ratio (X/Y) is less than 1, when in measuring the hardness of the outer side layer in a depth direction at intervals of 1.5 ?m from surface A thereof to a surface B on the polarizer side, the absolute value of the difference between an n-th and n+1 measured hardness (where n is an integer of 1 or more) is defined as the hardness difference (X), and the absolute value of the difference between the hardness of surface A and surface B is hardness difference (Y).Type: GrantFiled: March 28, 2016Date of Patent: June 5, 2018Assignee: FUJIFILM CorporationInventors: Ryo Satake, Megumi Sekiguchi