  • Patent number: 9039926
    Abstract: A production process for composite oxide expressed by a compositional formula: LiMn1-xAxO2, where “A” is one or more kinds of metallic elements other than Mn; and 0?“x”<1, obtained by preparing a raw-material mixture by mixing a metallic-compound raw material and a molten-salt raw material with each other, the metallic-compound raw material at least including an Mn-containing nitrate that includes one or more kinds of metallic elements in which Mn is essential, the molten-salt raw material including lithium hydroxide and lithium nitrate, and exhibiting a proportion of the lithium nitrate with respect to the lithium hydroxide (Lithium Nitrate/Lithium Hydroxide) that falls in a range of from 1 or more to 3 or less by molar ratio; reacting the raw-material mixture at 500° C. or less by melting it; and recovering the composite oxide being generated from the raw-material mixture that has undergone the reaction.
    Type: Grant
    Filed: February 7, 2011
    Date of Patent: May 26, 2015
    Assignee: KABUSHIKI KAISHA TOYOTA JIDOSHOKKI
    Inventors: Ryota Isomura, Hitotoshi Murase, Naoto Yasuda
  • Patent number: 8877381
    Abstract: A composite oxide is produced via the following: a raw-material mixture preparation step of preparing a raw-material mixture by mixing a metallic-compound raw material and a molten-salt raw material with each other, the metallic-compound raw material at least including one or more kinds of Mn-containing metallic compounds being selected from the group consisting of oxides, hydroxides and metallic salts that include one or more kinds of metallic elements in which Mn is essential, the molten-salt raw material including lithium hydroxide and lithium nitrate, and exhibiting a proportion of the lithium hydroxide with respect to the lithium nitrate (i.e., (Lithium Hydroxide)/(Lithium Nitrate)) that falls in a range of from 0.05 or more to less than 1 by molar ratio; a molten reaction step of reacting said raw-material mixture at from 300° C. or more to 550° C. or less by melting it: and a recovery step of recovering said composite oxide being generated from said raw-material mixture that has undergone the reaction.
    Type: Grant
    Filed: March 7, 2011
    Date of Patent: November 4, 2014
    Assignee: Kabushiki Kaisha Toyota Jidoshokki
    Inventors: Naoto Yasuda, Hitotoshi Murase, Ryota Isomura
  • Publication number: 20130171525
    Abstract: A production process according to the present invention is a novel production process for composite oxide, production process whose a major product is a lithium-manganese-based oxide that includes at least the following: a lithium (Li) element; and a tetravalent manganese (Mn) element, and lithium-manganese-based oxide whose crystal structure belongs to a layered rock-salt structure; said composite oxide is obtained via the following: a molten reaction step of reacting at least the following one another: a metal-containing raw material; and a molten-salt raw material at a melting point of the molten-salt raw material or more, the metal-containing raw material including one or more kinds of metallic elements in which Mn is essential, the molten-salt raw material including lithium hydroxide but not including any other compound virtually, and the molten-salt raw material including Li in an amount that exceeds a theoretical composition of Li being included in said composite oxide to be targeted; and a recovery
    Type: Application
    Filed: August 6, 2011
    Publication date: July 4, 2013
    Applicant: KABUSHIKI KAISHA TOYOTA JIDOSHOKKI
    Inventors: Naoto Yasuda, Toru Abe, Ryota Isomura
  • Publication number: 20130017449
    Abstract: The present invention is characterized in that it is a positive-electrode active material for lithium-ion secondary battery, the positive-electrode active material being capable of absorbing and releasing lithium; it includes the following at least: a first compound exhibiting an irreversible capacity; and a second compound being capable of absorbing more lithium than an amount of lithium that has been released at the time of first-round charging; and it exhibits an irreversible capacity decreasing as a whole of active material. An irreversible capacity of the resulting positive-electrode active material can be reduced by combining the specific compounds to use.
    Type: Application
    Filed: April 4, 2011
    Publication date: January 17, 2013
    Applicant: KABUSHIKI KAISHA TOYOTA JIDOSHOKKI
    Inventors: Naoto Yasuda, Hitotoshi Murase, Ryota Isomura, Toru Abe
  • Publication number: 20120321954
    Abstract: The present invention is a production process for composite oxide being expressed by a compositional formula: LiMn1-xAxO2 (where “A” is one or more kinds of metallic elements other than Mn; and 0?“x”<1), and the composite oxide is obtained via the following: a raw-material mixture preparation step of preparing a raw-material mixture by mixing a metallic-compound raw material and a molten-salt raw material with each other, the metallic-compound raw material at least including an Mn-containing nitrate that includes one or more kinds of metallic elements in which Mn is essential, the molten-salt raw material including lithium hydroxide and lithium nitrate, and exhibiting a proportion of the lithium nitrate with respect to the lithium hydroxide (i.e., (Lithium Nitrate)/(Lithium Hydroxide)) that falls in a range of from 1 or more to 3 or less by molar ratio; a molten reaction step of reacting the raw-material mixture at 500° C.
    Type: Application
    Filed: February 7, 2011
    Publication date: December 20, 2012
    Applicant: KABUSHIKI KAISHA TOYOTA JIDOSHOKKI
    Inventors: Ryota Isomura, Hitotoshi Murase, Naoto Yasuda
  • Publication number: 20120315544
    Abstract: A composite oxide is produced via the following: a raw-material mixture preparation step of preparing a raw-material mixture by mixing a metallic-compound raw material and a molten-salt raw material with each other, the metallic-compound raw material at least including one or more kinds of Mn-containing metallic compounds being selected from the group consisting of oxides, hydroxides and metallic salts that include one or more kinds of metallic elements in which Mn is essential, the molten-salt raw material including lithium hydroxide and lithium nitrate, and exhibiting a proportion of the lithium hydroxide with respect to the lithium nitrate (i.e., (Lithium Hydroxide)/(Lithium Nitrate)) that falls in a range of from 0.05 or more to less than 1 by molar ratio; a molten reaction step of reacting said raw-material mixture at from 300° C. or more to 550° C.
    Type: Application
    Filed: March 7, 2011
    Publication date: December 13, 2012
    Applicant: KABUSHIKI KAISHA TOYOTA JIDOSHOKKI
    Inventors: Naoto Yasuda, Hitotoshi Murase, Ryota Isomura
  • Publication number: 20120282526
    Abstract: A composite oxide, whose major component is a lithium-manganese-system oxide including Li and tetravalent Mn at least and having a crystal structure that belongs to a layered rock-salt structure, is produced via the following: a raw-material mixture preparation step of preparing a raw-material mixture by mixing a metallic-compound raw material and a molten-salt raw material with each other, the metallic-compound raw material at least including one or more kinds of metallic compounds being selected from the group consisting of oxides, hydroxides and metallic salts that include one or more kinds of metallic elements in which Mn is essential, the molten-salt raw material including lithium hydroxide and lithium nitrate, and exhibiting a proportion of the lithium hydroxide with respect to the lithium nitrate (i.e.
    Type: Application
    Filed: December 20, 2010
    Publication date: November 8, 2012
    Applicant: KABUSHIKI KAISHA TOYOTA JIDOSHOKKI
    Inventors: Naoto Yasuda, Ryota Isomura