Patents by Inventor Ryousuke Sawa

Ryousuke Sawa has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 8152585
    Abstract: The present invention provides a method for manufacturing a plasma display panel having a front plate provided with a front substrate, a display electrode formed on the front substrate, a dielectric layer covering the display electrode, and a protective layer covering the dielectric layer. In the method above, after the protective layer has been formed, the front plate is processed in a moisture-free atmosphere for only a period where the front plate has a temperature of 400° C. or lower.
    Type: Grant
    Filed: November 10, 2009
    Date of Patent: April 10, 2012
    Assignee: Panasonic Corporation
    Inventors: Masaki Nishimura, Koyo Sakamoto, Ryousuke Sawa
  • Patent number: 8067322
    Abstract: A glass composition for lamps includes the following by weight percent: SiO2: 60-75 wt %; CeO2+Ce2O3: 0.01-5.2 wt %; SnO+SnO2: 0.01-5.2 wt %; Al2O3: 0.5-6 wt %; B2O3: 0-5 wt %; Li2O+Na2O+K2O: 13-20 wt %; MgO: 0.5-5 wt %; CaO: 1-10 wt %; SrO: 0-10 wt %; BaO: 0-10 wt %; ZnO: 0-10 wt %; Fe2O3+FeO: 0-0.2 wt %; and TiO2: 0-1 wt %. The glass composition for lamps that contains no lead or antimony achieves high ultraviolet screening capacity, ensuring fewer occurrences of initial coloring and ultraviolet ray caused coloring of glass.
    Type: Grant
    Filed: July 7, 2006
    Date of Patent: November 29, 2011
    Assignee: National Institute of Advanced Industrial Science and Technology
    Inventors: Ryousuke Sawa, Junko Abe, Tomoko Atagi, Masanobu Itou, Tomoko Akai, Masaru Yamashita
  • Publication number: 20110159772
    Abstract: The present invention provides a method for manufacturing a plasma display panel having a front plate provided with a front substrate, a display electrode formed on the front substrate, a dielectric layer covering the display electrode, and a protective layer covering the dielectric layer. In the method above, after the protective layer has been formed, the front plate is processed in a moisture-free atmosphere for only a period where the front plate has a temperature of 400° C. or lower.
    Type: Application
    Filed: November 10, 2009
    Publication date: June 30, 2011
    Inventors: Masaki Nishimura, Koyo Sakamoto, Ryousuke Sawa
  • Publication number: 20100216624
    Abstract: A glass composition for lamps includes the following by weight percent: SiO2: 60-75 wt %; CeO2+Ce2O3: 0.01-5.2 wt %; SnO+SnO2: 0.01-5.2 wt %; Al2O3: 0.5-6 wt %; B2O3: 0-5 wt %; Li2O+Na2O+K2O: 13-20 wt %; MgO: 0.5-5 wt %; CaO: 1-10 wt %; SrO: 0-10 wt %; BaO: 0-10 wt %; ZnO: 0-10 wt %; Fe2O3+FeO: 0-0.2 wt %; and TiO2: 0-1 wt %. The glass composition for lamps that contains no lead or antimony achieves high ultraviolet screening capacity, ensuring fewer occurrences of initial coloring and ultraviolet ray caused coloring of glass.
    Type: Application
    Filed: August 7, 2006
    Publication date: August 26, 2010
    Inventors: Ryousuke Sawa, Junko Abe, Tomoko Atagi, Masanobu Itou, Tomoko Akai, Masaru Yamashita