Patents by Inventor Sang-Yuel JUNG

Sang-Yuel JUNG has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 9752202
    Abstract: Provided are a method and a refining device for producing molten steel of outstanding cleanliness, and more particularly provides a method and device for refining inclusions by forming droplets from molten steel and dropping same into slag during pre-processing in a continuous casting process in a steel-making process.
    Type: Grant
    Filed: May 13, 2013
    Date of Patent: September 5, 2017
    Assignee: POSCO
    Inventors: Ja Yong Choi, Seung Min Han, Sun Koo Kim, Hee Ho Lee, Sang Yuel Jung, Young Jong Seo
  • Publication number: 20150122083
    Abstract: Provided are a method and a refining device for producing molten steel of outstanding cleanliness, and more particularly provides a method and device for refining inclusions by forming droplets from molten steel and dropping same into slag during pre-processing in a continuous casting process in a steel-making process.
    Type: Application
    Filed: May 13, 2013
    Publication date: May 7, 2015
    Applicant: POSCO
    Inventors: Ja Yong Choi, Seung Min Han, Sun Koo Kim, Hee Ho Lee, Sang Yuel Jung, Young Jong Seo
  • Publication number: 20080156144
    Abstract: The present invention relates to a method for reducing to metallic chromium the chromium oxide material found in slag formed in an electric arc furnace during the process of making stainless steel in that furnace. The chromium oxide content of the slag can be effectively reduced to a relatively low concentration by maintaining the slag in a liquid phase while at the same time blowing into the furnace via a carrier gas certain amounts of powdered aluminum dross. In particular, powdered aluminum dross can be blown into the furnace in amounts ranging from about 10 to 20 kg of dross per ton of molten steel in the furnace. Alternatively, powdered aluminum dross can be blown into the furnace in a thrown-in amount which satisfies the equation: 0.5?[Thrown-In Al dross (ton)×100]/[Slag in Furnace (ton)×Cr2O3 (wt %)]?1.0. Via such a method used during the stainless steel making process, the recovery of valuable chromium and the rate of chromium oxide reduction can be increased.
    Type: Application
    Filed: December 26, 2007
    Publication date: July 3, 2008
    Applicant: POSCO
    Inventors: Sang-Yuel JUNG, Yong Hwan KIM, Sun-Min BYUN, Sang-Beom LEE, Hyun-Chul CHUN