  • Publication number: 20130232937
    Abstract: A spinnable, gel-free and thermally stable polyester composition includes at least one dicarboxylic acid or monoesters thereof or diesters thereof; at least one diol; at least one carboxylic acid anhydride; at least one sodium or lithium based aromatic co-monomer and at least one hydroxyl terminated polyester polyol. The polyester is produced by esterifying at least one dicarboxylic acid or monoesters thereof or diesters thereof and at least one diol along with at least one acid anhydride at a temperature in the range of 250° C. to 290° C. and pressure in the range of 0 kg/cm2g to 5 kg/cm2g; and polycondensing the esterified mixture along with at least one sodium or lithium based aromatic compound and at least one hydroxyl terminated polyether polyol at a temperature in the range of 250° C. to 290° C. and under vacuum of 0.1 torr to 10 torr.
    Type: Application
    Filed: September 6, 2012
    Publication date: September 12, 2013
    Applicant: Reliance Industries Limited
    Inventors: Vikas Madhusudan Nadkarni, Santosh Raghavendra Huilgol, Shilpa Girish Nayak, Ashwin Kumar Jain, Makarand Renukadas Megde, Sanjay Kesarwani
  • Publication number: 20100180563
    Abstract: The present invention discloses an easily alkali soluble polyester comprising at least one dicarboxylic acid or monoesters thereof or diesters thereof; at least one diol; at least one carboxylic acid anhydride; at least one sodium or lithium based aromatic co-monomer and at least one hydroxyl terminated polyester polyol. The polyester is produced by esterifying at least one dicarboxylic acid or monoesters thereof or diesters thereof and at least one diol alongwith at least one acid anhydride at a temperature in the range of 250 to 290° C. and pressure in the range of 0 to 5 kg/cm2g; and polycondensing the esterified mixture along with at least one sodium or lithium based aromatic compound and at least one hydroxyl terminated polyether polyol at temperature in the range of 250 to 290° C. and under vacuum of 0.1 to 10 torr.
    Type: Application
    Filed: March 30, 2007
    Publication date: July 22, 2010
    Applicant: RELIANCE INDUSTRIES LIMITED
    Inventors: Vikas Madhusudan Nadkarni, Santosh Raghavendra Huilgol, Shilpa Girish Nayak, Ashwin Kumar Jain, Makarand Renukadas Megde, Sanjay Kesarwani