Patents by Inventor Stanislav Najmr

Stanislav Najmr has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 4685935
    Abstract: A process for producing a pure magnesium sulphite from crude crystalline magnesium sulphite. Into a full suspension or flow containing magnesium sulphite crystals at least one further water-containing and heat-supplying flow is led. The heat-supplying flow rapidly increases the temperature of the suspension to above 80.degree. C. in less than 10 seconds, preferably in less than 2 seconds. The solid water-insoluble fraction is then separated from the resulting flow, and the pure product is recrystallized from the solution. The solution may be recycled into the process either for further purification or for use as at least one heat-supplying flow.
    Type: Grant
    Filed: June 26, 1986
    Date of Patent: August 11, 1987
    Assignee: Vysoka Skola chemicko-technologicka
    Inventors: Stanislav Najmr, Zdenek Jerman, Jaroslav Kralicek
  • Patent number: 4474737
    Abstract: Process of purification of magnesic raw material. Sulphur dioxide is allowed to react with an aqueous suspension of calcinated magnesite, crude or contaminated magnesium oxide, magnesium hydroxide, hydrated magnesium carbonates, or crude crystals of magnesium sulphite, and, after reaching a pH of 3 to 7.5 the reaction mixture is separated into a solid phase at least one fraction of which is rich in MgSO.sub.3.xH.sub.2 O, wherein x stands for 3 or 6, and at least one fraction containing concentrated impurities. The whole process is carried out at least once. A reaction mixture having a pH below 5 can be preferably transferred to pH 5.2 by the addition of an alkali, e.g. magnesium oxide or magnesium hydroxide, whereupon separation of at least two fractions of the solid phase is accomplished. The fractions obtained can be further purified by mixing in a hydrophilic liquid, and by a following separation. The fraction of crude magnesium sulphite crystals can be heated to a temperature over 60 degress C.
    Type: Grant
    Filed: January 10, 1983
    Date of Patent: October 2, 1984
    Assignee: Vysoka, skola chemiko-technologicka
    Inventors: Stanislav Najmr, Zdenek Jerman, Jaroslav Kralicek