  • Publication number: 20230167557
    Abstract: A method for manufacturing a hot-rolled and coated steel sheet having a thickness between 1.8 mm and 5 mm. The method contains the steps of: providing a semi-product having a composition containing: 0.04%?C?0.38%, 0.40%?Mn?3%, 0.005%?Si?0.70%, 0.005%?Al?0.1%, 0.001%?Cr?2%, 0.001%?Ni?2%, 0.001%?Ti?0.2%, Nb?0.1%, B?0.010%, 0.0005%?N?0.010%, 0.0001%?S?0.05%, 0.0001%?P?0.1%, Mo?0.65%, W?0.30%, Ca?0.006%, hot-rolling with a final rolling temperature FRT, to obtain a hot-rolled steel product having a thickness between 1.8 mm and 5 mm, then cooling down to a coiling temperature Tcoil satisfying: 450° C.
    Type: Application
    Filed: January 10, 2023
    Publication date: June 1, 2023
    Inventors: Thomas HENRION, Ronan JACOLOT, Martin BEAUVAIS
  • Publication number: 20200224297
    Abstract: A method for manufacturing a hot-rolled and coated steel sheet having a thickness between 1.8 mm and 5 mm. The method contains the steps of: providing a semi-product having a composition containing: 0.04%?C?0.38%, 0.40%?Mn?3%, 0.005%?Si?0.70%, 0.005%?Al?0.1%, 0.001%?Cr?2%, 0.001%?Ni?2%, 0.001%?Ti?0.2%, Nb?0.1%, B?0.010%, 0.0005%?N?0.010%, 0.0001%?S?0.05%, 0.0001%?P?0.1%, Mo?0.65%, W?0.30%, Ca?0.006%, hot-rolling with a final rolling temperature FRT, to obtain a hot-rolled steel product having a thickness between 1.8 mm and 5 mm, then cooling down to a coiling temperature Tcoil satisfying: 450° C.
    Type: Application
    Filed: November 23, 2017
    Publication date: July 16, 2020
    Inventors: Thomas HENRION, Ronan JACOLOT, Martin BEAUVAIS