Patents by Inventor Thomas W. Ballinger

Thomas W. Ballinger has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 9133583
    Abstract: A process for making a stiffened and rigid paper includes preparing a pulp slurry consisting essentially of water, a cellulosic pulp, a crosslinker, and a starch, and optionally a binder; draining the liquid from the pulp slurry to form a web; and drying the web. Alternatively, a process for making a stiffened and rigid paper includes the step of adding at least one crosslinker at one or more locations, such as at the wet-end, dry-end, or at both ends of the papermaking process. Suitable crosslinkers include a glyoxal-containing crosslinker, a gluteraldehyde, a polyfunctional aziridine, a zirconium-containing crosslinker, a titanium-containing crosslinker, and an epichlorohydrin, and mixtures thereof. When a binder is employed, it can be added either in the dry or wet form. Provided is a neutral or alkaline process to produce a paper product having the improved mechanical properties of a laminated product in the Z-direction, without a lamination step.
    Type: Grant
    Filed: June 20, 2013
    Date of Patent: September 15, 2015
    Assignee: P.H. Glatfelter Company
    Inventor: Thomas W. Ballinger
  • Publication number: 20130284388
    Abstract: A process for making a stiffened and rigid paper includes preparing a pulp slurry consisting essentially of water, a cellulosic pulp, a crosslinker, and a starch, and optionally a binder; draining the liquid from the pulp slurry to form a web; and drying the web. Alternatively, a process for making a stiffened and rigid paper includes the step of adding at least one crosslinker at one or more locations, such as at the wet-end, dry-end, or at both ends of the papermaking process. Suitable crosslinkers include a glyoxal-containing crosslinker, a gluteraldehyde, a polyfunctional aziridine, a zirconium-containing crosslinker, a titanium-containing crosslinker, and an epichlorohydrin, and mixtures thereof. When a binder is employed, it can be added either in the dry or wet form. Provided is a neutral or alkaline process to produce a paper product having the improved mechanical properties of a laminated product in the Z-direction, without a lamination step.
    Type: Application
    Filed: June 20, 2013
    Publication date: October 31, 2013
    Inventor: Thomas W. Ballinger
  • Patent number: 8496784
    Abstract: A process for making a stiffened and rigid paper includes preparing a pulp slurry consisting essentially of water, a cellulosic pulp, a crosslinker, and a starch, and optionally a binder; draining the liquid from the pulp slurry to form a web; and drying the web. Alternatively, a process for making a stiffened and rigid paper includes the step of adding at least one crosslinker at one or more locations, such as at the wet-end, dry-end, or at both ends of the papermaking process. Suitable crosslinkers include a glyoxal-containing crosslinker, a gluteraldehyde, a polyfunctional aziridine, a zirconium-containing crosslinker, a titanium-containing crosslinker, and an epichlorohydrin, and mixtures thereof. When a binder is employed, it can be added either in the dry or wet form. Provided is a neutral or alkaline process to produce a paper product having the improved mechanical properties of a laminated product in the Z-direction, without a lamination step.
    Type: Grant
    Filed: April 5, 2011
    Date of Patent: July 30, 2013
    Assignee: P.H. Glatfelter Company
    Inventor: Thomas W. Ballinger
  • Publication number: 20120255696
    Abstract: A process for making a stiffened and rigid paper includes preparing a pulp slurry consisting essentially of water, a cellulosic pulp, a crosslinker, and a starch, and optionally a binder; draining the liquid from the pulp slurry to form a web; and drying the web. Alternatively, a process for making a stiffened and rigid paper includes the step of adding at least one crosslinker at one or more locations, such as at the wet-end, dry-end, or at both ends of the papermaking process. Suitable crosslinkers include a glyoxal-containing crosslinker, a gluteraldehyde, a polyfunctional aziridine, a zirconium-containing crosslinker, a titanium-containing crosslinker, and an epichlorohydrin, and mixtures thereof. When a binder is employed, it can be added either in the dry or wet form. Provided is a neutral or alkaline process to produce a paper product having the improved mechanical properties of a laminated product in the Z-direction, without a lamination step.
    Type: Application
    Filed: April 5, 2011
    Publication date: October 11, 2012
    Applicant: P.H. GLATFELTER COMPANY
    Inventor: Thomas W. Ballinger