  • Patent number: 11230641
    Abstract: Disclosed herein is a film comprising a polymer blend, the polymer blend comprising a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C. Disclosed herein too is a method of manufacturing a film comprising blending a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole to form a polymer blend; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C.; and forming the polymer blend into a film.
    Type: Grant
    Filed: July 21, 2016
    Date of Patent: January 25, 2022
    Assignee: DOW GLOBAL TECHNOLOGIES LLC
    Inventors: Jacquelyn A. Degroot, Thor E. Gardarsson, Lisa S. Madenjian
  • Publication number: 20180223092
    Abstract: Disclosed herein is a film comprising a polymer blend, the polymer blend comprising a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C. Disclosed herein too is a method of manufacturing a film comprising blending a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole to form a polymer blend; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C.; and forming the polymer blend into a film.
    Type: Application
    Filed: July 21, 2016
    Publication date: August 9, 2018
    Inventors: Jacquelyn A. Degroot, Thor E. Gardarsson, Lisa S. Madenjian