Patents by Inventor Tiao-Tang LI

Tiao-Tang LI has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Publication number: 20130136867
    Abstract: An environmental friendly process for manufacturing and recycling a painted plastic product includes several steps: (a) selecting an engineering material, (b) applying the engineering material to a mold for forming a crude product via an injection molding method or a compression molding method, (c) tuning an ambient temperature below 160 Celsius degrees, and spraying a thermosetting powdered paint to coat on the crude product directly by an electrostatic gun so as to form an unfinished product, (d) putting the unfinished product into an oven, and baking the unfinished product for 10 to 15 minutes so as to form the painted plastic product. Under this arrangement, when said steps are applied, the engineering material is molded, sprayed with the thermosetting powdered paint, and baked so as to form the painted plastic product without an introduction of the chemical pretreatment steps.
    Type: Application
    Filed: January 22, 2013
    Publication date: May 30, 2013
    Inventor: Tiao-Tang Li
  • Publication number: 20130017339
    Abstract: An eco-friendly process for coating a plastic product includes several steps: (a) adding a conducting material to a thermoplastic material, (b) mixing the conducting material and the thermoplastic material homogeneously, and then molding into a product (c) spraying charged paint uniformly on the product (d) baking the painted product in ambient temperature atmosphere. Under this arrangement, plastic product made of different material could be produced without pre-treatment.
    Type: Application
    Filed: July 15, 2011
    Publication date: January 17, 2013
    Inventor: Tiao-Tang LI
  • Publication number: 20110123720
    Abstract: A method for painting a plastic powder product includes the steps of: adding a conductive material into engineering plastics; high pressure injection molding the engineering plastics with the conductive material in a module to manufacture a plastic powder product; surface treating the plastic powder product for removing oil stains and inks from the plastic powder product, an electrostatic gun spraying paint on the plastic powder product; baking the plastic powder product in an ultraviolet oven for hardening the plastic powder product at a temperature between 90. degree. C. and 120. degree. C. for about 3 to 15 minutes.
    Type: Application
    Filed: November 25, 2009
    Publication date: May 26, 2011
    Applicant: Govern General International Co., Ltd.
    Inventor: Tiao-Tang LI