Patents by Inventor Ting-Mu CHUANG

Ting-Mu CHUANG has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 11962015
    Abstract: Provided are an electrolytic copper foil, an electrode and a lithium-ion cell comprising the same. The electrolytic copper foil has a first surface and a second surface opposite the first surface. An absolute difference of the FWHM of the characteristic peaks of (111) planes of the first surface and the second surface analyzed by GIXRD is less than 0.14, the first and the second surfaces each have a nanoindentation hardness of 0.3 GPa to 3.0 GPa, and the yield strength of the electrolytic copper foil is more than 230 MPa. By controlling the absolute difference of the FWHM of the characteristic peaks of (111) plane of these two surfaces, the nanoindentation hardness of these two surfaces and the yield strength, the electrolytic copper foil can have improved tolerance to the repeated charging and discharging and reduced warpage, thereby improving the yield rate and value of the lithium-ion cell.
    Type: Grant
    Filed: September 8, 2022
    Date of Patent: April 16, 2024
    Assignee: CHANG CHUN PETROCHEMICAL CO., LTD.
    Inventors: Ting-Mu Chuang, Sung-Shiuan Lin, Yao-Sheng Lai, Jui-Chang Chou
  • Publication number: 20230420688
    Abstract: Provided are an electrolytic copper foil, an electrode and a lithium-ion cell comprising the same. The electrolytic copper foil has a first surface and a second surface opposite the first surface. An absolute difference of the FWHM of the characteristic peaks of (111) planes of the first surface and the second surface analyzed by GIXRD is less than 0.14, the first and the second surfaces each have a nanoindentation hardness of 0.3 GPa to 3.0 GPa, and the yield strength of the electrolytic copper foil is more than 230 MPa. By controlling the absolute difference of the FWHM of the characteristic peaks of (111) plane of these two surfaces, the nanoindentation hardness of these two surfaces and the yield strength, the electrolytic copper foil can have improved tolerance to the repeated charging and discharging and reduced warpage, thereby improving the yield rate and value of the lithium-ion cell.
    Type: Application
    Filed: September 8, 2022
    Publication date: December 28, 2023
    Inventors: Ting-Mu CHUANG, SUNG-SHIUAN LIN, Yao-Sheng LAI, Jui-Chang CHOU