  • Patent number: 9475037
    Abstract: The invention relates to a nickel hexaaluminate-comprising catalyst for reforming hydrocarbons, preferably methane, in the presence of carbon dioxide, which comprises hexaaluminate in a proportion in the range from 65 to 95% by weight, preferably from 70 to 90% by weight, and a crystalline, oxidic secondary phase selected from the group consisting of LaAlO3, SrAl2O4 and BaAl2O4 in the range from 5 to 35% by weight, preferably from 10 to 30% by weight. The BET surface area of the catalyst is ?5 m2/g, preferably ?10 m2/g. The molar nickel content of the catalyst is ?3 mol %, preferably ?2.5 mol % and more preferably ?2 mol %. The interlayer cations are preferably Ba and/or Sr. The process for producing the catalyst comprises the steps: (i) production of a mixture of metal salts, preferably nitrate salts of Ni and also Sr and/or La, and a nanoparticulate aluminum source, (ii) molding and (iii) calcination.
    Type: Grant
    Filed: March 6, 2014
    Date of Patent: October 25, 2016
    Assignee: BASF SE
    Inventors: Stephan Schunk, Ekkehard Schwab, Andrian Milanov, Guido Wasserschaff, Thomas Roussiere, Gerhard Cox, Bernd Hinrichsen, Ulrich Floerchinger
  • Publication number: 20160008791
    Abstract: The invention relates to a nickel hexaaluminate-comprising catalyst for reforming hydrocarbons, preferably methane, in the presence of carbon dioxide, which comprises hexaaluminate in a proportion in the range from 65 to 95% by weight, preferably from 70 to 90% by weight, and a crystalline, oxidic secondary phase selected from the group consisting of LaAlO3, SrAl2O4 and BaAl2O4 in the range from 5 to 35% by weight, preferably from 10 to 30% by weight. The BET surface area of the catalyst is ?5 m2/g, preferably ?10 m2/g. The molar nickel content of the catalyst is ?3 mol %, preferably ?2.5 mol % and more preferably ?2 mol %. The interlayer cations are preferably Ba and/or Sr. The process for producing the catalyst comprises the steps: (i) production of a mixture of metal salts, preferably nitrate salts of Ni and also Sr and/or La, and a nanoparticulate aluminum source, (ii) molding and (iii) calcination.
    Type: Application
    Filed: March 6, 2014
    Publication date: January 14, 2016
    Applicant: BASF SE
    Inventors: Stephan SCHUNK, Ekkehard SCHWAB, Andrian MILANOV, Guido WASSERSCHAFF, Thomas ROUSSIERE, Gerhard COX, Bernd HINRICHSEN, Ulrich FLOERCHINGER