  • Publication number: 20060013952
    Abstract: There is provided a method of forming a coat on an inner surface of a bearing, in which a jig 13 is attached to a rotor 2 while holding four bearings 12 for example, so as to form those in a cylinder shape. Then, while the rotor 2 is rotated at a circumferential speed of 0.3 m/sec, a nozzle 8 for airless spraying is inserted into the rotor 2, so that the nozzle 8 injects a coating material 30 from the inside of the bearings 12 toward an inner surfaces of the bearings 12 to apply the coating material thereon. Because the coating material 30 is injected from the nozzle 8 without using compressed air, the fly amount of the coating material is made less as compared to air spray painting.
    Type: Application
    Filed: August 8, 2005
    Publication date: January 19, 2006
    Inventors: Tsuyoshi Nakashima, Takuya Tanaka, Weixing Zhong, Takayuki Shibayama
  • Patent number: 6983681
    Abstract: An object of the present invention is to provide a sliding member which can slide for a longer period of time even in a dry state. In the present invention, sliding layers 3 are provided on the surfaces of a base material 2, and the sliding layer 3 contains polybenzimidazole (PBI) and 1 to 70 vol % of a solid lubricant. Since PBI, which is a thermoplastic resin, has higher heat resistance and also has higher material strength than PAI, PI, and EP, which are the conventionally used thermosetting resins, the wear resistance and the anti-seizure property can be improved and a decrease in material strength caused by high-temperature atmosphere, heat generation at the time of sliding, etc. can be restrained. Furthermore, the initial conformability can be improved because of high elongation percentage. Also, since the sliding layer contains the solid lubricant, the coefficient of friction can be decreased, and hence the anti-seizure property can be enhanced.
    Type: Grant
    Filed: February 20, 2004
    Date of Patent: January 10, 2006
    Assignee: Daido Metal Company Ltd.
    Inventors: Hideki Iwata, Takuya Tanaka, Weixing Zhong, Takeshi Shindo, Kotaro Kashiyama
  • Patent number: 6926923
    Abstract: There is provided a method of forming a coat on an inner surface of a bearing, in which a jig 13 is attached to a rotor 2 while holding four bearings 12 for example, so as to form those in a cylinder shape. Then, while the rotor 2 is rotated at a circumferential speed of 0.3 m/sec, a nozzle 8 for airless spraying is inserted into the rotor 2, so that the nozzle 8 injects a coating material 30 from the inside of the bearings 12 toward an inner surfaces of the bearings 12 to apply the coating material thereon. Because the coating material 30 is injected from the nozzle 8 without using compressed air, the fly amount of the coating material is made less as compared to air spray painting.
    Type: Grant
    Filed: August 22, 2003
    Date of Patent: August 9, 2005
    Assignee: Daido Metal Company Ltd.
    Inventors: Tsuyoshi Nakashima, Takuya Tanaka, Weixing Zhong, Takayuki Shibayama
  • Publication number: 20040166341
    Abstract: An object of the present invention is to provide a sliding member which can slide for a longer period of time even in a dry state. In the present invention, sliding layers 3 are provided on the surfaces of a base material 2, and the sliding layer 3 contains polybenzimidazole (PBI) and 1 to 70 vol % of a solid lubricant. Since PBI, which is a thermoplastic resin, has higher heat resistance and also has higher material strength than PAI, PI, and EP, which are the conventionally used thermosetting resins, the wear resistance and the anti-seizure property can be improved and a decrease in material strength caused by high-temperature atmosphere, heat generation at the time of sliding, etc. can be restrained. Furthermore, the initial conformability can be improved because of high elongation percentage. Also, since the sliding layer contains the solid lubricant, the coefficient of friction can be decreased, and hence the anti-seizure property can be enhanced.
    Type: Application
    Filed: February 20, 2004
    Publication date: August 26, 2004
    Applicant: Daido Metal Company Ltd.
    Inventors: Hideki Iwata, Takuya Tanaka, Weixing Zhong, Takeshi Shindo, Kotaro Kashiyama
  • Publication number: 20040062860
    Abstract: There is provided a method of forming a coat on an inner surface of a bearing, in which a jig 13 is attached to a rotor 2 while holding four bearings 12 for example, so as to form those in a cylinder shape. Then, while the rotor 2 is rotated at a circumferential speed of 0.3 m/sec, a nozzle 8 for airless spraying is inserted into the rotor 2, so that the nozzle 8 injects a coating material 30 from the inside of the bearings 12 toward an inner surfaces of the bearings 12 to apply the coating material thereon. Because the coating material 30 is injected from the nozzle 8 without using compressed air, the fly amount of the coating material is made less as compared to air spray painting.
    Type: Application
    Filed: August 22, 2003
    Publication date: April 1, 2004
    Applicant: Daido Metal Company Ltd.
    Inventors: Tsuyoshi Nakashima, Takuya Tanaka, Weixing Zhong, Takayuki Shibayama