Patents by Inventor WOONG TAE YOON

WOONG TAE YOON has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 10329434
    Abstract: The present invention relates to a method for preparing a graphene-containing inorganic coating composition for coating non-ferrous metal objects and a graphene-containing inorganic coating composition prepared thereby, in which the inorganic coating composition contains liquid silica sol that emits far-infrared rays and powdery graphene that has very excellent thermal conductivity, and thus it emits far-infrared rays beneficial to the human body while having excellent durability and thermal conductivity. The method comprises: adding isopropyl alcohol as a solvent to liquid silica sol and a liquid sealant, followed by uniform stirring for 2-3 hours, thereby preparing a first liquid binder; adding powdery graphene, filler and pigment to the first liquid binder, followed by stirring for 8-10 hours, thereby preparing a second binder; and adding a predetermined amount of an adhesion-enhancing agent to the second binder, followed by aging at a temperature of 25 to 32° C. for 9 to 11 hours.
    Type: Grant
    Filed: August 18, 2017
    Date of Patent: June 25, 2019
    Inventors: Woong Tae Yoon, Sang An Kim
  • Publication number: 20190055415
    Abstract: The present invention relates to a method for preparing a graphene-containing inorganic coating composition for coating non-ferrous metal objects and a graphene-containing inorganic coating composition prepared thereby, in which the inorganic coating composition contains liquid silica sol that emits far-infrared rays and powdery graphene that has very excellent thermal conductivity, and thus it emits far-infrared rays beneficial to the human body while having excellent durability and thermal conductivity. The method comprises: adding isopropyl alcohol as a solvent to liquid silica sol and a liquid sealant, followed by uniform stirring for 2-3 hours, thereby preparing a first liquid binder; adding powdery graphene, filler and pigment to the first liquid binder, followed by stirring for 8-10 hours, thereby preparing a second binder; and adding a predetermined amount of an adhesion-enhancing agent to the second binder, followed by aging at a temperature of 25 to 32° C. for 9 to 11 hours.
    Type: Application
    Filed: August 18, 2017
    Publication date: February 21, 2019
    Inventors: WOONG TAE YOON, SANG AN KIM