Patents by Inventor Xiaojiang RUAN

Xiaojiang RUAN has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 11242577
    Abstract: The present invention relates to a rack steel plate with a thickness up to 177.8 mm by a continuous casting slab, the constituents and mass percentages including C0.11˜0.15%, Si0.15˜0.35%, Mn0.95˜1.25%, P?0.010%, S?0.002%, Cr0.45˜0.75%, Mo0.4˜0.6%, Ni1.3˜2.6%, Cu0.2˜0.4%, Al0.06˜0.09%, V0.03˜0.06%, Nb?0.04%, N?0.006%, B0.001˜0.002%, the balance is Fe and unavoidable impurity elements. The manufacture method includes, in sequence, KR molten steel pretreatment, converter smelting, LF refining, RH refining, continuous casting through a straight-arc continuous casting machine, shielding the continuous casting slab a cover and slowly cooling, cleaning the continuous casting slab, heating, high-pressure water descaling, control rolling, straightening, slowly cooling, quenching and tempering treatment.
    Type: Grant
    Filed: October 18, 2016
    Date of Patent: February 8, 2022
    Assignee: JIANGYIN XING CHENG SPECIAL STEEL WORKS CO., LTD
    Inventors: Pifeng Miao, Gang Qian, Guanyou Liu, Liang Chen, Xiaolin Wu, Jingtao Li, Zhuzhong Gao, Xiaojiang Ruan
  • Publication number: 20200071783
    Abstract: The present invention relates to a rack steel plate with a thickness up to 177.8 mm by a continuous casting slab, the constituents and mass percentages including C0.11˜0.15%, Si0.15˜0.35%, Mn0.95˜1.25%, P?0.010%, S?0.002%, Cr0.45˜0.75%, Mo0.4˜0.6%, Ni1.3˜2.6%, Cu0.2˜0.4%, Al0.06˜0.09%, V0.03˜0.06%, Nb?0.04%, N?0.006%, B0.001˜01002%, the balance is Fe and unavoidable impurity elements. The manufacture method includes, in sequence, KR molten steel pretreatment, converter smelting, LF refining, RH refining, continuous casting through a straight-arc continuous casting machine, shielding the continuous casting slab a cover and slowly cooling, cleaning the continuous casting slab, heating, high-pressure water descaling, control rolling, straightening, slowly cooling, quenching and tempering treatment.
    Type: Application
    Filed: October 18, 2016
    Publication date: March 5, 2020
    Applicant: JIANGYIN XING CHENG SPECIAL STEEL WORKS CO., LTD
    Inventors: Pifeng MIAO, Gang QIAN, Guanyou LIU, Liang CHEN, Xiaolin WU, Jingtao LI, Zhuzhong GAO, Xiaojiang RUAN
  • Publication number: 20180100211
    Abstract: A steel, including: between 0.45 and 0.70 wt. % of carbon, between 0.10 and 0.50 wt. % of silicon, between 0.30 and 0.70 wt. % of manganese, between 0.20 and 0.60 wt. % of chromium, less than or equal to 0.025 wt. % of phosphorus, between 0.003 and 0.030 wt. % of sulfur, less than or equal to 0.1 wt. % of molybdenum, less than or equal to 0.2 wt. % of nickel, less than or equal to 0.04 wt. % of aluminum, less than or equal to 0.3 wt. % of copper, less than or equal to 0.001 wt. % of calcium, less than or equal to 0.003 wt. % of titanium, less than or equal to 0.001 wt. % of oxygen, less than or equal to 0.04 wt. % of arsenic, less than or equal to 0.03 wt. % of tin.
    Type: Application
    Filed: December 10, 2017
    Publication date: April 12, 2018
    Inventors: Min CHEN, Feng LI, Qing YIN, Jiaolong ZHAI, Ke GENG, Jianfeng ZHANG, Zhen HUANG, Jian BAO, Xiaojiang RUAN