Patents by Inventor Xinjin Zhao

Xinjin Zhao has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 9931595
    Abstract: Compositions for reduction of NOx generated during a catalytic cracking process, preferably, a fluid catalytic cracking process, are disclosed. The compositions comprise a fluid catalytic cracking catalyst composition, preferably containing a Y-type zeolite, and a particulate NOx reduction composition containing ferrierite zeolite particles. Preferably, the NOx reduction composition contains ferrierite zeolite particles bound with an inorganic binder. In the alternative, the ferrierite zeolite particles are incorporated into the cracking catalyst as an integral component of the catalyst. NOx reduction compositions in accordance with the invention are very effective for the reduction of NOx emissions released from the regenerator of a fluid catalytic cracking unit operating under FCC process conditions without a substantial change in conversion or yield of cracked products. Processes for the use of the compositions are also disclosed.
    Type: Grant
    Filed: July 9, 2010
    Date of Patent: April 3, 2018
    Assignee: W. R. Grace & Co.-Conn.
    Inventors: George Yaluris, Michael Scott Ziebarth, Xinjin Zhao
  • Patent number: 9365779
    Abstract: A catalyst composition comprising at least about 10% by weight pentasil, at least about 12% by weight Y-type zeolite at a pentasil to Y zeolite ratio of at least 0.25, and wherein the pentasil and Y zeolite comprise at least about thirty-five percent of the catalyst have been shown to optimize light olefin yields and LPG from FCC processes. Embodiments having matrix surface areas greater than 25 m2/g, phosphorous and rare earth are preferred. The compositions of this invention are particularly useful in typical fluid catalytic cracking (FCC) processes.
    Type: Grant
    Filed: November 3, 2005
    Date of Patent: June 14, 2016
    Assignee: W. R. GRACE & CO.-CONN.
    Inventors: Wu Cheng Cheng, Meenakshi Sundaram Krishnamoorthy, Ranjit Kumar, Xinjin Zhao, Michael Scott Ziebarth
  • Patent number: 8642499
    Abstract: A particulate catalytic cracking catalyst which comprises a zeolite having catalytic cracking ability under catalytic cracking conditions, added silica, precipitated alumina and, optionally clay. The catalytic cracking catalyst has a high matrix surface area and is useful in a catalytic cracking process, in particularly, a fluid catalytic cracking process, to improve bottoms conversion at a constant coke formation.
    Type: Grant
    Filed: November 21, 2007
    Date of Patent: February 4, 2014
    Assignee: W. R. Grace & Co.-Conn.
    Inventors: Wu-Cheng Cheng, Kevin John Sutovich, Ruizhong Hu, Ranjit Kumar, Xinjin Zhao
  • Patent number: 8084383
    Abstract: The present invention is directed to certain catalyst compositions and processes that are capable of reducing sulfur compounds normally found as part of the gasoline fraction streams of fluid catalytic cracking processes. The present invention is a cracking catalyst composition comprising a zeolite in combination with a Lewis Acid containing component, wherein the cracking catalyst composition comprises 0.2% Na2O or less. It has been found that sulfur compounds in hydrocarbon feeds to fluid catalytic cracking processes can be reduced by at least 15% compared to the same composition, which does not comprise the aforementioned Lewis Acid containing component.
    Type: Grant
    Filed: March 16, 2004
    Date of Patent: December 27, 2011
    Assignee: W.R. Grace & Co.-Conn.
    Inventors: Ruizhong Hu, Xinjin Zhao, Richard Franklin Wormsbecher, Michael Scott Ziebarth
  • Publication number: 20110036754
    Abstract: A particulate catalytic cracking catalyst which comprises a zeolite having catalytic cracking ability under catalytic cracking conditions, added silica, precipitated alumina and, optionally clay. The catalytic cracking catalyst has a high matrix surface area and is useful in a catalytic cracking process, in particularly, a fluid catalytic cracking process, to improve bottoms conversion at a constant coke formation.
    Type: Application
    Filed: November 21, 2007
    Publication date: February 17, 2011
    Inventors: Wu-Cheng Cheng, Kevin John Sutovich, Ruizhong Hu, Ranjit Kumar, Xinjin Zhao
  • Publication number: 20100276337
    Abstract: Compositions for reduction of NOx generated during a catalytic cracking process, preferably, a fluid catalytic cracking process, are disclosed. The compositions comprise a fluid catalytic cracking catalyst composition, preferably containing a Y-type zeolite, and a particulate NOx reduction composition containing ferrierite zeolite particles. Preferably, the NOx reduction composition contains ferrierite zeolite particles bound with an inorganic binder. In the alternative, the ferrierite zeolite particles are incorporated into the cracking catalyst as an integral component of the catalyst. NOx reduction compositions in accordance with the invention are very effective for the reduction of NOx emissions released from the regenerator of a fluid catalytic cracking unit operating under FCC process conditions without a substantial change in conversion or yield of cracked products. Processes for the use of the compositions are also disclosed.
    Type: Application
    Filed: July 9, 2010
    Publication date: November 4, 2010
    Inventors: George Yaluris, Michael Scott Ziebarth, Xinjin Zhao
  • Patent number: 7641787
    Abstract: Compositions for reduction of NOx generated during a catalytic cracking process, preferably, a fluid catalytic cracking process, are disclosed. The compositions comprise a fluid catalytic cracking catalyst composition, preferably containing a Y-type zeolite, and a particulate NOx composition containing particles of a zeolite having a pore size ranging from about 3 to about 7.2 Angstroms and a SiO2 to Al2O3 molar ratio of less than about 500. Preferably, the NOx reduction composition contains NOx reduction zeolite particles bound with an inorganic binder. In the alternative, the NOx reduction zeolite particles are incorporated into the cracking catalyst as an integral component of the catalyst. Compositions in accordance with the invention are very effective for the reduction of NOx emissions released from the regenerator of a fluid catalytic cracking unit operating under FCC process conditions without a substantial change in conversion or yield of cracked products.
    Type: Grant
    Filed: November 7, 2008
    Date of Patent: January 5, 2010
    Assignee: W.R. Grace & Co.-Conn.
    Inventors: George Yaluris, Michael Scott Ziebarth, Xinjin Zhao
  • Publication number: 20090068079
    Abstract: Compositions for reduction of NOx generated during a catalytic cracking process, preferably, a fluid catalytic cracking process, are disclosed. The compositions comprise a fluid catalytic cracking catalyst composition, preferably containing a Y-type zeolite, and a particulate NOx composition containing particles of a zeolite having a pore size ranging from about 3 to about 7.2 Angstroms and a SiO2 to Al2O3 molar ratio of less than about 500. Preferably, the NOx reduction composition contains NOx reduction zeolite particles bound with an inorganic binder. In the alternative, the NOx reduction zeolite particles are incorporated into the cracking catalyst as an integral component of the catalyst. Compositions in accordance with the invention are very effective for the reduction of NOx emissions released from the regenerator of a fluid catalytic cracking unit operating under FCC process conditions without a substantial change in conversion or yield of cracked products.
    Type: Application
    Filed: November 7, 2008
    Publication date: March 12, 2009
    Inventors: George Yaluris, Michael Scott Ziebarth, Xinjin Zhao
  • Patent number: 7452839
    Abstract: The sulfur content of liquid cracking products, especially the cracked gasoline, of the catalytic cracking process is reduced by the use of a sulfur reduction catalyst composition comprising a porous molecular sieve which contains a metal in an oxidation state above zero within the interior of the pore structure of the sieve as well as a rare earth component which enhances the cracking activity of the cracking catalyst. The molecular sieve is normally a faujasite such as USY. The primary sulfur reduction component is normally a metal of Period 3 of the Periodic Table, preferably vanadium. The rare earth component preferably includes cerium which enhances the sulfur reduction activity of the catalyst. The sulfur reduction catalyst may be used in the form of a separate particle additive or as a component of an integrated cracking/sulfur reduction catalyst.
    Type: Grant
    Filed: December 16, 2004
    Date of Patent: November 18, 2008
    Assignee: W. R. Grace & Co.-Conn.
    Inventors: Wu-Cheng Cheng, Terry G. Roberie, Hye Kyung Cho Timken, Scott Kevin Purnell, Xinjin Zhao
  • Publication number: 20080093263
    Abstract: A catalyst composition comprising at least about 10% by weight pentasil, at least about 12% by weight Y-type zeolite at a pentasil to Y zeolite ratio of at least 0.25, and wherein the pentasil and Y zeolite comprise at least about thirty-five percent of the catalyst have been shown to optimize light olefin yields and LPG from FCC processes. Embodiments having matrix surface areas greater than 25 m2/g, phosphorous and rare earth are preferred. The compositions of this invention are particularly useful in typical fluid catalytic cracking (FCC) processes.
    Type: Application
    Filed: November 3, 2005
    Publication date: April 24, 2008
    Inventors: Wu Cheng Cheng, Meenakshi Krishnamoorthy, Ranjit Kumar, Xinjin Zhao, Michael Ziebarth
  • Patent number: 7304011
    Abstract: Compositions for reduction of NOx generated during a catalytic cracking process, preferably, a fluid catalytic cracking process, are disclosed. The compositions comprise a fluid catalytic cracking catalyst composition, preferably containing a Y-type zeolite, and a particulate NOx composition containing particles of a zeolite having a pore size ranging from about 3 to about 7.2 Angstoms and a SiO2 to Al2O3 molar ratio of less than about 500. Preferably, the NOx reduction composition contains NOx reduction zeolite particles bound with an inorganic binder. In the alternative, the NOx reduction zeolite particles are incorporated into the cracking catalyst as an integral component of the catalyst. Compositions in accordance with the invention are very effective for the reduction of NOx emissions released from the regenerator of a fluid catalytic cracking unit operating under FCC process conditions without a substantial change in conversion or yield of cracked products, e.g., gasoline and light olefins.
    Type: Grant
    Filed: April 15, 2004
    Date of Patent: December 4, 2007
    Assignee: W.R. Grace & Co. -Conn.
    Inventors: George Yaluris, Michael Scott Ziebarth, Xinjin Zhao
  • Patent number: 7153413
    Abstract: The sulfur content of liquid cracking products, especially the cracked gasoline, is reduced in a catalytic cracking process employing a cracking catalyst containing a high content of vanadium. The cracking process involves introducing at least one vanadium compound into a hydrocarbon-sulfur containing feedstock to be charged to a fluid catalytic cracking reactor operating under steady state conditions and containing an equilibrium fluid cracking catalyst inventory within the reactor. The amount of sulfur in the liquid products, in particular gasoline and LCO fractions, is reduced as a result of the increased vanadium content on the equilibrium catalyst. Advantageously, sulfur reduction is achieved even in the presence of other metal contaminants, such as nickel and iron, on the equilibrium catalyst.
    Type: Grant
    Filed: July 10, 2001
    Date of Patent: December 26, 2006
    Assignee: W.R. Grace &Co.-Conn.
    Inventors: Terry G. Roberie, Ranjit Kumar, Michael S Ziebarth, Wu-Cheng Cheng, Xinjin Zhao, Nazeer Bhore
  • Publication number: 20050230285
    Abstract: Compositions for reduction of NOx generated during a catalytic cracking process, preferably, a fluid catalytic cracking process, are disclosed. The compositions comprise a fluid catalytic cracking catalyst composition, preferably containing a Y-type zeolite, and a particulate NOx composition containing particles of a zeolite having a pore size ranging from about 3 to about 7.2 Angstoms and a SiO2 to Al2O3 molar ratio of less than about 500. Preferably, the NOx reduction composition contains NOx reduction zeolite particles bound with an inorganic binder. In the alternative, the NOx reduction zeolite particles are incorporated into the cracking catalyst as an integral component of the catalyst. Compositions in accordance with the invention are very effective for the reduction of NOx emissions released from the regenerator of a fluid catalytic cracking unit operating under FCC process conditions without a substantial change in conversion or yield of cracked products, e.g., gasoline and light olefins.
    Type: Application
    Filed: April 15, 2004
    Publication date: October 20, 2005
    Inventors: George Yaluris, Michael Ziebarth, Xinjin Zhao
  • Publication number: 20050232839
    Abstract: Compositions for reduction of NOx generated during a catalytic cracking process, preferably, a fluid catalytic cracking process, are disclosed. The compositions comprise a fluid catalytic cracking catalyst composition, preferably containing a Y-type zeolite, and a particulate NOx reduction composition containing particles of a zeolite having a pore size ranging from about 3 to about 7.2 Angstoms and a SiO2 to Al2O3 molar ratio of less than about 500. Preferably, the NOx reduction composition contains NOx reduction zeolite particles bound with an inorganic binder. In the alternative, the NOx reduction zeolite particles are incorporated into the cracking catalyst as an integral component of the catalyst. Compositions in accordance with the invention are very effective for the reduction of NOx emissions released from the regenerator of a fluid catalytic cracking unit operating under FCC process conditions without a substantial change in conversion or yield of cracked products.
    Type: Application
    Filed: August 2, 2004
    Publication date: October 20, 2005
    Inventors: George Yaluris, Michael Ziebarth, Xinjin Zhao
  • Publication number: 20050205464
    Abstract: The present invention is directed to certain catalyst compositions and processes that are capable of reducing sulfur compounds normally found as part of the gasoline fraction streams of fluid catalytic cracking processes. The present invention is a cracking catalyst composition comprising a zeolite in combination with a Lewis Acid containing component, wherein the cracking catalyst composition comprises 0.2% Na2O or less. It has been found that sulfur compounds in hydrocarbon feeds to fluid catalytic cracking processes can be reduced by at least 15% compared to the same composition, which does not comprise the aforementioned Lewis Acid containing component.
    Type: Application
    Filed: March 16, 2004
    Publication date: September 22, 2005
    Inventors: Ruizhong Hu, Xinjin Zhao, Richard Wormsbecher, Michael Ziebarth
  • Publication number: 20050130834
    Abstract: The sulfur content of liquid cracking products, especially the cracked gasoline, of the catalytic cracking process is reduced by the use of a sulfur reduction catalyst composition comprising a porous molecular sieve which contains a metal in an oxidation state above zero within the interior of the pore structure of the sieve as well as a rare earth component which enhances the cracking activity of the cracking catalyst. The molecular sieve is normally a faujasite such as USY. The primary sulfur reduction component is normally a metal of Period 3 of the Periodic Table, preferably vanadium. The rare earth component preferably includes cerium which enhances the sulfur reduction activity of the catalyst. The sulfur reduction catalyst may be used in the form of a separate particle additive or as a component of an integrated cracking/sulfur reduction catalyst.
    Type: Application
    Filed: December 16, 2004
    Publication date: June 16, 2005
    Inventors: Wu-Cheng Cheng, Terry Roberie, Hey Kyung Timken, Scott Purnell, Xinjin Zhao
  • Patent number: 6902665
    Abstract: Compositions comprising a component containing (i) an acidic oxide support, (ii) an alkali metal and/or alkaline earth metal or mixtures thereof, (iii) a transition metal oxide having oxygen storage capability, and (iv) palladium promote CO combustion in FCC processes while minimizing the formation of NOx. The acidic oxide support preferably contains silica alumina. Ceria is the preferred oxygen storage oxide.
    Type: Grant
    Filed: December 18, 2001
    Date of Patent: June 7, 2005
    Assignee: W. R. Grace & Co.-Conn.
    Inventors: Alan W. Peters, Edward F. Rakiewicz, Gordon Dean Weatherbee, Xinjin Zhao
  • Publication number: 20050100493
    Abstract: Compositions for reduction of NOx generated during a catalytic cracking process, preferably, a fluid catalytic cracking process, are disclosed. The compositions comprise a fluid catalytic cracking catalyst composition, preferably containing a Y-type zeolite, and a particulate NOx composition containing ferrierite zeolite particles. Preferably, the NOx reduction composition contains ferrierite zeolite particles bound with an inorganic binder. In the alternative, the ferrierite zeolite particles are incorporated into the cracking catalyst as an integral component of the catalyst. NOx reduction compositions in accordance with the invention are very effective for the reduction of NOx emissions released from the regenerator of a fluid catalytic cracking unit operating under FCC process conditions without a substantial change in conversion or yield of cracked products, e.g., gasoline and light olefins. Processes for the use of the compositions are also disclosed.
    Type: Application
    Filed: November 6, 2003
    Publication date: May 12, 2005
    Inventors: George Yaluris, Michael Ziebarth, Xinjin Zhao
  • Publication number: 20050100494
    Abstract: Compositions for reduction of NOx generated during a catalytic cracking process, preferably, a fluid catalytic cracking process, are disclosed. The compositions comprise a fluid catalytic cracking catalyst composition, preferably containing a Y-type zeolite, and a particulate NOx reduction composition containing ferrierite zeolite particles. Preferably, the NOx reduction composition contains ferrierite zeolite particles bound with an inorganic binder. In the alternative, the ferrierite zeolite particles are incorporated into the cracking catalyst as an integral component of the catalyst. NOx reduction compositions in accordance with the invention are very effective for the reduction of NOx emissions released from the regenerator of a fluid catalytic cracking unit operating under FCC process conditions without a substantial change in conversion or yield of cracked products. Processes for the use of the compositions are also disclosed.
    Type: Application
    Filed: August 2, 2004
    Publication date: May 12, 2005
    Inventors: George Yaluris, Michael Ziebarth, Xinjin Zhao
  • Patent number: 6884744
    Abstract: A catalyst useful in cracking of hydrocarbon feedstock comprising particulate material composed of at least 70 weight percent zeolite and the remainder substantially composed of silica sol, alumina sol or mixtures thereof; wherein the particulate material has a kinetic conversion activity of at least about 3; and compositions for fluid catalytic cracking of petroleum feedstock comprising said catalyst and a second particulate material having a kinetic conversion activity of less than 3 wherein said catalyst composition having a kinetic conversion activity of at least about 2.
    Type: Grant
    Filed: April 13, 2001
    Date of Patent: April 26, 2005
    Assignee: W. R. Grace & Co.-Conn.
    Inventors: Wu-Cheng Cheng, Philip S. Deitz, Xinjin Zhao