Patents by Inventor Yanju LIU

Yanju LIU has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 10738163
    Abstract: A fast-response thermoplastic shape-memory polyimide and a preparation method thereof, related to a polyimide and a preparation method thereof. The present invention aims to solve the problem in high-temperature conditions of slow shape recovery poor stability, and poor mechanical properties of a shape-memory polymer prepared by utilizing an existing method. The structural formula of the polyamide of the present invention is as represented by formula (I). The preparation method is: 1. preparation of a diamine solution; 2. preparation of an anhydride-terminated high molecular weight polyamic acid; 3. preparation of a viscous sol-gel; and, 4. preparation of the thermoplastic shape-memory polyimide. The thermoplastic shape-memory polyimide prepared per the present invention is provided with a very fast shape recovery rate and improved shape-memory effect. The present invention is applicable in the field of polyimide preparation.
    Type: Grant
    Filed: November 19, 2018
    Date of Patent: August 11, 2020
    Assignee: Harbin Institute of Technology
    Inventors: Jingsong Leng, Xinli Xiao, Yanju Liu, Deyan Kong
  • Publication number: 20190085133
    Abstract: A fast-response thermoplastic shape-memory polyimide and a preparation method thereof, related to a polyimide and a preparation method thereof. The present invention aims to solve the problem in high-temperature conditions of slow shape recovery poor stability, and poor mechanical properties of a shape-memory polymer prepared by utilizing an existing method. The structural formula of the polyamide of the present invention is as represented by formula (I). The preparation method is: 1. preparation of a diamine solution; 2. preparation of an anhydride-terminated high molecular weight polyamic acid; 3. preparation of a viscous sol-gel; and, 4. preparation of the thermoplastic shape-memory polyimide. The thermoplastic shape-memory polyimide prepared per the present invention is provided with a very fast shape recovery rate and improved shape-memory effect. The present invention is applicable in the field of polyimide preparation.
    Type: Application
    Filed: November 19, 2018
    Publication date: March 21, 2019
    Applicant: Harbin Institute of Technology
    Inventors: Jingsong LENG, Xinli XIAO, Yanju LIU, Deyan KONG
  • Patent number: 10155850
    Abstract: A fast-response thermoplastic shape-memory polyimide and a preparation method thereof, related to a polyimide and a preparation method thereof. The present invention aims to solve the problem in high-temperature conditions of slow shape recovery poor stability, and poor mechanical properties of a shape-memory polymer prepared by utilizing an existing method. The structural formula of the polyamide of the present invention is as represented by formula (I). The preparation method is: 1. preparation of a diamine solution; 2. preparation of an anhydride-terminated high molecular weight polyamic acid; 3. preparation of a viscous sol-gel; and, 4. preparation of the thermoplastic shape-memory polyimide. The thermoplastic shape-memory polyimide prepared per the present invention is provided with a very fast shape recovery rate and improved shape-memory effect. The present invention is applicable in the field of polyimide preparation.
    Type: Grant
    Filed: January 7, 2015
    Date of Patent: December 18, 2018
    Assignee: Harbin Institute of Technology
    Inventors: Jingsong Leng, Xinli Xiao, Yanju Liu, Deyan Kong
  • Publication number: 20160369055
    Abstract: A fast-response thermoplastic shape-memory polyimide and a preparation method thereof, related to a polyimide and a preparation method thereof. The present invention aims to solve the problem in high-temperature conditions of slow shape recovery poor stability, and poor mechanical properties of a shape-memory polymer prepared by utilizing an existing method. The structural formula of the polyamide of the present invention is as represented by formula (I). The preparation method is: 1. preparation of a diamine solution; 2. preparation of an anhydride-terminated high molecular weight polyamic acid; 3. preparation of a viscous sol-gel; and, 4. preparation of the thermoplastic shape-memory polyimide. The thermoplastic shape-memory polyimide prepared per the present invention is provided with a very fast shape recovery rate and improved shape-memory effect. The present invention is applicable in the field of polyimide preparation.
    Type: Application
    Filed: January 7, 2015
    Publication date: December 22, 2016
    Applicant: HARBIN INSTITUTE OF TECHNOLOGY
    Inventors: Jingsong LENG, Xinli XIAO, Yanju LIU, Deyan KONG