  • Patent number: 9694450
    Abstract: A method for manufacturing a piston with a re-molten reinforced combustion chamber throat is provided. The manufacturing steps includes: a) piston rough machining: machining allowances of the combustion chamber throat and the combustion chamber bottom are 1-3 mm; b) piston washing and degreasing treatment; c) coating or spraying a surfactant on the combustion chamber throat and the combustion chamber bottom that need to be re-molten, wherein the surfactant formula comprises the components TiO2, SiO2, CuCl2 and MnCl2 that are mixed in percentage: 1-30% of TiO2, 1-30% of SiO2, 1-40% of CuCl2 and 1-50% of MnCl2; after the four components are uniformly mixed, a suspension is prepared by using acetone as a solvent a mass ratio of 1:(3-8); d) re-melting the piston by using an A-TIG welding method; and f) after re-melting, processing the piston into a finished product.
    Type: Grant
    Filed: January 29, 2015
    Date of Patent: July 4, 2017
    Assignee: SHANDONG BINZHOU BOHAI PISTON CO., LTD.
    Inventors: Zengjian Feng, Shiying Liu, Zihe Shang, Longchang Wang, Yanjun Li, Yanshou Cui, Yunxin Li, Xinghua Geng, Shili Wang, Zhaojie Pang, Tateoki Iizuka
  • Publication number: 20170165796
    Abstract: A method for manufacturing a piston with a re-molten reinforced combustion chamber throat is provided. The manufacturing steps includes: a) piston rough machining: machining allowances of the combustion chamber throat and the combustion chamber bottom are 1-3 mm; b) piston washing and degreasing treatment; c) coating or spraying a surfactant on the combustion chamber throat and the combustion chamber bottom that need to be re-molten, wherein the surfactant formula comprises the components TiO2, SiO2, CuCl2 and MnCl2 that are mixed in percentage: 1-30% of TiO2, 1-30% of SiO2, 1-40% of CuCl2 and 1-50% of MnCl2; after the four components are uniformly mixed, a suspension is prepared by using acetone as a solvent a mass ratio of 1: (3-8); d) re-melting the piston by using an A-TIG welding method; and f) after re-melting, processing the piston into a finished product.
    Type: Application
    Filed: January 29, 2015
    Publication date: June 15, 2017
    Applicant: SHANDONG BINZHOU BOHAI PISTON CO., LTD.
    Inventors: Zengjian FENG, Shiying LIU, Zihe SHANG, Longchang WANG, Yanjun LI, Yanshou CUI, Yunxin LI, Xinghua GENG, Shili WANG, Zhaojie PANG, Tateoki IIZUKA