  • Patent number: 7815757
    Abstract: The oxide film thickness of the steel material surface (dH2O+do2) is made to become 15 nm or less where post-treatment after water-cooling is not needed by suitably setting the conditions of the water-cooling start temperature (Ti), water-cooling end temperature (To), steel material thickness (d), concentration of solute oxygen in the cooling water (Do), and cooling rate (CR) in the equation of dH2O+do2=7.98×10?4(Ti?To)dDo+{5.50×10?3(Ti2?To2)?6.51(Ti?To)}/CR.
    Type: Grant
    Filed: April 5, 2006
    Date of Patent: October 19, 2010
    Assignees: Nippon Steel Corporation, Nippon Steel Engineering Co., Ltd.
    Inventors: Hisamoto Wakabayashi, Yasumitu Kondo, Tooru Akashi
  • Publication number: 20090038715
    Abstract: The oxide film thickness of the steel material surface (dH2O+do2) is made to become 15 nm or less where post-treatment after water-cooling is not needed by suitably setting the conditions of the water-cooling start temperature (Ti), water-cooling end temperature (To), steel material thickness (d), concentration of solute oxygen in the cooling water (Do), and cooling rate (CR) in the equation of dH2O+do2=7.98×10?4(Ti?To)dDo+{5.50×10?3(Ti2?To2)?6.51 (Ti?To)}/CR.