Patents by Inventor Yinping ZHONG

Yinping ZHONG has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 9631044
    Abstract: A method for preparing a comb-like polyurethane, including: 1) adding a diol to a reaction vessel, stirring, heating, vacuum dehydrating, and cooling the diol; adding a diisocyanate to the diol, and pre-polymerizing the diisocyanate and the diol under vacuum to yield a polyurethane prepolymer; 2) dissolving lysine in a mixture of water and an organic solvent to yield a first solution, adding the first solution to the polyurethane prepolymer to yield a first reaction mixture; stopping stirring and allowing the first reaction mixture to stand for between 10 and 12 hrs, pouring the first reaction mixture into water, and drying a precipitate to yield a polyurethane elastomer containing carboxyl groups; 3) dissolving the polyurethane elastomer in an organic solvent to yield a second solution; adding an epoxy-terminated polyethylene glycol to the second solution, and stirring a resulting mixture at between 110 and 130° C.
    Type: Grant
    Filed: October 12, 2015
    Date of Patent: April 25, 2017
    Assignees: SICHUAN UNIVERSITY, LAVAL UNIVERSITY
    Inventors: Xingyi Xie, Ze Zhang, Xiangyang Wu, Qiang Fu, Yinping Zhong
  • Publication number: 20160102167
    Abstract: A method for preparing a comb-like polyurethane, including: 1) adding a diol to a reaction vessel, stirring, heating, vacuum dehydrating, and cooling the diol; adding a diisocyanate to the diol, and pre-polymerizing the diisocyanate and the diol under vacuum to yield a polyurethane prepolymer; 2) dissolving lysine in a mixture of water and an organic solvent to yield a first solution, adding the first solution to the polyurethane prepolymer to yield a first reaction mixture; stopping stirring and allowing the first reaction mixture to stand for between 10 and 12 hrs, pouring the first reaction mixture into water, and drying a precipitate to yield a polyurethane elastomer containing carboxyl groups; 3) dissolving the polyurethane elastomer in an organic solvent to yield a second solution; adding an epoxy-terminated polyethylene glycol to the second solution, and stirring a resulting mixture at between 110 and 130° C.
    Type: Application
    Filed: October 12, 2015
    Publication date: April 14, 2016
    Inventors: Xingyi XIE, Ze ZHANG, Xiangyang WU, Qiang FU, Yinping ZHONG