Patents by Inventor Yoshimichi Daijyo

Yoshimichi Daijyo has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 8286900
    Abstract: A method of estimating the hydration reactivity of coal ash with high precision and determining the amount of milling water for obtaining a milling product in funicular form at the stage of milling; and a molding method being free from the problem of adhesion to a pressurization board at the stage of molding after the milling. When any collected coal ash exhibits a corrected basicity ((CaO+Fe2O3+MgO)/SiO2 (weight ratio)) of 0.1 or higher and a reactivity index (corrected basicity/(R2O/Al2O3) (weight ratio)) of 10 or higher, the coal ash as a raw ash is transferred to raw ash silo (2). Otherwise, the coal ash is transferred to waste ash silo (3). The raw ash within the raw ash silo (2) is poured in mill (8), and lime and gypsum are added and further milling water is charged thereto and milled.
    Type: Grant
    Filed: October 25, 2007
    Date of Patent: October 16, 2012
    Assignees: Kawasaki Plant Systems Kabushiki Kaisha, Japan Coal Energy Center, Kawasaki Jukogyo Kabushiki Kaisha
    Inventors: Noboru Takikawa, Yasunori Shibata, Atsushi Kondo, Tamaki Sakurai, Yoshiteru Kato, Kozo Kuga, Tomokazu Tengan, Tatsuya Ishihara, Atsushi Chinen, Yoshimichi Daijyo, Noboru Yasuda, Masahiko Doi
  • Publication number: 20100108788
    Abstract: A method of estimating the hydration reactivity of coal ash with high precision and determining the amount of milling water for obtaining a milling product in funicular form at the stage of milling; and a molding method being free from the problem of adhesion to a pressurization board at the stage of molding after the milling. When any collected coal ash exhibits a corrected basicity ((CaO+Fe2O3+MgO)/SiO2 (weight ratio)) of 0.1 or higher and a reactivity index (corrected basicity/(R2O/Al2O3) (weight ratio)) of 10 or higher, the coal ash as a raw ash is transferred to raw ash silo (2). Otherwise, the coal ash is transferred to waste ash silo (3). The raw ash within the raw ash silo (2) is poured in mill (8), and lime and gypsum are added and further milling water is charged thereto and milled.
    Type: Application
    Filed: October 25, 2007
    Publication date: May 6, 2010
    Applicant: Kawasaki Plant Systems Kabushiki Kaisha
    Inventors: Noboru Takikawa, Yasunori Shibata, Atsushi Kondo, Tamaki Sakurai, Yoshiteru Kato, Kozo Kuga, Tomokazu Tengan, Tatsuya Ishihara, Atsushi Chinen, Yoshimichi Daijyo, Noboru Yasuda, Masahiko Doi