Patents by Inventor Yu Qing Guo

Yu Qing Guo has filed for patents to protect the following inventions. This listing includes patent applications that are pending as well as patents that have already been granted by the United States Patent and Trademark Office (USPTO).

  • Patent number: 6455615
    Abstract: This invention provides a flexible polymer modified waterproofing cement material which can be used on a substrate or in concealed areas of construction engineering, water conservancy projects, municipal works, and its making process. The waterproofing material is made by kneading a hydraulic cement, a polymer dispersion, a water-soluble polymer or re-dispersible resin and water at a weight ratio of cement/polymer of about 100:15 to about 100:150 under conditions of about 25° C. to about 120° C., about 20 rpm to about 80 rpm until the water content of the kneaded materials reaches about 5% to about 20%. The kneaded material is mixed with a toughening polymer at a weight ratio of about 100:10 to about 100:50, then is calendered into sheets. These materials can adhere to dry or wet substrates firmly. They can be used in cold or hot and wet climate areas. After application, the waterproofing structure formed can bear retractive stress and deformation of the base or can resist outer impact.
    Type: Grant
    Filed: January 12, 2001
    Date of Patent: September 24, 2002
    Assignee: Tianjin Building Materials Science Research Institute
    Inventors: Ji Guang Yu, Dong Xia, Lei Zhu, Yu Qing Guo, Peng Chen
  • Publication number: 20010008910
    Abstract: This invention provides a flexible polymer modified waterproofing cement material which can be used on a substrate or in concealed areas of construction engineering, water conservancy projects, municipal works, and its making process. The waterproofing material is made by kneading a hydraulic cement, a polymer dispersion, a water-soluble polymer or re-dispersible resin and water at a weight ratio of cement/polymer of about 100:15 to about 100:150 under conditions of about 25° C. to about 120° C., about 20 rpm to about 80 rpm until the water content of the kneaded materials reaches about 5% to about 20%. The kneaded material is mixed with a toughening polymer at a weight ratio of about 100:10 to about 100:50, then is calendered into sheets. These materials can adhere to dry or wet substrates firmly. They can be used in cold or hot and wet climate areas. After application, the waterproofing structure formed can bear retractive stress and deformation of the base or can resist outer impact.
    Type: Application
    Filed: January 12, 2001
    Publication date: July 19, 2001
    Applicant: Tianjin Building Materials Science Research Institute
    Inventors: Ji Guang Yu, Dong Xia, Lei Zhu, Yu Qing Guo, Peng Chen