  • Patent number: 10480043
    Abstract: A seamless steel pipe for line pipe has a chemical composition consisting, by mass percent, of C: 0.03-0.15%, Si: ?0.50%, Mn: 1.0-2.0%, P: ?0.050%, S: ?0.005%, Cr: 0.1-1.0%, Al: 0.001-0.10%, N: ?0.01%, Ni: 0.05-2.0%, B: 0.0003-0.0015%, Ca: 0.0002-0.0050%, Mo: 0.10-0.50%, Ti: 0.001-0.05%, Cu: 0-2.0%, Nb: 0-0.05%, V: 0-0.10%, the balance: Fe and impurities, and satisfying the conditions of 2Nb+4V+Mo?0.50, wherein a metal micro-structure of the steel pipe contains 50% or more of bainite, in an area fraction, a wall thickness of the steel pipe is 25 mm or larger, and in a scale formed on the surface of the steel pipe, metal particles consisting mainly of Ni or Cu having an average circle-equivalent diameter of 0.1-5 mm exist. A distance from a boundary between the base metal of the steel pipe and the scale to a region in which the metal particles do not exist is 20 mm or longer.
    Type: Grant
    Filed: May 12, 2015
    Date of Patent: November 19, 2019
    Assignee: NIPPON STEEL CORPORATION
    Inventors: Yuji Arai, Yukimasa Ueda
  • Patent number: 10392675
    Abstract: There is provided a seamless steel pipe having high strength and high toughness even if having a thick wall. A seamless steel pipe according to the present embodiment consists of: in mass %, C: 0.03 to 0.08%, Si: not more than 0.25%, Mn: 0.3 to 2.0%, P: not more than 0.05%, S: not more than 0.005%, Al: 0.001 to 0.10%, Cr: 0.02 to 1.0%, Ni: 0.02 to 1.0%, Mo: 0.02 to 0.8%, N: 0.002 to 0.008%, Ca: 0.0005 to 0.005%, and Nb: 0.01 to 0.1%, the balance being Fe and impurities, and has a wall thickness of not less than 50 mm.
    Type: Grant
    Filed: April 10, 2013
    Date of Patent: August 27, 2019
    Assignee: NIPPON STEEL CORPORATION
    Inventors: Yukimasa Ueda, Yuji Arai
  • Patent number: 9651175
    Abstract: There is provided a seamless steel pipe for line pipe, wherein a chemical composition consists, by mass percent, of C: 0.03-0.10%, Si: ?0.50%, Mn: 1.0-2.0%, P: ?0.050%, S: ?0.005%, Cr: 0.05-1.0%, Mo: 0.01-0.30%, Al: 0.001-0.10%, N: ?0.01%, Ni: 0.04-2.0%, Ca: 0.0005-0.0050%, Cu: 0-2.0%, Ti: 0-0.05%, Nb: 0-0.05%, V: 0-0.10%, the balance: Fe and impurities, and satisfies the conditions of Cu+Ni: ?0.10%, and Mo+V: ?0.30%, wherein in a scale formed on the surface of the steel pipe, metal particles consisting mainly of Ni or Cu having an average circle-equivalent diameter of 0.1-5 ?m exist, and a distance from a boundary between the base metal of the steel pipe and the scale to a region in which the metal particles do not exist is 20 ?m or longer.
    Type: Grant
    Filed: June 13, 2014
    Date of Patent: May 16, 2017
    Assignee: NIPPON STEEL & SUMITOMO METAL CORPORATION
    Inventors: Yuji Arai, Yukimasa Ueda, Kei Murata, Yasuyoshi Hidaka
  • Publication number: 20170067129
    Abstract: A seamless steel pipe for line pipe has a chemical composition consisting, by mass percent, of C: 0.03-0.15%, Si: ?0.50%, Mn: 1.0-2.0%, P: ?0.050%, S: ?0.005%, Cr: 0.1-1.0%, Al: 0.001-0.10%, N: ?0.01%, Ni: 0.05-2.0%, B: 0.0003-0.0015%, Ca: 0.0002-0.0050%, Mo: 0.10-0.50%, Ti: 0.001-0.05%, Cu: 0-2.0%, Nb: 0-0.05%, V: 0-0.10%, the balance: Fe and impurities, and satisfying the conditions of 2Nb+4V+Mo?0.50, wherein a metal micro-structure of the steel pipe contains 50% or more of bainite, in an area fraction, a wall thickness of the steel pipe is 25 mm or larger, and in a scale formed on the surface of the steel pipe, metal particles consisting mainly of Ni or Cu having an average circle-equivalent diameter of 0.1-5 mm exist. A distance from a boundary between the base metal of the steel pipe and the scale to a region in which the metal particles do not exist is 20 mm or longer.
    Type: Application
    Filed: May 12, 2015
    Publication date: March 9, 2017
    Inventors: Yuji Arai, Yukimasa Ueda
  • Publication number: 20160161028
    Abstract: There is provided a seamless steel pipe for line pipe, wherein a chemical composition consists, by mass percent, of C: 0.03-0.10%, Si: ?0.50%, Mn: 1.0-2.0%, P: ?0.050%, S: ?0.005%, Cr: 0.05-1.0%, Mo: 0.01-0.30%, Al: 0.001-0.10%, N: ?0.01%, Ni: 0.04-2.0%, Ca: 0.0005-0.0050%, Cu: 0-2.0%, Ti: 0-0.05%, Nb: 0-0.05%, V: 0-0.10%, the balance: Fe and impurities, and satisfies the conditions of Cu+Ni: ?0.10%, and Mo+V: ?0.30%, wherein in a scale formed on the surface of the steel pipe, metal particles consisting mainly of Ni or Cu having an average circle-equivalent diameter of 0.1-5 ?m exist, and a distance from a boundary between the base metal of the steel pipe and the scale to a region in which the metal particles do not exist is 20 ?m or longer.
    Type: Application
    Filed: June 13, 2014
    Publication date: June 9, 2016
    Inventors: Yuji ARAI, Yukimasa UEDA, Kei MURATA, Yasuyoshi HIDAKA
  • Publication number: 20150083282
    Abstract: There is provided a seamless steel pipe having high strength and high toughness even if having a thick wall. A seamless steel pipe according to the present embodiment consists of: in mass %, C: 0.03 to 0.08%, Si: not more than 0.25%, Mn: 0.3 to 2.0%, P: not more than 0.05%, S: not more than 0.005%, Al: 0.001 to 0.10%, Cr: 0.02 to 1.0%, Ni: 0.02 to 1.0%, Mo: 0.02 to 0.8%, N: 0.002 to 0.008%, Ca: 0.0005 to 0.005%, and Nb: 0.01 to 0.1%, the balance being Fe and impurities, and has a wall thickness of not less than 50 mm.
    Type: Application
    Filed: April 10, 2013
    Publication date: March 26, 2015
    Inventors: Yukimasa Ueda, Yuji Arai