  • Patent number: 10377728
    Abstract: A preparation method of an acidic and hydrophobic Pd/C catalytic material comprises performing a simple treatment with chlorosulfonic acid and trimethylchlorosilane, washing and drying a treatment product to obtain a modified Pd/C catalytic material. A method for preparing 2,5-methylfuran by catalyzing a carbohydrate with modified Pd/C comprises: dissolving the carbohydrate in alcohol, allowing a reaction to proceed with modified Pd/C as a catalyst and polymethylhydrosiloxane as a hydrogen donor at a temperature of 80˜140° C. for 1-5 hours, and performing centrifugation to separate the catalyst from the product. The content of the modified Pd/C content is 1-3 mol % relative to the carbohydrate; the polymethylhydrosiloxane amount is equivalent to 4-10 times the carbohydrate amount, and the carbohydrate concentration in the alcohol is 2-6 wt %.
    Type: Grant
    Filed: October 12, 2017
    Date of Patent: August 13, 2019
    Assignee: GUIZHOU UNIVERSITY
    Inventors: Li Hu, Yang Song, Zhao Wenfeng, Xue Wei, Fang Zhen
  • Publication number: 20190152936
    Abstract: A preparation method of an acidic and hydrophobic Pd/C catalytic material comprises performing a simple treatment with chlorosulfonic acid and trimethylchlorosilane, washing and drying a treatment product to obtain a modified Pd/C catalytic material. A method for preparing 2,5-methylfuran by catalyzing a carbohydrate with modified Pd/C comprises: dissolving the carbohydrate in alcohol, allowing a reaction to proceed with modified Pd/C as a catalyst and polymethylhydrosiloxane as a hydrogen donor at a temperature of 80˜140° C. for 1-5 hours, and performing centrifugation to separate the catalyst from the product. The content of the modified Pd/C content is 1-3 mol % relative to the carbohydrate; the polymethylhydrosiloxane amount is equivalent to 4-10 times the carbohydrate amount, and the carbohydrate concentration in the alcohol is 2-6 wt %.
    Type: Application
    Filed: October 12, 2017
    Publication date: May 23, 2019
    Applicant: Guizhou University
    Inventors: Li Hu, Yang Song, Zhao Wenfeng, Xue Wei, Fang Zhen