ANTIMICROBIAL COLLOIDAL SILVER PRODUCTS AND METHOD OF MAKING SAME
Gelatinous materials combined with the Colloidal Silver additive to formulate an antimicrobial product having cushioning properties. Embodiments of the present invention can include gelatinous materials selected from a group consisting of thermosetting polymer, Styrene-Ethylene-Butadiene-Styrene polymer (SEBS), Thermoplastic Elastomer (TPE), and Polyurethane (PU) gelatin with and without a raised geometry on an outer surface.
Latest Eco Product Group LLC Patents:
- ANTIMICROBIAL COLLOIDAL SILVER PRODUCTS AND METHOD OF MAKING SAME
- Antimicrobial colloidal silver products and method of making same
- ANTIMICROBIAL COLLOIDAL SILVER PRODUCTS AND METHOD OF MAKING SAME
- ANTIMICROBIAL COLLOIDAL SILVER PRODUCTS AND METHOD OF MAKING SAME
- Antimicrobial colloidal silver products and method of making same
The present invention is a Continuation of U.S. Divisional patent application Ser. No. 15/936,574, filed Mar. 27, 2018, which claims the benefit of U.S. Continuation patent application Ser. No. 14/583,975, filed Dec. 29, 2014, which claims the benefit of U.S. Non-Provisional application Ser. No. 13/151,937, filed Jun. 2, 2011, which claims the benefit of U.S. Provisional Application Ser. No. 61/350,626, filed on Jun. 2, 2010, all are incorporated herein by reference.
FIELD OF THE INVENTIONThe present invention is related generally to the field of antimicrobial products, and in particular antimicrobial colloidal silver products.
BACKGROUND OF THE INVENTIONTraditionally, TPE Gels (Thermoplastic Elastomers) are developed by the hydrogenation of tri-block co-polymers of styrene and butadene. The present invention formulation allows for the glass transition of its rubber block below −50° C. thus maintaining its rubbery properties. This material content gel is made up of visco-elastic properties that are transformed into a gelatinous mass. The Tri-Block Co-Polymer, for example, uses mineral oil as a plasticizer. The Styrene-Ethylene-Butadiene-Styrene polymer (SEBS) description then becomes styrene and ethylene-butylene, and mineral oil is used for the modification of viscosity, and flexibility and strength of blends. The major applications for this type of gel have been for sealants, adhesives, coatings, footwear, athletic equipment, and other cushioning parts.
SUMMARY OF THE INVENTIONGenerally, the present invention includes gelatinous materials combined with the Colloidal Silver additive to formulate an antimicrobial product having cushioning properties. Embodiments of the present invention can include gelatinous materials selected from a group consisting of thermosetting polymer, Styrene-Ethylene-Butadiene-Styrene polymer (SEBS), Thermoplastic Elastomer (TPE), and Polyurethane (PU) gelatin with and without a raised geometry on an outer surface.
For a better understanding of the present invention, together with other and further objects thereof, reference is made to the accompanying drawings and detailed description.
The present invention is illustratively shown and described in reference to the accompanying drawings, in which:
As used herein in the specification and claims, including as used in the examples and unless otherwise expressly specified, all numbers may be read as if prefaced by the word “about”, even if the term does not expressly appear. Also, any numerical range recited herein is intended to include all sub-ranges subsumed therein.
The phrase “cross-linked network” means the one polymer chain is linked or bonded to another polymer chain.
The phrase “monolithic structure” means a solid, single part and not an assembly of two or more components.
The phrase “comprehensively suspended colloidal silver” means silver particulates are suspended evenly throughout the gel material or suspended unevenly but along a target surface, such as the outer surface, of the gel material, both of which provides sufficient antimicrobial protection for its intended purpose.
One embodiment of the present invention comprises a gelatinous material with a colloidal silver additive suspended substantially evenly within the gelatin material. The gelatinous material can either be a thermosetting polymer, Styrene-Ethylene-Butadiene-Styrene polymer (SEBS), Thermoplastic Elastomer (TPE), or Polyurethane (PU) gelatin. The thermo-reversible solid material is composed of a liquid organic phased entrapped in a three-dimensionally cross-linked network. The solubility of the liquid organic can add elasticity to a product creating a jelly-like substance or gelatinous material. The combination of organic material plus SEBS material creates a thermoplastic elastomer. The polymers will be used in a final form in hardness and softness ranging from 0 to 40 on the shore A scale and harder consistencies on the Shore DD Scale from 0 to 80. The range of the TPE Gels will be from 0 to 40 on the 00 scale of measurement (Durometer). For the purpose of illustration, one embodiment of the gelatinous material is:
Substance A: Polymeric Methylene diphenyl di-isocyanate (MDI) 100%;
Substance B: 265 Molecular weight (Mw) polyether triol 100%;
Ratio A:B about 1:1; and
Shore D about 80.
One method of preparing the present invention, illustrated in
The prefabricated forms are allowed to set-up or air dry with very little pressure in order to derive the cast parts. The process of pouring the gelatinous material at ambient pressure conditions (1 atmosphere) and air casting is contrary to the conventional method of injection molding the gelatinous material under pressure conditions (above 1 atmosphere).
The next step is to mix the Colloidal silver additive in liquid or powder form into the gelatinous material in the cast prior to the first melt stage. Thusly, the colloidal silver is dispersed into part A and B of the A/B gelatinous material.
As stated above, the gelatinous material and Colloidal silver additive are combined to form a gelatinous mixture through a cast/pouring method. The gelatinous mixture in the cast is heated to a predetermined temperature ranging from about 300 degrees F. to up to the boiling point of the gelatinous material, and poured into prefabricated forms that are in the shape of the products to be derived from the casting of the materials.
In one embodiment of the gelatinous material in pellet form, the Colloidal silver additive is suspended simultaneously with the pellets, heated about 300° F., and poured into the prefabricated forms under ambient pressures conditions (1 atmosphere) and not under pressure (above 1 atmosphere) as.
The resultant material derived from either process will be a gelatinous material with comprehensively suspended colloidal silver throughout the gelatinous material. The final shape of the gelatinous material can take many forms, examples of which are provided below. However, the scope of the present invention is not to be limited to the examples provided herein.
One embodiment of the present invention is illustrated in
Another embodiment of the present invention is an exercise roller 38 illustrated in
Yet another embodiment of the present invention is a monolithic exercise roller 54 without a diameter through a longitudinal axis L of the product illustrated in
Yet another embodiment of the present invention is a monolithic exercise roller 54 illustrated in
Examples of flat mat 2 can have total lengths defined as the sum of top surface cutout length 24, bottom surface cutout length 28, and semi-circular projection portion length 46 about 18 inches to about 26 inches. Flat mat 2 can have widths about 14 inches to about 40 inches. However, lengths and widths longer or shorter are acceptable.
Examples of the exercise rollers 38, 54 can have lengths about 14 inches to about 40 inches and diameters about 6 inches to about 8 inches. However, lengths longer or shorter and diameters larger or smaller are acceptable.
Yet another antimicrobial colloidal silver product according to the present invention is a shoe insert (not shown).
Alternative embodiments of the present invention for all products can be capability of generating heating. The products can be microwaveable or include induction heating elements power by AC or DC sources. The induction heating elements can either be embedded within the gel material of the formed product (
Further alternative embodiments of the present invention for all products can be capable of being cooled to greater than the freezing point of the gel material such that the properties of malleability and cushioning are still present. The freezing point ranges depends on the composition of the gel material. The product can be place in the refrigerator or freezer to achieve the desired cooling temperature.
While the disclosure has been described in detail and with reference to specific embodiments thereof, it will be apparent to one skilled in the art that various changes and modifications can be made therein without departing from the spirit and scope of the embodiments. Thus, it is intended that the present disclosure cover the modifications and variations of this disclosure provided they come within the scope of the appended claims and their equivalents.
Claims
1. A product of the process comprising the steps of: wherein the gelatinous material is a mixture of Substance A and Substance B at a ratio of A:B about 1:1, wherein Substance A is Polymeric Methylene diphenyl di-isocyanate (MDI) 100% and Substance B is 265 Molecular weight (Mw) polyether triol 100%; and wherein the product is a flat mat.
- loading a gelatinous material into a cast;
- loading Colloidal Silver into the cast;
- heating the cast to a predetermined temperature to form a mixture with Colloidal Silver evenly dispersed in mixture;
- pouring heated mixture into a prefabricated form that are in the shape of the products to be derived from the casting of the materials;
- air cooling the prefabricated form; and
- removing the gel product with Colloidal Silver from the prefabricated form,
2. The product according to claim 1, wherein the mat has raised geometric projections on at least one surface of the mat.
3. The product according to claim 2, wherein the mat is an exercise mat.
4. The product according to claim 1, wherein the mat is rolled and joined at opposing ends to form a substantially circular roller.
5. The product according to claim 4, wherein the circular roller has raised geometric projections on the outer surface of the roller.
6. The product according to claim 4, wherein the mat is rolled around an insert.
7. The product according to claim 6, wherein the circular roller has raised geometric projections on the surface of the roller.
8. The product according to claim 1, wherein the mat is a shoe insert.
Type: Application
Filed: Jan 21, 2020
Publication Date: Jun 11, 2020
Applicant: Eco Product Group LLC (Pittsburgh, PA)
Inventor: Thomas P. Davis (Wexford, PA)
Application Number: 16/748,345