Abstract: Two-component adhesive-, sealing- or coating compositions are being described which are separately packed, and comprise the component A and the component D, whereby the component A is curing as soon as it gets in touch with water or the component D which contains the curing agent for the component A.The component D can be, or a component B containing an ingredient which is curing at the contact of water, or, possibly, at the contact with the component A, orthe component D can also be a mixture of solid matter and a volatile ingredient which is causing the cross-linking of the component A.The advantage of the novel two-component systems is that the component D is working as a curing agent for the component A, however, a surplus thereof is, or self-curing, or it does not leave a nuissance residue in the cured composition.
Type:
Grant
Filed:
December 6, 1996
Date of Patent:
April 13, 1999
Assignee:
Sika AG, vorm. Kaspar Winkler & Co.
Inventors:
Peter Merz, Norman E. Blank, Hans-Peter Tschan, Reinhard Ernst Wappmann, Lutz Zabel
Abstract: A binder producible by reaction of aromatic polyesters with polyols and fatty acid esters as well as a process for the production of such a binder are described.The inventive binder is particularly suitable for the production of polyurethanes and results in floor coverings with especially favorable properties.
Type:
Grant
Filed:
March 26, 1997
Date of Patent:
March 2, 1999
Assignee:
Sika AG vorm. kaspar Winkler & Co.
Inventors:
Ulrich Gerber, Paul Schelbert, Werner Meyer
Abstract: Novel water-soluble linear copolymers of vinylacetate with monomeric addition products of amines, amino acids, amino groups containing aromatic sulfonic acids, amino alcohols of maleic anthydride. The copolymers are useful as fluidizers in water containing solid matter suspensions.
Abstract: The invention relates to a setting- and hardening-accelerator for hydraulic binders containing at least a nitrate- or sulfite component, at least a thio-cyanate component, at least an alkanolamine component and at least a carboxylic acid component, as well as a method of setting- and hardening-acceleration of hydraulic binders or mixtures containing hydraulic binders.
Type:
Grant
Filed:
March 2, 1995
Date of Patent:
February 25, 1997
Assignee:
Sika Ag, vorm. Kaspar Winkler & Co.
Inventors:
Theodor A. Buerge, Urs Maeder, Franz Wombacher, Beat Marazzani
Abstract: In a process for accelerating the setting and hardening of a material which contains a hydraulic binder or which consists of a hydraulic binder there is used a setting accelerator mixture which is free of alkali metals and free of chlorides. Said setting accelerating mixture contains at least one water soluble sulfate of a polyvalent cation and a further constituent which is selected from the group consisting of calcium aluminate, calcium sulfoaluminate, basic aluminum salts, mixtures thereof or mixtures containing at least one of said constituents and a further component. If the water soluble sulfate of the polyvalent cation is aluminum sulfate, then said compound has to contain crystal water in order to provide the water solubility of said product.
Type:
Grant
Filed:
December 6, 1994
Date of Patent:
October 1, 1996
Assignee:
Sika AG, vorm. Kaspar Winkler & Co.
Inventors:
Theodor A. B urge, Klemens B osch, Dieter Mai
Abstract: A curing agent for aqueous epoxy resin emulsions comprising 10-80% by weight of at least one emulsifier, 1-80% by weight of at least one coemulsifier, and 5-80% by weight of at least one bis(diamine)-diepoxide adduct. Optionally, the curing agent contains 0-80% by weight of a diamine or a mixture of two or more diamines.
Abstract: There is described a thixotroping and set accelerating additive for mixtures which contain as component a hydraulic binder and/or a latent-hydraulic binder and furthermore water and optionally also an aggregate and/or other additives. The inventive thixotroping and set accelerating additive consists of one or more esters of the carbonic acid or said additive is a mixture which has a pH-value of not more than 8.0, preferably not more than 7.5 and contains as component at least one of said carbonic acid esters.Optionally the inventive additives can comprise further components which frequently are added to materials containing a hydraulic binder in order to improve the workability and/or the properties of the final building material, like concrete plasticizers, concrete super-plasticizers, set retarding agents, set accelerating agents, air entraining agents and optionally further thixotroping agents and mixtures of two or more such additives.
Type:
Grant
Filed:
December 16, 1993
Date of Patent:
September 26, 1995
Assignee:
Sika AG, vorm. Kaspar Winkler & Co.
Inventors:
Theodor A. Burge, Urs Mader, Ueli Sulser, Franz Wombacher
Abstract: Admixtures for spray concrete or mortar which contain silicic acid sol or consist of it, are used for the processing of spray concrete or mortar according to the dry or the wet method. Said admixtures lead to a clear reduction of dust formation and of rebound. With the processing of spray concrete or mortar the addition of the inventive admixtures takes place preferably during the spraying, for example at the spray nozzle.
Type:
Grant
Filed:
June 19, 1992
Date of Patent:
February 14, 1995
Assignee:
Sika AG vorm. Kaspar Winkler & Co.
Inventors:
Theodor A. Burge, Gustav Bracher, Dieter Mai
Abstract: A curing agent for aqueous epoxy resin emulsions is described, which curing agent contains 10-80% by weight of at least one emulsifier, 1-80% by weight of at least one coemulsifier, and 5-80% by weight of at least one bis(diamine)-diepoxide adduct. Optionally, the curing agent furthermore contains 0-80% by weight of a diamine or a mixture of two or more diamines. Said curing agent has the ability of forming microemulsions when water is added, preferably non-ionic oil-in-water microemulsions. Said microemulsions have a good shelf life. They are useful as curing agent for any desired aqueous epoxy resin dispersions, and they can also be used as curing agent in compositions based on epoxy resin and cement mortar.
Abstract: A reactive, after cooling still viscous-plastic moldable hot-melt adhesive contains a mixture ofat least one thermoplastic material,at least one binder on isocyanate basis, andat least one thixotropic agent,and the isocyanate content, referred to the total of the hot-melt adhesive, is in the range from 0.01 to 10 percent by weight.
Type:
Grant
Filed:
November 19, 1993
Date of Patent:
August 30, 1994
Assignee:
Sika AG, vorm. Kaspar Winkler & Co.
Inventors:
Peter W. Merz, Lutz Zabel, Christian Fischer
Abstract: A method for the start up of a concrete pump using a small amount of an aqueous suspension of polymers, amorphous silicone dioxide and water-reducer rather than a conventional cement slurry.
Abstract: Disclosed is a glass body suitable for cementing to a further material. At the time of cementing, there is at least one profile of a cement on the glass body, and it is already solidified at the time of cementing and serves as a range spacer. Furthermore, there is a profile of a second cement on the glass body which cement is still moldable and has adhesive characteristics at the time of cementing. When producing the adhesive connection, the second cement is formed and pressed against the other material. Because the profile of the second, still adhesive cement is directly on the glass body or possibly a layer of a material impermeable to ultraviolet or, where necessary, an intermediate layer of primer, a very good adhesion can be achieved.
Abstract: Disclosed is a highly reactive hydraulic binder for the preparation of building, construction and raw materials which contains burned oil shale and at least one compound, selected from the group, consisting ofan amorphous oxide of 3- and/or 4-valent cations,an amorphous hydroxide of 3- and/or 4-valent cations, andan aluminate of 1- and/or 2-valent cations, as well asat least one water reducing agent.
Abstract: Novel water-soluble linear copolymers of N-vinylamides with monomeric addition products of amines, amino acids, amino groups containing aromatic sulfonic acids, amino alcohols of maleic anhydride as well as maleic esters of polyoxyalkyleneglycols or their monoethers. There is also described the process for the preparation of these copolymers. The copolymers are useful as fluidizers in water containing solid matter suspensions.
Type:
Grant
Filed:
May 16, 1990
Date of Patent:
March 31, 1992
Assignee:
Sika AG vorm. Kaspar Winkler & Co.
Inventors:
Theodor A. Burge, Jurg Widmer, Irene Schober, Ueli Sulser
Abstract: A thixotropic hot-melt adhesive contains reactive silane groups and is still viscous and plastically moldable after cooling. It contains a mixture ofat least one thermoplastic material, andat least one thixotropic agent,wherein silane groups are contained either in the thermoplastic material itself or in at least one added silane-based binder.
Abstract: A one-component adhesive and/or sealing mass which is stable and pumpable at temperatures up to 30.degree. C. containsat least one prepolymer on the basis of a polyurethane, which contains from 0.1 to 15 percent by weight, referred to the prepolymer, of free, reactive isocyanate groups, andat least one with heat activatable hardener.Thereby the stoichiometric ratio between said prepolymer and said hardener is chosen in such a way that only a partial cross-linkage is possible during heating said mass to temperatures from 60.degree. C. to 180.degree. C., and that a product is obtained having from high viscous to plastic characteristics.The inventive masses may be used for bonding and/or sealing of one or more materials of the same or different origin to a composite.
Abstract: A moisture curable composition contains:(a) one or more episulfide compounds having on the average more than one 1,2-epithiopropyl ether group of the formula I ##STR1## per molecule, and (b) one or more aliphatic N,N'-dialkyl-substituted diketimines of the general formula II ##STR2## wherein A is a divalent aliphatic, cycloaliphatic or arylaliphatic group, andR.sup.1 and R.sup.2 are each an alkyl group, or form together with the C-atom, to which they are bonded, a cycloalkyl group or cycloalkenyl group, and(c) at least one component, selected from the group of the setting accelerators as well as commercially available solvents, reactive diluents, plasticizers, thixotropic aids, fillers and pigments.This composition may be used as lacquers, paints and coatings for steel and concrete.There is also described a process for the preparation of 1,2-epithiopropyl ethers.
Abstract: For the preparation of a building and/or construction material a polymer modified, aqueous dispersion, containing amorphous silicon dioxide and at least one polymer, is mixed and reacted with at least one inorganic binder, and occasionally with at least one aggregate, and hardens thereby.The polymer modified, aqueous dispersion contains amorphous silicon dioxide and at least one polymer.This polymer modified, aqueous dispersion is used for the preparation of a building and/or construction material.
Abstract: For the acceleration of the setting and of the hardening of a hydraulic binding agent such as cement, limestone, hydraulic limestone and gypsum as well as mortar and concrete prepared thereof, are added to the mixture, which contains said binding agent, from 0.5 to 10 percent by weight, referred to the weight of this binding agent, of an alkali-free setting- and hardening-accelerator, whereby this accelerator contains aluminum hydroxide.
Abstract: Highly concentrated aqueous solutions of low viscosity of melamine/aldehyde resins are obtained by reacting to a precondensate in a first step melamine and an aldehyde in an alkaline medium and in the presence of water together with at least one compound (I), selected from the group, consisting of an alkali sulfite, an alkaline earth sulfite, an amino sulfonic acid, an amino carboxylic acid, a hydroxycarboxylic acid, a hydroxycarboxylic acid lactone, and a polyhydroxy carboxylic acid lactone, reacting then the thus obtained mixture in a second step with at least one compound (II), selected from the group, consisting of an amino carboxylic acid, a carboxylic acid, a hydroxy carboxylic acid, a hydroxy carboxylic acid lactone, a sulfamic acid, an amino sulfonic acid, a polyhydroxy carboxylic acid and a polyhydroxy carboxylic acid lactone, and then making alkaline the obtained resin solution by adding at least one basic compound (III).
Type:
Grant
Filed:
December 14, 1983
Date of Patent:
February 26, 1985
Assignee:
Sika AG, vorm. Kaspar Winkler & Co.
Inventors:
Theodor A. Burge, Jurg Widmer, Theodor Meyer, Ulrich Sulser