Patents Assigned to BASF
  • Publication number: 20130053534
    Abstract: A process for distilling an aqueous NPG mixture comprising NPG, a tertiary amine, water and the adduct of tertiary amine and formic acid (amine formate), said distillation being performed in a distillation column, which comprises drawing off a gaseous stream in the upper region of the column and feeding it to two condensers connected in series, the first condenser being operated in such a way that a portion of the gaseous stream is condensed in the first condenser and the second condenser being operated in such a way that the uncondensed portion of the gaseous stream is essentially fully condensed in the second condenser, the condensed stream from the first condenser being recycled fully or partly as reflux into the column.
    Type: Application
    Filed: August 17, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Helmut Kronemayer, Kai Stehmeier, Ralf Edinger, Stefan Rittinger, Michael Steiniger
  • Publication number: 20130053597
    Abstract: A process for preparing ethylenediaminediacetonitrile (EDDN) and/or ethylenediamine-monoacetonitrile (EDMN) by conversion of formaldehyde (FA), hydrogen cyanide (HCN) and ethylenediamine (EDA), which comprises using stabilizer-free HCN, or HCN which has been stabilized with an organic acid, in the process.
    Type: Application
    Filed: August 30, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Hermann Luyken, Sebastian Ahrens, Gordon Brasche, Jens Baldamus, Robert Baumann, Randolf Hugo, Stephanie Jaegli, Johann-Peter Melder, Jörg Pastre, Boris Buschhaus
  • Publication number: 20130052125
    Abstract: Molecular sieves, improved methods for their synthesis, and catalysts, systems and methods of using these molecular sieves as catalysts in a variety of processes such as abating pollutants in exhaust gases and conversion processes are described. The molecular sieves are made using a tailored colloid including an alumina source, a silica source and a structure directing agent.
    Type: Application
    Filed: August 23, 2012
    Publication date: February 28, 2013
    Applicant: BASF Corporation
    Inventors: Ahmad Moini, Saeed Alerasool, Subramanian Prasad
  • Publication number: 20130048240
    Abstract: Paper coating or binding formulations are provided that comprise aqueous copolymer emulsions including copolymers derived from one or more copolymerizable surfactants of formula I and one or more monomers. The paper coating or binding formulations can include one or more mineral fillers, coating pigments, or mixtures thereof, wherein the total weight concentration of the one or more mineral fillers, coating pigments, or mixtures thereof is 65% or higher, based on the total weight of the composition. Paper products coated with the paper coating or binding formulations, methods of making the paper coating or binding formulations, and methods of making the coated paper products are also disclosed.
    Type: Application
    Filed: March 21, 2011
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventor: Peter C. Hayes
  • Publication number: 20130052383
    Abstract: Cavity blocks contain a rigid polyurethane foam having a density in the range of 30-70 g/L in at least one chamber, the rigid polyurethane foam being obtained by reacting at least one polyisocyanate a) with at least one compound having at least two isocyanate-reactive hydrogen atoms b) in the presence of at least one catalyst d) and using at least one blowing agent c), comprising at least one blowing agent ci), which only develops its blowing effect at the time of the reaction of a) with b), and at least one blowing agent cii), which has a boiling point which is below the temperature at which said components a) and b) are mixed, wherein the pressure buildup during the foaming reaction of the polyurethane remains below 20 kPa, and the invention also relates to the corresponding process for producing the cavity blocks.
    Type: Application
    Filed: August 27, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventor: Peter WINTERMANN
  • Publication number: 20130052393
    Abstract: The invention relates to a vacuum insulation panel comprising a barrier film and a core material having a density in the range from 50 to 350 kg/m3, wherein the core material comprises a mixture of A) from 30 to 100 percent by weight of nanoporous polymer particles which have a cell count in the range from 1000 to 100 000 cells/mm, where at least 60 percent by weight of the nanoporous polymer particles have a particle size of less than 100 ?m in the sieve analysis in accordance with DIN 66165, and B) from 0 to 70 percent by weight of pyrogenic or precipitated silica, and also a process for the production thereof.
    Type: Application
    Filed: August 24, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Klaus Hahn, Elena Khazova, Jan Kurt Walter Sandler, Marc Fricke, Maria-Kristin Sommer, Roland Hingmann
  • Publication number: 20130053584
    Abstract: A process for reacting ethylenediamine-formaldehyde adduct (EDFA) and/or ethylene-diamine-monoformaldehyde adduct (EDMFA) with hydrogen cyanide (HCN) in a reactor with limited backmixing at a temperature in the range from 20 to 120° C., wherein the residence time in the reactor is 300 seconds or less.
    Type: Application
    Filed: August 30, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Hermann Luyken, Sebastian Ahrens, Gordon Brasche, Jens Baldamus, Robert Baumann, Randolf Hugo, Stephanie Jaegli, Johann-Peter Melder, Jörg Pastre, Boris Buschhaus
  • Publication number: 20130053535
    Abstract: The present invention relates to a process for producing moldings comprising (A) at least one lactam, (B) at least one activator, and (C) at least one catalyst, where (A) to (C) proceed through treatments comprising a) mixing of (A), (B), and (C), b) metering of (A), (B), and (C) into an apparatus for producing mixture droplets, and producing mixture droplets, and c) depositing the mixture droplets comprising (A), (B), and (C) on a belt, and d) producing moldings.
    Type: Application
    Filed: August 17, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Dietrich Scherzer, Philippe Desbois, Freddy Gruber, Achim Stammer
  • Publication number: 20130052444
    Abstract: The present invention relates to a process for producing moldings comprising (A) at least one lactam, (B) at least one activator, and (C) at least one catalyst, where (A) to (C) proceed through treatments comprising a) mixing of (A), (B), and (C), b) metering of (A), (B), and (C) into an apparatus for producing mixture droplets, and producing mixture droplets, and c) depositing the mixture droplets comprising (A), (B), and (C) on a belt, and d) producing moldings.
    Type: Application
    Filed: August 17, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Dietrich Scherzer, Philippe Desbois, Freddy Gruber, Achim Stammer
  • Publication number: 20130048137
    Abstract: The present invention relates to a process for producing insulated pipes, the use of a polyurethane system comprising an isocyanate component (a), a polyol mixture (b) and at least one catalyst for producing insulated pipes, wherein the cream time for the polyurethane system is less than the time for introduction of the polyurethane system into the pipe, the use of specific amines as catalyst in a polyurethane system for producing insulated pipes and also an insulated pipe which can be obtained by the process of the invention.
    Type: Application
    Filed: August 29, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Christof GRIESER-SCHMITZ, Gianpaolo Tomasi, Ludwig Windeler, Alex Popov, Carsten Ellersiek, Annika Halwe-Bommelmann
  • Publication number: 20130048570
    Abstract: Gravity sedimentation of a first aqueous suspension of solid particles in a vessel results in formation of a second aqueous suspension of solid particles in the present invention. The process involves adding at least one organic polymeric flocculant to the first aqueous suspension to form a suspension of flocculated solid. The flocculated solids settle to form a bed of consolidated solids. Introducing an effective amount of an agent into the bed of consolidated solids or into the flocculated solids that are settling leads to formation of the second aqueous suspension. The second aqueous suspension of solid particles has a higher solids content than the first aqueous suspension of solid particles. The agent is a free radical agent or an oxidizing agent.
    Type: Application
    Filed: April 8, 2011
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Paul Stocks, Ian John Flanagan, Gregor Brodt, Stephen Adkins
  • Publication number: 20130053540
    Abstract: A process for preparing TETA and/or DETA by the action of EDDN and/or EDMN with hydrogen in the presence of a catalyst, wherein the catalyst used is a catalyst of the Raney type and the pressure in the course of hydrogenation is in the range from 170 to 240 bar.
    Type: Application
    Filed: August 31, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Hermann Luyken, Sebastian Ahrens, Gordon Brasche, Jens Baldamus, Robert Baumann, Randolf Hugo, Stephanie Jaegli, Johann-Peter Melder, Jörg Pastre, Boris Buschhaus
  • Publication number: 20130053484
    Abstract: An intermediate of the formula (I) wherein the radicals R1 are independently of one another methyl, ethyl or n-propyl, is suitable for preparing a compound of the formula (A) wherein X is a group of the formula (A-I) or (A-II), Y is C11-C17alkyl, and Z is a direct bond, —(CH2)8— or —CH2—S—CH2—. The compounds of the formula (A) are useful for stabilizing an organic material against thermal, oxidative or light induced degradation.
    Type: Application
    Filed: March 2, 2011
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Hans-Rudolf Meier, Kai-Uwe Schoning, Shrirang Bhikaji Hindalekar
  • Publication number: 20130053582
    Abstract: ?-Hydroxycarboxylic esters and ?-lactones which are suitable as flavors can be prepared by electrochemical reductive cross-coupling of ?,?-unsaturated esters with carbonyl compounds in an undivided electrolysis cell having a cathode composed of lead, lead alloys, cadmium, cadmium alloys, mercury, steel, glassy carbon or boron-doped diamonds and a basic aqueous electrolyte comprising an electrolyte salt which suppresses the cathodic formation of hydrogen.
    Type: Application
    Filed: August 24, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Itamar Michael Malkowsky, Florian Stecker, Simone Lutter, Olivier Abillard, Ralf Pelzer
  • Publication number: 20130052469
    Abstract: Binder mixture comprising a hydroxyl-containing compound (A), and at least 1.0% by weight, based on the nonvolatile constituents of the binder mixture, of a phosphorus- and nitrogen-containing catalyst (D) for the crosslinking of silane groups, wherein the hydroxyl-containing compound (A) comprises a hydroxyl-functional polyester having on average at least one hydroxyl function of the polyester esterified with a C8 to C9 monocarboxylic acid, and the catalyst (D) is blocked with at least one tertiary amine of the formula (I) where R1 is an acyclic aliphatic or araliphatic hydrocarbon radical having at least 3 C atoms, R2 is an acyclic aliphatic or araliphatic hydrocarbon radical which is the same or different from R1 and/or R3, and R3 is hydrogen or an acyclic aliphatic or araliphatic hydrocarbon radical which is the same or different from R1 and/or R2.
    Type: Application
    Filed: August 3, 2010
    Publication date: February 28, 2013
    Applicant: BASF Coatings GmbH
    Inventors: Gunter Klein, Andreas Poppe, Sabine Holtschulte, Björn Feldmann, Ulrike Wenking, Karl-Heinz Joost
  • Publication number: 20130053537
    Abstract: A process for regenerating Raney catalysts by treating the catalyst with liquid ammonia with a water content of less than 5% by weight and with hydrogen having a partial pressure of 0.1 to 40 MPa in the temperature range from 50 to 350° C. for at least 0.1 hour.
    Type: Application
    Filed: August 30, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Hermann Luyken, Sebastian Ahrens, Gordon Brasche, Jens Baldamus, Robert Baumann, Randolf Hugo, Stephanie Jaegli, Johann-Peter Melder, Jörg Pastre, Boris Buschhaus
  • Publication number: 20130053296
    Abstract: The present invention relates to a solid with sufficiently low hygroscopicity which comprises glutamic acid-N,N-diacetic acid (GLDA) or derivatives and/or salts thereof, and a method for its production.
    Type: Application
    Filed: December 27, 2010
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventor: Andreas Baranyai
  • Publication number: 20130053538
    Abstract: A process for reacting ethylenediamine (EDA) with formaldehyde to give ethylenediamine-formaldehyde adduct (EDFA) and/or ethylenediamine-monoformaldehyde adduct (EDMFA), which comprises performing the reaction of FA with EDA at a temperature in the range from 20 to 70° C.
    Type: Application
    Filed: August 30, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Hermann Luyken, Sebastian Ahrens, Gordon Brasche, Jens Baldamus, Robert Baumann, Randolf Hugo, Stephanie Jaegli, Johann-Peter Melder, Jörg Pastre, Boris Buschhaus
  • Publication number: 20130049443
    Abstract: The invention relates to a wheel for a motor vehicle, comprising a wheel body (3) with a rim tape (7) for receiving a tire and also a rim star (9) or a wheel disk, through-openings (13) for fastening means for fastening the wheel on a nave on the motor vehicle being formed in the rim star (9) or in the wheel disk. The wheel (1) is produced from a polymer material and at least one reinforcing element (29;33) is accommodated in the rim tape (7) for reinforcement.
    Type: Application
    Filed: August 23, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Heiko HEß, Jörg Schnorr, Walter Rau, Sven Wenigmann
  • Publication number: 20130053536
    Abstract: A process for preparing EDDN and/or EDMN by a) conversion of FA, HCN and EDA, the conversion being effected in the presence of water, b) depleting water from the reaction mixture obtained in stage a), and c) treating the mixture from stage b) with an absorbent in the presence of an organic solvent, wherein the adsorbent is a solid acidic adsorbent.
    Type: Application
    Filed: August 30, 2012
    Publication date: February 28, 2013
    Applicant: BASF SE
    Inventors: Hermann Luyken, Sebastian Ahrens, Gordon Brasche, Jens Baldamus, Robert Baumann, Randolf Hugo, Stephanie Jaegli, Johann-Peter Melder, Jörg Pastre, Boris Buschhaus