  • Publication number: 20010032056
    Abstract: In a multi-axis machine tool (M) including an angular dividing head (HD) having a spindle head (9) mounted thereto, the positional correction includes determining an error representative vector componentwise representative of a plurality of positional errors with respect to a plurality of axes of the spindle head at a respective angular position dividable by the angular dividing head, and correcting an arbitrary positional error of the spindle head by calculating a component vector of the error representative vector associated with the respective angular position.
    Type: Application
    Filed: March 23, 2001
    Publication date: October 18, 2001
    Applicant: TOSHIBA KIKAI KABUSHIKI KAISHA
    Inventors: Tadashi Tanaka, Kazuo Nagashima
  • Patent number: 6176621
    Abstract: A rotary slide bearing part of a rotary slide slit bearing for supporting a rotary shaft thereon in a rotatable manner, has a first bearing surface portion adapted to be arranged adjacent to a second bearing surface portion of another rotary slide bearing part of the rotary slide slit bearing, a load from the shaft to be borne by the first bearing surface portion is larger than a load from the shaft to be borne by the second bearing surface portion, the first bearing surface portion includes a fluidal pressure generating surface facing close to the shaft to generate a fluidal pressure between the fluidal pressure generating surface and the shaft, a main groove arranged at an circumferential end of the first bearing surface portion adjacent to the second bearing surface portion, and a sub-groove extending from the main groove in a circumferential direction of the first bearing surface portion, and an axial width of the sub-groove is smaller than that of the main groove.
    Type: Grant
    Filed: July 2, 1998
    Date of Patent: January 23, 2001
    Assignee: Daido Metal Company Ltd.
    Inventors: Hiroshi Naitoh, Arihiro Kimura, Koji Kuroda, Hiroshi Murakami, Noriyoshi Ito, Tadashi Tanaka
  • Patent number: 5998339
    Abstract: A wet type sliding apparatus comprising a wet type radial bearing which starts in the presence of a lubricating liquid, wherein the radial bearing has a sliding surface consisting of a resin composition comprising 10 to 45% by weight of a carbon fiber and 0.1 to 8.5% by weight of a fluorocarbon polymer, the balance being substantially an aromatic polyetherketone resin or a polyarylene sulfide resin. The radial bearing in the above wet type sliding apparatus is excellent in wear resistance even under a high load.
    Type: Grant
    Filed: October 7, 1997
    Date of Patent: December 7, 1999
    Assignee: Daido Metal Company Ltd.
    Inventors: Eiji Kato, Shoji Yasunaga, Hidehiko Tamura, Tadashi Tanaka
  • Patent number: 5978595
    Abstract: A method of actively guiding and helping the user is disclosed, in which various supporting functions can be performed in accordance with a particular user situation. The method is equipped with user situation detection data having at least a user situation and a corresponding interaction pattern activated in such a user situation, supporting function select data having at least a user situation and a corresponding user supporting function name to be activated in the particular user situation, and at least one user supporting function. Each time an input is received from the user, the contents of the input are stored as an operation log data. The interaction pattern data of the user situation detection data is compared with the operation log data.
    Type: Grant
    Filed: September 26, 1997
    Date of Patent: November 2, 1999
    Assignee: Hitachi, Ltd.
    Inventors: Tadashi Tanaka, Mayumi Tamejima, Hirotaka Mizuno, Akihiko Koga, Yoji Taniguchi, Masahiko Ogawa
  • Patent number: 5920740
    Abstract: A development processing apparatus in which a photosensitive material is processed in processing solutions, and thereafter, the photosensitive material which has been processed in the processing solutions is subjected to drying processing by a dry air from a drying machine built in the development processing apparatus, comprising: a re-drying section which delivers the dry air from the drying machine to the outer side of the development processing apparatus; and photosensitive material holding means in which, in order to dry again the photosensitive material which has been subjected to drying processing by the dry air from the re-drying section, the photosensitive material which has been subjected to drying processing is held such that the surface of the photosensitive material which has been subjected to drying processing is substantially parallel to the direction of the dry air delivered from the re-drying section.
    Type: Grant
    Filed: March 13, 1998
    Date of Patent: July 6, 1999
    Assignee: Fuji Photo Film Co., Ltd.
    Inventor: Tadashi Tanaka
  • Patent number: 5911091
    Abstract: A method for processing photosensitive materials in which photosensitive materials are conveyed along a serial conveyance passage while guiding the photosensitive materials on both sides thereof by using pairs of guide members to successively perform development processing steps comprises the steps of dividing the conveyance passage into a plurality of blocks, a spacing distance between the pair of guide members on the conveyance passage being changeable in each of the divided blocks, and changing the spacing distance between the pair of guide members in each of the blocks, when a photosensitive material having a different widthwise dimension is introduced into the conveyance passage, in accordance with the widthwise dimension of the photosensitive material before introducing a forward end of the photosensitive material having the different widthwise dimension into each of the blocks.
    Type: Grant
    Filed: November 14, 1995
    Date of Patent: June 8, 1999
    Assignee: Fuji Photo Film Co., Ltd.
    Inventors: Nobuo Matsumoto, Tadashi Tanaka
  • Patent number: 5895516
    Abstract: A bearing alloy for high-temperature application essentially consisting of, by weight, 2 to 8% Cr, 2 to 10% Fe, 0.1 to 1.5% Si, 2 to 22% Co, 1.4 to 11% Mo, and the balance of Ni and unavoidable impurities, and having a structure in which hard particles of a Co--Mo--Cr--Si-system intermetallic compound are dispersed the matrix in the proportion of 5 to 35 weight percent to the matrix. The respective component of the intermetallic compound is also counted in the above alloy composition.
    Type: Grant
    Filed: July 25, 1996
    Date of Patent: April 20, 1999
    Assignee: Daido Metal Company Ltd.
    Inventors: Tadashi Tanaka, Masaaki Sakamoto, Koichi Yamamoto, Kouki Ozaki
  • Patent number: 5879791
    Abstract: A wet type sliding apparatus comprising a thrust bearing which operates in the presence of a lubricating liquid, wherein the thrust bearing has a sliding surface composed of a resin composition comprising a carbon fiber, a fluorocarbon polymer and a thermoplastic resin other than fluorocarbon polymer, the carbon fiber content being 10 to 45% by weight based on the weight of the composition and the fluorocarbon polymer content being 0.1 to 8.5% by weight based on the weight of the composition, the thrust bearing in said wet type sliding apparatus being excellent in wear resistance, mechanical strength and friction coefficient at the time of starting even under a high load.
    Type: Grant
    Filed: September 25, 1996
    Date of Patent: March 9, 1999
    Assignee: Daido Metal Company Ltd.
    Inventors: Eiji Kato, Shoji Yasunaga, Hidehiko Tamura, Tadashi Tanaka
  • Patent number: 5869536
    Abstract: A pharmaceutical composition for treating hyperkinetic disorders, which contains as an active ingredient an effective amount of 2-(4-methylamino butoxy)diphenylmethane, is provided. A method of treating hyperkinetic disorders with said pharmaceutical composition and use of said diphenylmethane for preparing said composition are also provided.
    Type: Grant
    Filed: July 11, 1995
    Date of Patent: February 9, 1999
    Assignee: Mitsubishi Chemical Corporation
    Inventors: Akihiro Tobe, Tadashi Tanaka, Tomoko Tamura
  • Patent number: 5846347
    Abstract: A multi-layered bearing having superior load-resistance comprises an aluminium base bearing alloy layer and a backing metal layer. The bearing alloy consists essentially of, by weight, 2-8% zinc, 0.1-8% silicon, 0.1-3% copper, 0.05-3% magnesium and the balance of aluminium. The bearing alloy is subjected to a solution treatment and an artificial aging treatment, and it has a hardness of Hv 70 or greater. The bearing alloy may contain at least one element selected from the following five elements of lead, manganese, vanadium, chromium and nickel, and may further contain strontium and/or titanium and boron. The hardness of the bearing alloy may be Hv 70 or higher by performing solution treatment on a bimetal at a temperature of 400.degree. C. or higher before the plastic working, and further by performing an artificial aging treatment thereon at a temperature of 250.degree. C. or lower.
    Type: Grant
    Filed: May 28, 1993
    Date of Patent: December 8, 1998
    Assignee: Daido Metal Company Ltd.
    Inventors: Tadashi Tanaka, Masaaki Sakamoto, Tohru Kato, Yoshiaki Sato
  • Patent number: 5834722
    Abstract: The improved method for treating waste gases by exposure to electron beams which comprises adding ammonia to a waste gas containing sulfur oxide (SO.sub.x) and/or nitrogen oxides (NO.sub.x) and thereafter exposing the gas to an electron beam so as to remove the sulfur oxides and/or nitrogen oxides therefrom is characterized by first mixing ammonia gas uniformly with air, then forming a homogeneous gas-liquid mixture from said gaseous mixture and water, and spraying said homogeneous mixture into a reactor. Efficient desulfurization can be realized even if the temperature of the waste gas being treated is fairly high at the exit of the reactor and the concentration of ammonium sulfamate in the by-product ammonium sulfate can be reduced.
    Type: Grant
    Filed: November 30, 1995
    Date of Patent: November 10, 1998
    Assignees: Ebara Corporation, Japan Atomic Energy Research Institute
    Inventors: Okihiro Tokunaga, Hideki Namba, Tadashi Tanaka, Yoshimi Ogura, Yoshitaka Doi, Masahiro Izutsu, Shinji Aoki
  • Patent number: 5780396
    Abstract: A sliding member excellent in cavitation resistance and friction properties which has a sliding surface composed of a resin composition comprising a tetrafluoroethylene-perfluoroalkyl vinyl ether copolymer resin and a polytetrafluoroethylene having a molecular weight of 5,000,000 to 15,000,000 and optionally a solid lubricant, wherein the proportion of the tetrafluoro-ethylene-perfluoroalkyl vinyl ether copolymer resin is 1 to 50% by volume based on the volume of the resin composition and the proportion of the solid lubricant is 0.5 to 10% by volume based on the volume of the resin composition. The addition of the solid lubricant results in an enhancement of friction properties and the use of an exfoliated graphite as the solid lubricant brings about a further enhancement of friction properties.
    Type: Grant
    Filed: January 23, 1996
    Date of Patent: July 14, 1998
    Assignee: Daido Metal Company Ltd.
    Inventors: Tadashi Tanaka, Hidehiko Tamura, Takahiro Niwa
  • Patent number: 5766777
    Abstract: A composite copper alloy bearing is provided with a backing metal layer, an intermediate layer of Cu--Pb alloy, and a surface layer of Al--Sn alloy. A thickness of the surface layer is not less than either larger value selected between 0.06 mm and a value 0.2 times the sum of thicknesses of the intermediate layer and the surface layer but not more than a value 0.5 times the sum of the thicknesses of the intermediate layer and the surface layer. With this construction, the surface layer exhibits excellent sliding properties while the intermediate layer maintains high conformability, and therefore there can be provided the composite copper alloy bearing which has high fatigue strength particularly even in a case where a shaft susceptible to misalignment is used.
    Type: Grant
    Filed: February 28, 1996
    Date of Patent: June 16, 1998
    Assignee: Daido Metal Company Ltd.
    Inventors: Tadashi Tanaka, Koichi Yamamoto, Yoshiaki Sato
  • Patent number: 5758222
    Abstract: A development processing apparatus in which a photosensitive material is processed in processing solutions, and thereafter, the photosensitive material which has been processed in the processing solutions is subjected to drying processing by a dry air from a drying machine built in the development processing apparatus, comprising: a re-drying section which delivers the dry air from the drying machine to the outer side of the development processing apparatus; and photosensitive material holding means in which, in order to dry again the photosensitive material which has been subjected to drying processing by the dry air from the re-drying section, the photosensitive material which has been subjected to drying processing is held such that the surface of the photosensitive material which has been subjected to drying processing is substantially parallel to the direction of the dry air delivered from the re-drying section.
    Type: Grant
    Filed: April 21, 1997
    Date of Patent: May 26, 1998
    Assignee: Fuji Photo Film Co., Ltd.
    Inventor: Tadashi Tanaka
  • Patent number: 5672848
    Abstract: A ceramic circuit board wherein a copper circuit plate is directly bonded at a predetermined position on a ceramic substrate and heat is applied; or the copper circuit plate is integrally bonded through a brazing material containing an active metal, such as Ti, Zr and Hf; and a semiconductor element is bonded onto a semiconductor element mounting portion of the copper circuit plate through a solder layer. The copper plate element is formed with grooves or holes thereon and is bonded on the semiconductor element mounting portion of the copper circuit plate, and the semiconductor element is integrally bonded onto a surface of a grooved or holed side of the copper plate element through a solder layer.
    Type: Grant
    Filed: December 28, 1994
    Date of Patent: September 30, 1997
    Assignee: Kabushiki Kaisha Toshiba
    Inventors: Hiroshi Komorita, Tadashi Tanaka, Takayuki Naba, Takashi Hino
  • Patent number: 5671835
    Abstract: A wet friction member which can maintain boundary lubrication by decreasing the thickness of oil film on a friction surface even when the sliding velocity increases. In a case where the friction surface of the friction member is in pressure contact with a mated member while rotating in a state of boundary lubrications a shearing resistance owing to viscosity of cooling oil is circumferentially applied to cooling oil in outer grooves in the friction surface. Since outer grooves extend from starting position of intermediate portions of the friction surface and terminate at the outer peripheral edge in a volute shape toward the direction of rotation, cooling oil in the outer grooves flows along the groove walls and is quickly discharged from opening portions at the outer peripheral edge.
    Type: Grant
    Filed: October 20, 1995
    Date of Patent: September 30, 1997
    Assignee: Daido Metal Company Ltd.
    Inventors: Tadashi Tanaka, Yoshikazu Mizuno, Mitsuru Sugita, Katsumi Sawano, Akira Ono
  • Patent number: 5666644
    Abstract: An end bearing used in an automatic transmission gear having a one-way clutch mechanism having multi-layers comprising a back metal, a copper alloy layer, a tin layer having a thickness of 0.5 to 4 .mu.m and a Cu-Sn intermetallic compound layer having a thickness of 0.5 to 4 .mu.m and having a Microvickers hardness of from 400 to 700, which intermetallic compound layer is positioned just under the tin layer and which intermetalic compound layer is are formed on the copper alloy of such an end bearing. According to the present invention, it is possible to improve anti-seizure characteristics of an end bearing even under a condition of a decrease in the amount of oil supply which decrease occurs in higher engine speed, thus enabling the provision of an end bearing having superior anti-seizure characteristics.
    Type: Grant
    Filed: November 23, 1994
    Date of Patent: September 9, 1997
    Assignee: Daido Metal Company Ltd.
    Inventors: Tadashi Tanaka, Masaaki Sakamoto, Koichi Yamamoto, Tsukimitsu Higuchi, Kouki Ozaki
  • Patent number: 5665480
    Abstract: A copper-lead alloy bearing having a high corrosion resistance, especially a high corrosion resistance to sulfur, comprising a back metal and a copper-lead-based bearing alloy bonded thereto. The copper-lead-based bearing alloy consists of more than 10 but not more than 20% Ni, 0.5 to 8% Sn, 8 to 30% Pb, not less an 0.005 but not more than 0.2% P, and the balance of Cu and incidental impurities.
    Type: Grant
    Filed: March 12, 1996
    Date of Patent: September 9, 1997
    Assignee: Daido Metal Company Ltd.
    Inventors: Tadashi Tanaka, Masaaki Sakamoto, Koichi Yamamoto, Tsukimitsu Higuchi
  • Patent number: 5654107
    Abstract: A wear resisting aluminum alloy composite material consisting of 10 to 40% by volume of a hybrid compact and the balance substantially an aluminum alloy matrix, wherein the hybrid compact contains 85 to 95% by weight of an inorganic whisker which is 0.2 to 1.2 .mu.m in diameter and 10 to 30 .mu.m in length, and 5 to 15% by weight of an alumina fiber which is 100 to 300 .mu.m in length, and the aluminum alloy matrix contains 4 to 12% by weight of a silicon having an average grain size of not more than 5 .mu.m. The composite material offers good properties such as anti-seizure property and wear resistance. The composite material is suitable for sliding members. Aluminum borate whisker and potassium titanate whisker may be preferably used as the inorganic whisker.
    Type: Grant
    Filed: October 5, 1995
    Date of Patent: August 5, 1997
    Assignee: Daido Metal Company Ltd.
    Inventors: Tadashi Tanaka, Masaaki Sakamoto, Koichi Yamamoto, Yoshiaki Sato, Eiji Kato
  • Patent number: 5643683
    Abstract: A wet type sliding apparatus in which a multilayer sliding member is used in the presence of a lubricating oil, characterized in that the multilayer sliding member is composed of (1) a backing metal layer, (2) a porous, sintered layer provided thereon and (3) a surface layer consisting essentially of polyetheretherketone formed by impregnating and coating the porous, sintered layer with a sliding resin consisting essentially of polyetheretherketone. The above sliding member has a small friction coefficient and excellent wear resistance. In particular, the sliding noise can be more effectively inhibited by adjusting the face roughness of the surface layer of the sliding member to 2 .mu.m or less.
    Type: Grant
    Filed: January 24, 1996
    Date of Patent: July 1, 1997
    Assignee: Daido Metal Company Ltd.
    Inventors: Tadashi Tanaka, Hidehiko Tamura, Takahiro Niwa, Izumi Maruyama, Yoshihiro Fukutani