Patent number: 7595074
Abstract: A method of preparing a phenolic polymer comprising: a) protecting at least one hydroxyl group of a substituted or unsubstituted phenol represented by Structural Formula (XXIX), wherein: R11, R12, R13, R14 and R15 are independently —H, —OH, —NH, —SH, a substituted or unsubstituted alkyl or aryl group, a substituted or unsubstituted alkoxycarbonyl or aryloxycarbonyl group, a substituted or unsubstituted alkoxy group or a saturated or unsaturated carboxylic acid group; or R11, R12, R13, R14 or R15, in conjunction with an adjacent R11, R12, R13, R14 or R15, forms a substituted or unsubstituted alkylene dioxy group; provided that at least one of R11, R12, R13, R14 or R15 is a tert-butyl group 1-ethenyl-2-carboxylic acid or ester thereof, a substituted or unsubstituted alkylene dioxy group or a substituted or unsubstituted n-alkoxycarbonyl group, at least one of R11, R12, R13, R14 or R15 is a hydroxyl group, and at least one of R11, R12, R13, R14 and R15 is —H; with a protecting group, wherein thereby obtaining on
Type:
Grant
Filed:
January 21, 2004
Date of Patent:
September 29, 2009
Assignees:
University of Massachusetts Lowell, The United States of America as represented by the Secretary of the Army
Inventors:
Ashok L. Cholli, Vijayendra Kumar, Ashish Dhawan, Jayant Kumar, Virinder Singh Parmar, Lynne Ann Samuelson, Ferdinando F. Bruno