    Abstract: An electrode of a lithium ion battery includes a current collector, an electrode material layer disposed on a top surface of the current collector, and a protective film located on a top surface of the electrode material layer. A composition of the protective film is at least one of AlxMyPO4 and AlxMy(PO3)3, M represents at least one chemical element of Cr, Zn, Mg, Zr, Mo, V, Nb, and Ta, and a valence of M is represented by k, wherein 0<x<1, 0<y<1, and 3x+ky=3.
    Type: Grant
    Filed: April 13, 2012
    Date of Patent: November 20, 2012
    Assignees: Tsinghua University, Hon Hai Precision Industry Co., Ltd.
    Inventors: Xiang-Ming He, Jian-Jun Li, Li-Chun Zhang, Wei-Hua Pu, Jian Gao
  • Patent number: 8273829
    Abstract: The present disclosure relates to a method for making a conjugated polymer. In the method, polyacrylonitrile, a solvent, and a catalyst are provided. The polyacrylonitrile is dissolved in the solvent to form a polyacrylonitrile solution. The catalyst is uniformly dispersed into the polyacrylonitrile solution. The polyacrylonitrile solution with the catalyst is heated to induce a cyclizing reaction of the polyacrylonitrile, thereby forming a conjugated polymer solution with conjugated polymer.
    Type: Grant
    Filed: March 18, 2011
    Date of Patent: September 25, 2012
    Assignees: Tsinghua University, Hon Hai Precision Industry Co., Ltd.
    Inventors: Xiang-Ming He, Li Wang, Wei-Hua Pu, Wen-Ting Sun, Jian-Jun Li
  • Publication number: 20120219704
    Abstract: A method for making a modified current collector of a lithium ion battery is provided. In the method, the modifier and a metal plate are provided. The modifier is a mixture of a phosphorus source having a phosphate radical, a trivalent aluminum source, and a metallic oxide provided in a liquid phase solvent. The modifier is coated on a surface of the metal plate to form a coating layer. The coated metal plate is heat treated to transform the coating layer into a protective film formed on the surface of the metal plate.
    Type: Application
    Filed: May 3, 2012
    Publication date: August 30, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, JIAN-JUN LI, LI-CHUN ZHANG, WEI-HUA PU, JIAN GAO, JIAN-GUO REN
  • Patent number: 8252463
    Abstract: A modified current collector includes a metal plate and a protective film disposed on a surface of the metal plate. A composition of the protective film is at least one of AlxMyPO4 and AlxMy(PO3)3. M represents at least one chemical element selected from the group consisting of Cr, Zn, Mg, Zr, Mo, V, Nb, and Ta. A valence of M is represented by k, wherein 0<x<1, 0<y<1, and 3x+ky=3.
    Type: Grant
    Filed: February 28, 2011
    Date of Patent: August 28, 2012
    Assignees: Tsinghua University, Hon Hai Precision Industry Co., Ltd.
    Inventors: Xiang-Ming He, Jian-Jun Li, Li-Chun Zhang, Wei-Hua Pu, Jian Gao, Jian-Guo Ren
  • Patent number: 8247116
    Abstract: An electrode of a lithium ion battery includes a current collector, an electrode material layer disposed on a top surface of the current collector, and a protective film located on a top surface of the electrode material layer. A composition of the protective film is at least one of AlxMyPO4 and AlxMy(PO3)3, M represents at least one chemical element selected from the group consisting of Cr, Zn, Mg, Zr, Mo, V, Nb, and Ta, and a valence of M is represented by k, wherein 0<x<1, 0<y<1, and 3x+ky=3.
    Type: Grant
    Filed: February 25, 2011
    Date of Patent: August 21, 2012
    Assignees: Tsinghua University, Hon Hai Precision Industry Co., Ltd.
    Inventors: Xiang-Ming He, Jian-Jun Li, Li-Chun Zhang, Wei-Hua Pu, Jian Gao
  • Publication number: 20120196177
    Abstract: An electrode of a lithium ion battery includes a current collector, an electrode material layer disposed on a top surface of the current collector, and a protective film located on a top surface of the electrode material layer. A composition of the protective film is at least one of AlxMyPO4 and AlxMy(PO3)3, M represents at least one chemical element of Cr, Zn, Mg, Zr, Mo, V, Nb, and Ta, and a valence of M is represented by k, wherein 0<x<1, 0<y<1, and 3x+ky=3.
    Type: Application
    Filed: April 13, 2012
    Publication date: August 2, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, JIAN-JUN LI, LI-CHUN ZHANG, WEI-HUA PU, JIAN GAO
  • Publication number: 20120196176
    Abstract: An electrode composite material includes an individual electrode active material particle and a protective film coated on a surface of the particle. A composition of the protective film is AlxMyPO4, AlxMy(PO3)3, or a combination thereof. M represents at least one of Cr, Zn, Mg, Zr, Mo, V, Nb, or Ta. A valence of M is represented by k, in which 0<x<1, 0<y<1, and 3x+ky=3. In addition, a molar ratio of an aluminum element, an M element, and a phosphorous element in AlxMyPO4 or AlxMy(PO3)3 is set by (MolAl+MolMetal):Molp equal to about 1:2.5 to about 1:4, MolAl is the amount of substance of the aluminum element, MolMetal is the amount of substance of the M element, and Molp is the amount of substance of the phosphorous element. A lithium ion battery includes the electrode composite material.
    Type: Application
    Filed: April 13, 2012
    Publication date: August 2, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, JIAN-JUN LI, LI-CHUN ZHANG, JIAN-GUO REN, JIAN GAO, WEI-HUA PU
  • Patent number: 8211570
    Abstract: An electrode composite material includes an individual electrode active material particle and a protective film coated on a surface of the particle. A composition of the protective film is at least one of AlxMyPO4 and AlxMy(PO3)3, M represents at least one chemical element selected from the group consisting of Cr, Zn, Mg, Zr, Mo, V, Nb, and Ta, and a valence of M is represented by k, wherein 0<x<1, 0<y<1, and 3x+ky=3.
    Type: Grant
    Filed: February 28, 2011
    Date of Patent: July 3, 2012
    Assignees: Tsinghua University, Hon Hai Precision Industry Co., Ltd.
    Inventors: Xiang-Ming He, Jian-Jun Li, Li-Chun Zhang, Jian-Guo Ren, Jian Gao, Wei-Hua Pu
  • Publication number: 20120148734
    Abstract: A method for making a separator of a lithium ion battery is provided. In the method, a modifier, and a porous membrane are provided. The modifier is a mixture of a phosphorus source having a phosphate radical, a trivalent aluminum source, and a metallic oxide provided in a liquid phase solvent. The modifier is coated on a surface of the porous membrane to form a coating layer. The coated porous membrane is dried to form a modifier layer disposed on the surface of the porous membrane.
    Type: Application
    Filed: February 16, 2012
    Publication date: June 14, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, WEI-HUA PU, LI-CHUN ZHANG, JIAN-GUO REN, JIAN-JUN LI, JIAN GAO
  • Publication number: 20120132107
    Abstract: A modifier of a lithium ion battery includes a clear solution fabricated from a phosphorous source having a phosphate radical, a trivalent aluminum source, and a metallic oxide provided in a liquid phase solvent. A molar ratio of the trivalent aluminum source, the metallic oxide, and the phosphorous source is set by (MolAl+MolMetal):Molp=about 1:2.5 to about 1:4. MolAl is the amount of substance of an aluminum element in the trivalent aluminum source, MolMetal is the amount of substance of a metallic element in the metallic oxide, and Molp is the amount of substance of a phosphorous element in the phosphorous source.
    Type: Application
    Filed: February 3, 2012
    Publication date: May 31, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, JIAN-JUN LI, LI-CHUN ZHANG, WEI-HUA PU, JIAN GAO
  • Patent number: 8182948
    Abstract: A separator of a battery includes a porous membrane and a modifier layer disposed on a surface of the porous membrane, wherein a material of the modifier layer is a dried mixture of a phosphorus source having a phosphate radical, a trivalent aluminum source, and a metallic oxide in a liquid phase solvent.
    Type: Grant
    Filed: February 25, 2011
    Date of Patent: May 22, 2012
    Assignees: Tsinghua University, Hon Hai Precision Industry Co., Ltd.
    Inventors: Xiang-Ming He, Wei-Hua Pu, Li-Chun Zhang, Jian-Guo Ren, Jian-Jun Li, Jian Gao
  • Publication number: 20120097235
    Abstract: The present disclosure relates to a method for making a conjugated polymer. In the method, polyacrylonitrile, a solvent, and a catalyst are provided. The polyacrylonitrile is dissolved in the solvent to form a polyacrylonitrile solution. The catalyst is uniformly dispersed into the polyacrylonitrile solution. The polyacrylonitrile solution with the catalyst is heated to induce a cyclizing reaction of the polyacrylonitrile, thereby forming a conjugated polymer solution with the conjugated polymer dissolved therein.
    Type: Application
    Filed: March 18, 2011
    Publication date: April 26, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, LI WANG, WEI-HUA PU, WEN-TING SUN, JIAN-JUN LI
  • Patent number: 8163193
    Abstract: A modifier of a lithium ion battery includes a mixture of a phosphorus source having a phosphate radical, a trivalent aluminum source, and a metallic oxide in a liquid phase solvent. A method for making the modifier of the lithium ion battery. In the method, a phosphorus source having a phosphate radical, a trivalent aluminum source, and a metallic oxide are provided. The phosphorus source, the trivalent aluminum source, and the metallic oxide are mixed in a liquid phase solvent to form a clear solution.
    Type: Grant
    Filed: February 23, 2011
    Date of Patent: April 24, 2012
    Assignees: Tsinghua University, Hon Hai Precision Industry Co., Ltd.
    Inventors: Xiang-Ming He, Jian-Jun Li, Li-Chun Zhang, Wei-Hua Pu, Jian Gao
  • Publication number: 20120059129
    Abstract: In a method for making sulfurized polyacrylonitrile, polyacrylonitrile, a first solvent, a catalyst, and sulfur or sodium thiosulfate are provided. The polyacrylonitrile is dissolved in the first solvent to form a polyacrylonitrile solution. The catalyst is uniformly dispersed in the polyacrylonitrile solution. The polyacrylonitrile solution with the catalyst is heated to induce a cyclizing reaction of the polyacrylonitrile, thereby forming a first conjugated polymer solution with a conjugated polymer. The sulfur or sodium thiosulfate is uniformly mixed with the conjugated polymer to form a mixture. The mixture is heated to form sulfurized polyacrylonitrile.
    Type: Application
    Filed: March 18, 2011
    Publication date: March 8, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, LI WANG, WEI-HUA PU, WEN-TING SUN, JIAN-JUN LI
  • Publication number: 20120059085
    Abstract: The present disclosure relates to a method for making a conjugated polymer. In the method, polyacrylonitrile, a solvent, and a catalyst are provided. The polyacrylonitrile is dissolved in the solvent to form a polyacrylonitrile solution. The catalyst is uniformly dispersed into the polyacrylonitrile solution. The polyacrylonitrile solution with the catalyst is heated to induce a cyclizing reaction of the polyacrylonitrile, thereby forming a conjugated polymer solution with conjugated polymer.
    Type: Application
    Filed: March 18, 2011
    Publication date: March 8, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, LI WANG, WEI-HUA PU, WEN-TING SUN, JIAN-JUN LI
  • Publication number: 20120059128
    Abstract: The present disclosure relates to a sulfurized polyacrylonitrile and a lithium-ion battery cathode active material. The sulfurized polyacrylonitrile includes a structural unit. A general molecular formula of the structural unit is ?C3HNS?n, in which n is a positive integer. The lithium-ion battery cathode active material includes sulfurized polyacrylonitrile and a sulfurized polyacrylonitrile with inserted ions.
    Type: Application
    Filed: March 18, 2011
    Publication date: March 8, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, LI WANG, WEI-HUA PU, WEN-TING SUN, JIAN-JUN LI
  • Publication number: 20120052390
    Abstract: An electrode composite material includes an individual electrode active material particle and a protective film coated on a surface of the particle. A composition of the protective film is at least one of AlxMyPO4 and AlxMy(PO3)3, M represents at least one chemical element selected from the group consisting of Cr, Zn, Mg, Zr, Mo, V, Nb, and Ta, and a valence of M is represented by k, wherein 0<x<1, 0<y<1, and 3x+ky=3.
    Type: Application
    Filed: February 28, 2011
    Publication date: March 1, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, JIAN-JUN LI, LI-CHUN ZHANG, JIAN-GUO REN, JIAN GAO, WEI-HUA PU
  • Publication number: 20120052368
    Abstract: A modified current collector includes a metal plate and a protective film disposed on a surface of the metal plate. A composition of the protective film is at least one of AlxMyPO4 and AlxMy(PO3)3. M represents at least one chemical element selected from the group consisting of Cr, Zn, Mg, Zr, Mo, V, Nb, and Ta. A valence of M is represented by k, wherein 0<x<1, 0<y<1, and 3x+ky=3.
    Type: Application
    Filed: February 28, 2011
    Publication date: March 1, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, JIAN-JUN LI, LI-CHUN ZHANG, WEI-HUA PU, JIAN GAO, JIAN-GUO REN
  • Publication number: 20120049108
    Abstract: A modifier of a lithium ion battery includes a mixture of a phosphorus source having a phosphate radical, a trivalent aluminum source, and a metallic oxide in a liquid phase solvent. A method for making the modifier of the lithium ion battery. In the method, a phosphorus source having a phosphate radical, a trivalent aluminum source, and a metallic oxide are provided. The phosphorus source, the trivalent aluminum source, and the metallic oxide are mixed in a liquid phase solvent to form a clear solution.
    Type: Application
    Filed: February 23, 2011
    Publication date: March 1, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY
    Inventors: XIANG-MING HE, JIAN-JUN LI, LI-CHUN ZHANG, WEI-HUA PU, JIAN GAO
  • Publication number: 20120052361
    Abstract: A separator of a battery includes a porous membrane and a modifier layer disposed on a surface of the porous membrane, wherein a material of the modifier layer is a dried mixture of a phosphorus source having a phosphate radical, a trivalent aluminum source, and a metallic oxide in a liquid phase solvent.
    Type: Application
    Filed: February 25, 2011
    Publication date: March 1, 2012
    Applicants: HON HAI PRECISION INDUSTRY CO., LTD., TSINGHUA UNIVERSITY