PROCESS FOR THE PRODUCTION OF CARBOHYDRATE CLEAVAGE PRODUCTS FROM A LIGNOCELLULOSIC MATERIAL

- ANNIKKI GMBH

A process for the production of carbohydrate cleavage products, characterized by a combination of the measures that a lignocellulosic material is treated with an aqueous solution containing an alcohol, in particular a C1-4-alcohol or a phenol, and having a pH-value of between 11.0 and 14.0 in order to cleave lignocellulose and separate cleavage products from the material, whereby a material enriched with cellulose and hemicellulose is obtained, and the obtained material enriched with cellulose and hemicellulose is treated with at least one carbohydrate-cleaving enzyme in order to obtain the carbohydrate cleavage products.

Skip to: Description  ·  Claims  · Patent History  ·  Patent History
Description

The present invention relates to a process for the production of carbohydrate cleavage products, in particular sugars such as pentoses and hexoses, from a lignocellulosic material. Furthermore, the invention relates to a process for obtaining alcohol from the sugars. For the purposes of the present specification and claims, the term “sugar” is intended to encompass also “sugar oligomers”.

In connection with the shortage of crude oil and the discussion of corn as an energy supplier, the renewable raw material lignocellulose (straw, wood, waste paper etc.) gains a lot of significance as a starting material for fuels or chemical products. The conversion of lignocellulose may occur in two fundamentally different ways: 1) the “Thermochemical Platform” in which the lignocellulose is first gasified and the synthesis gases are synthesized into desired products, and 2) the “Sugar Platform” in which the main focus lies on utilizing the sugars bound in the polymers cellulose and hemicelluloses, while lignin is still being used predominantly energetically. The present invention can be allocated to the second way.

In contrast to starch, the sugars of lignocellulose are present in tightly cross-linked, polymeric, crystalline structures of the cellulose and the hemicelluloses, which, in addition, are covered with a lignin coat, which thereby leads to an extremely tight complex. The most obvious way of obtaining sugar from lignocellulose would be the direct use of cellulases and hemicellulases. However, this is hampered on the raw material straw or wood by the density of the above-mentioned complex. Due to their high molecular weight, enzymes are unable to penetrate through the narrow pores into the lignocellulose. This means that a first step has to be taken which increases the porosity of the lignocellulose and thereby enables a further enzymatic saccharification.

This first step is referred to as “pretreatment” (decomposition). It is consistently very complex so that, e.g., during the manufacture of “second generation biofuels”, up to ⅓ of the production costs have to be spent therefor, which has a negative influence on cost-effectiveness. The methods employed are aimed either at liquefying primarily the hemicelluloses (e.g., steam explosion-, dilute acid-pretreatment) or at achieving the increase in porosity by liquefying lignin (e.g., lime-, ammonia-pretreatment).

For obtaining sugars and their oligomers, respectively, the decomposed lignocellulose substrate can be treated further enzymatically, wherein the type of pretreatment can have a strong influence on enzyme activity and yield. At high reaction temperatures, toxic breakdown products (e.g., furfural) form frequently, which, in case of a directly attached ethanol fermentation, can inhibit the yeasts; see, e.g., Chandra et al., Advances in Biochemical Engineering/Biotechnology, 108:67, 2007; Mansfield et al., Biotechnol. Prog. 15:804, 1999.

A severe disadvantage of these methods is that they are energy-intensive and proceed mainly at temperatures of slightly below 200° C.

A technological improvement in this field, e.g., due to the development of low-temperature methods (i.e., at a temperature of below 100° C.), would mean a decisive progress for any substantial utilization of the raw material lignocellulose. This is the object of the present invention.

From EP 1 025 305 B1, a chemical process for lignin depolymerization (Cu-system) is known. It is based on the catalytic effect of complexed copper in combination with hydrogen peroxide or organic hydroperoxides and is able to oxidatively cleave lignin at temperatures of below 100° C. The complexing agents used in the process are pyridine derivatives. It has been possible to demonstrate on synthetic lignin models that, when H2O2 is used as an oxidant, a cleavage of ether bonds of the lignin molecule occurs, whereby the lignin polymer disintegrates into oligomeric subunits. Using the Cu-system with an excess of organic hydroperoxides, it is possible to delignify wood. The system based on H2O2 appears to be better in terms of being technically feasible, has been tested as a bleaching additive in the peroxide bleaching of kraft pulp and has resulted in an improved delignification rate and a higher degree of whiteness.

Furthermore, it is known from “Oxidation of wood and its components in water-organic media”, Chupka et al., Proceedings: Seventh International symposium on wood and pulping chemistry, Vol. 3, 373-382, Beijing P.R. China, May 25-28, 1993, that the efficiency of an alkaline catalysis of the oxidation of wood and lignin increases substantially if an organic solvent, e.g., DMSO, acetone, ethanol, is added to the aqueous reaction medium. Furthermore, the authors suggest that, at pH-values of above 11, a drastic increase in the oxidation of the wood and the lignin occurs.

From WO 01/059204, a process for the production of pulp is known in which the starting material is subjected to a pretreatment, wherein the material is treated with a buffer solution and a delignification catalyst (transition metal). Delignification is carried out in the presence of oxygen, hydrogen peroxide or ozone.

In contrast, the process according to the invention for the production of sugars is characterized by a combination of the measures that

    • a lignocellulosic material is treated with an aqueous solution containing an alcohol, in particular a C1-4-alcohol or a phenol, and having a pH-value of between 11.0 and 14.0 in order to cleave lignocellulose and separate cleavage products from the material, whereby a material enriched with cellulose and hemicellulose is obtained, and
    • the obtained material enriched with cellulose and hemicellulose is treated with at least one carbohydrate-cleaving enzyme in order to obtain the carbohydrate cleavage products.

Aliphatic or cycloaliphatic, mono- or polyvalent alcohols or phenols, e.g., C1-6-alcohols, in particular a C1-4-alcohol such as methanol, ethanol, propanol and butanol, including their isomers; glycols (ethane diols, propane, butane, pentane, hexane diols), glycerol, propenol, butenol, cyclopentanol, cyclohexanol, benzyl alcohol; or phenols such as phenols, cresols, catechols, naphthols, but also amino alcohols such as ethanolamine, methanolamine and hexanolamine are suitable as alcohols. A C1-4-alcohol is preferred. For the purposes of the present patent application, phenols are also included in the generic term “alcohol”.

Moreover, the alcoholic solution of the lignin extract provides advantageous options for the further reprocessing of the lignin and xylan cleavage products, respectively.

In the process according to the invention, alcohol is present in an aqueous solution preferably in an amount of from 10 to 70% by volume, e.g., from 20 to 50% by volume, preferably from 30 to 40% by volume.

In the process according to the invention, the lignocellulosic material is present in the aqueous solution preferably in a stock density of 3-40% by weight, such as 5-40% by weight, in particular 5-20% by weight.

Preferably, the lignocellulose is cleaved at a temperature of below 100° C., such as below 80° C., e.g., below 60° C.

The pH-value can be adjusted with a base, preferably an inorganic base, for example, a caustic soda solution.

The present invention is based on the realization that a lignocellulosic material treated with an aqueous basic solution containing an alcohol, in particular a C1-4-alcohol or a phenol, and having a pH-value of between 11.0 and 14.0 can be processed enzymatically into carbohydrate cleavage products such as sugars in higher yields than a material delignified in another way, in particular without addition of alcohol.

Mainly pentoses and hexoses are formed as carbohydrate cleavage products. Preferred sugars include xylose and glucose.

A preferred embodiment of the process according to the invention is characterized in that the material enriched with cellulose and hemicellulose is treated with a xylanase and a cellulase in order to extract the sugars.

Straw, energy grasses such as, e.g., switch grass, elephant grass or abaca, sisal, bagasse, or untypical lignocellulose substrates such as spelts, e.g., rice spelts, preferably straw, energy grasses, bagasse or spelts, particularly preferably straw or bagasse, e.g., straw, are preferably used as lignocellulosic materials. Straw has a highly hydrophobic surface so that its wetting with aqueous solutions constitutes a problem. It has been shown that, by using alcohol, it is possible to introduce the reaction solution into the pores of the substrate even without pressure and to replace the existing air by reaction solution. Besides, it has been shown that alcohol accelerates the extraction of the cleavage products from straw and contributes to keeping the lignin cleavage products in solution. Furthermore, it has been shown that, in contrast, alcohol reduces the solubility of the hemicellulose and its cleavage products and thus the hemicellulose is kept in the substrate.

By pressing out the liquid phase from the substrate after the decomposition process, the substrate concentration is increased so that smaller enzyme amounts are required for the enzymatic hydrolysis and for other enzymatic subsequent treatments, respectively.

In the production of alcohol, enzyme costs are a critical cost factor. The result of alcohol is that the solubility of the hemicelluloses which possibly have been released during the reaction in the alkaline range in addition to the lignin and of the cleavage products thereof is drastically reduced and that they remain bound to the substrate. The advantages for the process are the high selectivity of the lignin degradation, in the event of a separation of the extraction solution from the solid, a very low concentration of hemicellulose and its cleavage products in the extraction solution, since the hemicellulose remains in the solids content and is thereby maintained for the enzymatic hydrolysis and the extraction of sugar.

Furthermore, the alcoholic solution of the lignin extract provides improved possibilities for the further reprocessing of the lignin and the manufacture of products from lignin.

Furthermore, it has been shown that, by using alcohol, in particular a C1-4-alcohol or a phenol, in the alkaline decomposition below 100° C., the degradation of the hemicelluloses is largely prevented so that approximately the entire hemicellulose is available for the further enzymatic cleavage and conversion of the xylose into higher-quality products and is not partially degraded during the decomposition and will not accumulate as a lignin/sugar mixture, such as in other processes.

By the delignification carried out in the decomposition, the porosity of the cell walls of the lignocellulosic material is increased, for example, in case of straw it is increased to such an extent that almost the entire xylose becomes accessible for the xylanase and approximately 100% of the xylan can be hydrolyzed and xylose can be obtained. This renders the process according to the present invention particularly suitable for manufacturing higher-quality products in combination with an enzymatic conversion of the xylose. In doing so, the enzymatic conversion can occur either directly in the mixture of xylose solution and solid, or also with the xylose solution separated from the solid.

In a further alcohol production from the remaining solid, which follows after the enzymatic hydrolysis of the xylan and the conversion according to the invention of xylose into xylitol, enzyme costs are a critical cost factor. They result partly also from unspecific bindings of enzymes to the lignin, see, e.g., Chandra et al, 2007, ibidem. The partial removal of the lignin reduces this loss in activity and has a cost-saving effect.

The advantages for a subsequent enzymatic process are, for example, that a very low concentration of hemicellulose and its cleavage products in the extraction solution results from the high selectivity of the lignin degradation, with the sugar polymers being preserved almost completely, the hemicellulose remains in the solids content and is thereby maintained for the enzymatic hydrolysis and the extraction of sugar as well as its further transformation. The result according to the invention is a maximum material utilization rate and, for example in connection with the use of xylose dehydrogenases, a high cost-effectiveness of the described process.

The implementation of a xylose transformation process into xylitol can be performed after the enzymatic release of the xylose directly in the solid/liquid mixture, which is obtained according to the present process of the invention, which further increases the cost-effectiveness of the entire process.

In the event of a transformation into xylitol, the residual alcohol from the decomposition process, which remains in the substrate after the solid has been pressed out, can be used directly as a substrate for the alcohol dehydrogenase for the regeneration of NAD into NADH. If the process is designed such that, for this purpose, the residual alcohol from the decomposition, which remains in the reaction mixture, is (partially) consumed, a removal of alcohol from the product solution becomes (partially) superfluous and the efficiency of the entire process is thereby further increased.

In the event of a transformation of the lignin cleavage products, the alcohol acts as a radical scavenger and a solvent for cleavage products from an enzymatic, biomimetic or chemical depolymerization of the higher-molecular lignin cleavage products into low-molecular ones.

The small content of hemicelluose and its cleavage products in the extract and the increased solubility of the lignin increase the throughput rates during a separation of the solid from the conversion products as well as their reprocessing by filtration.

The process according to the invention enables, for example, the separation of the three main components of the straw, namely of glucose, xylose as well as lignin, into material flows very low in extraneous materials and their further transformation into higher-quality products such as xylitol, and thus meets the requirements of an ideal biorefinery process.

A further advantage of the process according to the invention in comparison to other decomposition methods which proceed predominantly in a temperature range between 150° C. and 200° C. is its reaction temperature of below 100° C. The small energy expenditure allows to use the lignin obtained during the decomposition as a valuable product, rather than as an energy source for the decomposition method.

After the treatment with the aqueous solution containing an alcohol, in particular a C1-4-alcohol or a phenol, and H2O2, according to the process of the present invention, the solution containing lignin is separated and the decomposed solid is preferably treated with a xylanase, at 30-90° C., e.g., for 6-72 hours, and the liquid phase is separated from the solid, whereupon the liquid phase is preferably reacted further into resultant products, e.g., xylitol.

The solid remaining after the separation of the liquid phase is preferably treated with cellulase, whereby, via a further fermentation of the solid/glucose solution, ethanol, butanol or other fermentation products can be obtained; or the remaining solid is subjected to a thermal or thermochemical conversion and the resulting products such as fuel components, fuel additives and/or other chemical products such as, e.g., phenols are separated; or the remaining solid is subjected to a microbial conversion by bacteria, yeasts or fungi; or the remaining solid is subjected to a further delignification step for the purpose of obtaining a cellulose fibre material.

The remaining solid can be fermented in a biogas plant and can be processed further into biogas.

One of the economically most interesting resultant products of xylose is xylitol.

The main sources for the recovery of xylose are cooking liquors from the pulp industry which contain an abundance of breakdown products, mainly of lignin and of hemicellulose, so that xylose must be obtained by complex separation and purification steps. For example, H. Harms describes in “Willkommen in der natürlichen Welt von Lenzing, weltweit führend in der Cellulosefaser Technologie”, Herbsttagung der osterreichischen Papierindustrie, Frantschach (Nov. 15, 2007), the recovery of xylose from the thick liquor by gel filtration, a technically very complex method which usually is not used for bulk products. The xylose obtained in this way is then converted catalytically into xylitol.

In a further aspect, the xylose obtained according to the present invention is converted into xylitol without fermentation, by conversion with a xylose reductase, e.g., a xylose dehydrogenase, for example from Candida tenuis, wherein optionally a xylose reductase and optionally a cosubstrate for the regeneration of the cofactor and optionally alcohol dehydrogenase and optionally NAD(P)H are added to the xylose solution; in particular with the xylitol obtained being separated from the lignin cleavage products by filtration.

By means of the following Example 1 and Comparative Example 1A, the influence of the pretreatment in the presence of alcohol on the yield of reducing sugars after an enzymatic hydrolysis is documented.

EXAMPLE 1 Pretreatment of Wheat Straw

Wheat straw is crushed to a particle size of approx. 2 cm. 5 g of crushed wheat straw is suspended in a 500 mL reaction vessel in 200 mL of a solution consisting of 49.5% water, 50% ethanol and 0.5% hydrogen peroxide. The suspension is heated to 50° C. in a water bath, is thermostated, and the pH-value of the suspension is adjusted to an initial pH-value of 12 with an aqueous NaOH solution. The mixture is magnetically stirred continuously at 200 rpm, 60° C., for 24 hours. Thereupon, the solids content is filtered off and washed with 1 L of distilled water.

For the enzymatic hydrolysis, 100 mg of a pretreated substrate from each parallel trial were set to pH 4.8 with 9.8 mL of 50 mM Na-acetate buffer and mixed with 200 μL of Accellerase 1000 Suspension (www.genencor.com). Accellerase is an enzyme mixture of cellulases and hemicellulases. The enzymatic hydrolysis was performed at 50° C. in a shaking water bath. The soluble monomers released after 48 hours from hexoses and pentoses were determined in 1 mL of a liquid supernatant in the form of reducing sugars according to the DNS method (Miller et al., Analytical Chemistry 31(3):426, 1959), related to the amount of weighed-in, pretreated substrate and expressed in percent of the maximum theoretical yield.

The maximum theoretical yield of reducing sugars was determined separately and is 705 mg+/−5% per g of untreated straw.

Per test stock, 5 parallel trials were conducted. The yield of reducing sugars was 99%+/−4%.

COMPARATIVE EXAMPLE 1A

Example 1 was repeated, but without the addition of alcohol. The yield of reducing sugars was merely 64%+/−3%.

EXAMPLE 2 Pretreatment of Wheat Straw

Wheat straw is crushed to a particle size of approx. 2 cm. 2.5 g of crushed wheat straw is suspended in a 500 mL reaction vessel in 200 mL of a solution consisting of 49.5% water and 50% isopropanol. The suspension is heated to 50° C. in a water bath, is thermostated, and the pH-value of the suspension is adjusted to an initial pH-value of 13 (or 14, respectively) with an aqueous NaOH solution. The mixture is magnetically stirred continuously at 200 rpm, 60° C., for 24 hours. Thereupon, the solids content is filtered off and washed with 1 L of distilled water.

For the enzymatic hydrolysis, 100 mg of a pretreated substrate from each parallel trial were set to pH 4.8 with 9.8 mL of 50 mM Na-acetate buffer and mixed with 200 μL of Accellerase 1000 Suspension (www.genencor.com). Accellerase is an enzyme mixture of cellulases and hemicellulases. The enzymatic hydrolysis was performed at 50° C. in a shaking water bath. The soluble monomers released after 48 hours from hexoses and pentoses were determined in 1 mL of a liquid supernatant in the form of reducing sugars according to the DNS method, related to the amount of weighed-in, pretreated substrate and expressed in percent of the maximum theoretical yield.

The maximum theoretical yield of reducing sugars was determined separately and is 705 mg+/−5% per g of untreated straw.

Per test stock, 5 parallel trials were conducted. The yield of reducing sugars was 97%+/−4%.

EXAMPLE 3

Enzymatic Xylitol Production from a Xylose Solution Produced from Straw According to the Process Described in Example 2. Isopropanol is Used as a Cosubstrate.

The reaction solution contains 5 mg/mL xylose.

Xylose reductase (XR) from Candida tenuis reduces xylose to xylitol. Said XR requires NADH (nicotinamide adenine dinucleotide reduced) as a coenzyme, which is oxidized to the coenzyme NAD+ during the reaction. The regeneration of the oxidized cofactor is effected by the parallel activity of an alcohol dehydrogenase (ADH: enzyme-coupled regeneration). Isopropanol is used as a cosubstrate. Isopropanol and NAD+ are reacted into NADH and acetone by the ADH, as is shown in Reaction Scheme 1:

In Table 1, the reaction ratios in the 5 different test reactions #049, #050, #051, #052, #053 and #054 are illustrated:

TABLE 1 Reaction number #049 #050 #052 #053 #054 Substrate batch I [μl] 250 250 250 500 500 XR C. tenuis 2 U/mL [μL] 50 50 50 20 mM NADH [μL] 50 50 50 ADH L. kefir 5 U/mL [μL] 50 50 Isopropanol [μL] 50 50 50 mM Na-phosphate puffer, pH 7.0 750 650 550 500 300 [μL]

Total volume: 1 mL

Temperature: 26±2° C.

Magnetic stirrer: 200 rpm
Time: 15 hours

For deactivating the enzymes, all samples were heated to 95° C. for 15 minutes and centrifuged in preparation for the subsequent HPLC analysis.

Analysis—HPLC: Column SUGAR SP0810+precolumn SUGAR SP-G

Detector: refractive index detector
Eluent: deionized H2O
Flow: 0.75 mL/min
Amount of sample: 10 μL
HPLC quantification precision: ±10%

Retention Time: Xylose: 13.97 min Xylitol: 37.73 min Isopropanol: 16.69 min Acetone: 16.54 min Results:

The substrate concentration of sample #049 was determined by HPLC and amounted to 0.9 mg/mL.

The reaction mixture #050 includes only xylose reductase (0.1 U/mL) and NADH (1 mM). After the reaction lasting for 15 hours, 0.085 mg of xylose was consumed. The xylitol concentration was below the detection limit.

Reaction #052 is comparable to Reaction #050, but with the difference that, in this case, the regeneration system is applied. The result is a total conversion of the xylose used. Concentrations used: XR (0.1 U/mL), NADH (1 mM), ADH (0.25 U/mL) and isopropanol (5%).

The xylose concentration of sample #053 was determined to be 2.121 mg/mL, which corresponds to the expected xylose concentration.

Reaction #054 is comparable to Reaction #052, but includes an initial xylose concentration increased by factor 2 (50% substrates in the reaction). The concentration of the xylitol produced was measured to be 0.945 mg xylitol. Concentrations used: XR (0.1 U/mL), NADH (1 mM), ADH (0.25 U/mL) and Isopropanol (5%).

In Table 2, the results of the reactions are summarized based on the measured HPLC data (Xylose consumed and Xylitol recovered; b.D.L. means “below the detection limit”):

TABLE 2 Reaction number 049 050 052 053 054 Xylose prior to the reaction 0.9 0.815 0.8 2.121 1.945 [mg/mL] Xylose after the reaction 0.815 b.D.L. 1.013 [mg/mL] Xylose consumed in the b.D.L. 0.932 reaction [mg/mL] Recovery of xylitol [mg/mL] b.D.L. 0.994 0.945 Xylitol yield relative to the b.D.L. 100 47.9 xylose concentration [%]

EXAMPLE 4

Enzymatic Xylitol Production from a Xylose Solution Produced from Straw According to the Process Described in Example 2. Ethanol is Used as a Cosubstrate.

The volume of the substrate solution was (cf. Example 2) reduced to 50% using a rotary evaporator in order to increase the xylose concentration (˜10 mg/mL xylose).

The regeneration of the oxidized cofactor was effected by the activity of the xylose reductase (XR) from Candida tenius which was used and the additional activity of an aldehyde dehydrogenase from Saccharomyces cerevisiae which was used (Sigma-Aldrich: Catalogue No. A6338; (EC) No.: 1.2.1.5; CAS No.: 9028-88-0). This is both a substrate-coupled and an enzyme-coupled reaction. Ethanol is used as a cosubstrate. In the first step, ethanol and NAD+ are converted into NADH and acetaldehyde by the activity of the XR. In the second step, acetaldehyde and NAD+ are converted into acetate by the activity of the aldehyde dehydrogenase (AldDH) (cf. for this purpose: Sigma-Aldrich: Catalogue No. A6338; and “Characterization and Potential Roles of Cytosolic and Mitochondrial Aldehyde Dehydrogenases in Ethanol Metabolism in Saccharomyces cerevisiae”, Wang et al, Molecular Cloning, 1998, Journal of Bacteriology, p. 822-830, respectively). Per mol of converted cosubstrate, 2 mols of reduction equivalent (NADH) would form in this case (cf. Reaction Scheme 2).

In Table 3, the reaction ratios of the 4 different test reactions 247, 249, 250 and 253 are illustrated. Different ethanol concentrations and AldDH concentrations were used. Cofactor and substrate concentrations were kept constant.

TABLE 3 Reaction number 247 249 250 253 Substrate batch III 300 (56 mM) 300 (56 mM) 300 (56 mM) 300 (56 mM) [μL] XR C. tenius 25 (0.25 U/mL) 25 (0.25 U/mL) 25 (0.25 U/mL) 25 (0.25 U/mL) 5 U/mL [μL] 20 mM NAD+ [μL] 10 (0.4 mM) 10 (0.4 mM) 10 (0.4 mM) 10 (0.4 mM) AldDH S. cervisiae 25 (0.25 U/mL) 25 (0.25 U/mL) 0 0 5 U/mL [μL] Ethanol 50% [μL] 75 (1286 mM) 70 (1200 mM) 75 (1286 mM) 70 (1200 mM) 50 mM TrisHCl buffer 65 70 90 95 pH 7.0 [μL]

Total volume: 0.5 mL

Temperature: 25±2° C. Thermomixer: 500 rpm

Time 112 hours

For deactivating the enzymes, all samples were heated to 70° C. for 15 minutes and centrifuged and filtered in preparation for the subsequent HPLC analysis (PVDF; 0.2 μm).

Analysis—HPLC: Column SUGAR SP0810+precolumn SUGAR SP-G

Column temperature: 90° C.
Detector: refractive index detector
Eluent: deionized H2O
Flow: 0.90 mL/min
Amount of sample: 10 μL
HPLC quantification precision: ±10%

Results:

The maximum yield (Reaction 249) could be achieved with an ethanol concentration of 1.2 mol/L. In doing so, a total of 1.38 mg/mL of xylitol was produced, which corresponds to a yield of 21.2% of xylitol in theory.

In Table 4, the results of the reactions based on the measured HPLC data are summarized.

TABLE 4 Reaction number 247 249 250 253 Theoretical total concentration [mg/mL] 6.288 6.407 6.268 6.150 Xylose after the reaction [mg/mL] 5.057 5.046 5.385 5.365 Xylose consumed in the reaction [mg/mL] 1.231 1.361 0.883 0.785 Recovery of xylitol [mg/mL] 1.248 1.379 0.894 0.796

It is evident from the results that ethanol can be used as a cosubstrate. As can be shown clearly by comparing Reactions 249 (reaction mixture including AldDH) and 253 (reaction mixture without AldDH), the addition of the aldehyde dehydrogenase leads to a clear increase in the yield of xylitol. The difference of converted xylose from xylitol amounts to ˜8%. This result in connection with the above-mentioned citations from literature allows only the conclusion that AldDH oxidizes the acetaldehyde forming in the first partial reduction further to acetic acid (cf. Reaction Scheme 2). This energetically favourable reaction and the increased concentration of NADH associated therewith shifts the equilibrium from the educt towards the product xylitol in the first partial reaction.

Claims

1. A process for the production of carbohydrate cleavage products, the process comprising:

treating a lignocellulosic material with an aqueous solution containing an alcohol and having a pH-value of between 11.0 and 14.0 in order to cleave lignocellulose and separate cleavage products from the material, whereby a material enriched with cellulose and hemicellulose is obtained, and
treating the obtained material enriched with cellulose and hemicellulose with at least one carbohydrate-cleaving enzyme in order to obtain the carbohydrate cleavage products.

2. A process according to claim 1, wherein the aqueous solution has a pH-value of between 11.0 and 13.0.

3. A process according to claim 1, wherein the cleavage occurs at a temperature of below 100° C.

4. A process according to claim 3, wherein the cleavage occurs at a temperature of below 40° C.

5. A process according to claim 1, wherein straw, bagasse, energy grasses and/or spelts are used as a lignocellulosic material.

6. A process according to claim 1, wherein the lignocellulosic material is present in the aqueous solution in a stock density of 5-40% by weight.

7. A process according to claim 1, wherein the material enriched with cellulose and hemicellulose is treated with a xylanase and/or a cellulase in order to extract the sugars.

8. A process according to claim 1, wherein the sugars obtained are fermented into alcohol which is separated and recovered.

9. A process according to claim 1, wherein the decomposed solid is converted with a xylanase and the liquid phase obtained is converted into xylitol, and the remaining solid:

is reacted further with cellulase in order to obtain different fermentation products;
or
is subjected to a thermal or thermochemical conversion;
or
is subjected to a microbial conversion by bacteria, yeasts or fungi;
or
is subjected to a further delignification step for the purpose of obtaining a cellulose fibre material.

10. A process according to claim 9, wherein the decomposed solid is converted with a xylanase and the liquid phase obtained is converted into xylitol using a xylose dehydrogenase, and the remaining solid:

is reacted further with cellulase in order to obtain different fermentation products;
or
is subjected to a thermal or thermochemical conversion;
or
is subjected to a microbial conversion by bacteria, yeasts or fungi;
or
is subjected to a further delignification step for the purpose of obtaining a cellulose fibre material.

11. A process according to claim 9, wherein the solid remaining after the separation of the products is fermented in a biogas plant and is processed further into biogas.

12. A process according to claim 2, wherein the cleavage occurs at a temperature of below 100° C.

13. A process according to claim 12, wherein the carbohydrate cleavage products include a sugar.

14. A process according to claim 1, wherein the alcohol includes a C1-4-alcohol or a phenol.

15. A process according to claim 14, wherein straw, bagasse, energy grasses and/or spelts are used as a lignocellulosic material.

16. A process according to claim 15, wherein the lignocellulosic material is present in the aqueous solution in a stock density of 5-40% by weight.

17. A process according to claim 16, wherein material enriched with cellulose and hemicellulose is treated with a xylanase and/or a cellulase in order to extract the sugars.

18. A process according to claim 17, wherein the sugars obtained are fermented into alcohol which is separated and recovered.

19. A process according to claim 18, wherein the solid remaining after the separation of the fermentation products is fermented in a biogas plant and is processed further into biogas.

Patent History
Publication number: 20180230503
Type: Application
Filed: Apr 11, 2018
Publication Date: Aug 16, 2018
Applicant: ANNIKKI GMBH (Graz)
Inventors: Karin FACKLER (Wien), Kurt MESSNER (Wien), Chularat KRONGTAEW (Bangyai), Ortwin ERTL (Graz)
Application Number: 15/951,027
Classifications
International Classification: C12P 19/14 (20060101); C12P 7/14 (20060101); C12P 5/02 (20060101); C12P 7/02 (20060101); C12P 7/18 (20060101);