NON-ORTHOGONAL ADDITIVE MANUFACTURING AND THE TREATMENT OF PARTS MANUFACTURED THEREOF
The present disclosure provides a 3D printer including a receiving surface for accepting the accumulation of material layers, and a gantry having a shaft and carriage that is translated along the shaft, and an extruder assembly that is articulated to rotate a printing plane, wherein the extruder assembly is attached to the carriage and the articulated extruder assembly is manipulated to rotate the printing plane away from parallel with the receiving surface.
The present application claims the benefit of U.S. Provisional Patent Application No. 62/716,852, filed Aug. 9, 2018, the content of which is hereby incorporated by reference in its entirety.
GOVERNMENT SUPPORTThis invention was made with government support under CEED SINIT-16-0013 awarded by Consortium for Energy, Environment and Demilitarization (CEED). The U.S. government has certain rights in the invention.
BACKGROUNDAdditive manufacturing, or 3D printing, uses a layered approach to build parts and is an important manufacturing tool in a number of industries for the fabrication of automotive components, aerospace components, packaging materials, construction components, medical components, and the like. Conventionally, in 3D printing, layers are printed horizontally and built up vertically layer upon layer to form an end product or part thereof. Therefore, the print angle (i.e., the angle between the print plane and the horizontal plane) is commonly referred to as a zero degree angle. Additional support material not essential to the final part geometry is required for layers that overhang beyond previously deposited layers in the horizontal direction.
Parts are often 3D printed with their longitudinal axis oriented in the vertical direction to minimize the amount of support material needed, but are then limited by the vertical height, z-height, of the printer. In situations where the part size is greater than the machine capacity, the part may be split into separate pieces, printed, and then joined afterwards. The splitting and joining process creates complexity where mating surfaces need to be well aligned and typically requires additional machining.
Alternatively, to accommodate larger parts, a larger build volume may be constructed. For a conventional 3-axis printer additional y-axis length is the least expensive to incorporate using longer rails, extra x-axis width is more expensive due to the extra length of the gantry, and extra z-axis height is the most expensive to expand due to the greater stiffness required to overcome the inertia of the gantry at a greater height. Increasing a printer's build volume is therefore a cost balance between greater z-height and the surplus material required to support overhanging geometry.
Therefore, there is a need for an improved 3D printing system and method to build large 3D parts.
SUMMARYIn one aspect, the present disclosure provides 3D printers including a horizontal surface for accepting the accumulation of material layers, and a gantry having a shaft and carriage that is translated along the shaft, and an extruder assembly that is articulated to rotate a printing plane (e.g., to provide up to 5 axes of movement), wherein the extruder assembly is attached to the carriage and the articulated extruder assembly is manipulated to rotate the printing plane away from parallel with the horizontal surface. In some embodiments, the gantry offers a print area with a certain width and height through which a part that exceeds the print volume is printed by gradually moving the part away from the print area. In some embodiments, the printing plane angle relative to the horizontal bed is changed to increase material throughput for a given part geometry and layer cooling rate requirement. In some embodiments, the print angle is changed so that a 3D part with overhangs or hollow sections can be printed without the need for support material, or, in some cases, with a drastically reduced requirement for support material. In some embodiments, the extension of the part volume beyond printer volume drives the parallel post-processing of the part by means of a separate working volume into which the part enters and machining operations are executed.
In some embodiments, the print angle may be greater than or equal to 0 degree, greater than or equal to 30 degrees, greater than or equal to 45 degrees, greater than or equal to 60 degrees, or greater than or equal to 90 degrees, between 0 and 90 degrees, between 0 and 80 degrees, between 0 and 70 degrees, between 0 and 60 degrees, between 0 and 50 degrees, between 0 and 40 degrees, between 0 and 30 degrees, between 0 and 20 degrees, between 0 and 10 degrees, between 10 and 80 degrees, between 10 and 70 degrees, between 10 and 60 degrees, between 10 and 50 degrees, between 10 and 40 degrees, between 10 and 30 degrees, between 10 and 20 degrees, between 20 and 80 degrees, between 30 and 80 degrees, between 40 and 80 degrees, between 50 and 80 degrees, between 10 and 50 degrees, and 0 to 45 degrees. In another embodiment, the print angle is between 0 and −90 degrees (e.g., between 0 and −80 degrees, between 0 and −70 degrees, between 0 and −60 degrees, between 0 and −50 degrees, between 0 and −40 degrees, between 0 and −30 degrees, between 0 and −20 degrees, between 0 and −10 degrees, between −10 and −80 degrees, between −10 and −70 degrees, between −10 and −60 degrees, between −10 and −50 degrees, between −10 and −40 degrees, between −10 and −30 degrees, between −10 and −20 degrees, between −20 and −80 degrees, between −30 and −80 degrees, between −40 and −80 degrees, between −50 and −80 degrees, between −10 and −50 degrees, and 0 to −45 degrees). Other ranges are also possible.
In some embodiments, the surface that accepts initial material accumulation may be a rigid member with a curved receiving surface including the cross-section of an angled bar containing an internal radius, and a length spanning the width of said 3D printer's print volume in the x-direction, wherein the cross-section of the rigid member is consistent along the x-direction and said internal radius is constant or non-constant so as to increase the surface contact with material deposited by said 3D printer.
In another aspect, the present disclosure describes a 3D printer which includes a receiving surface for accepting the accumulation of material layers, a gantry, and an extruder assembly that is articulated to rotate a printing plane, wherein the extruder assembly is operably attached to the gantry (e.g., via a carriage) and the articulated extruder assembly is manipulated to rotate the printing plane away from parallel with the receiving surface.
In some embodiments, the receiving surface is movable. In some embodiments, the receiving surface includes a flat belt. In some embodiments, the receiving surface includes a plurality of pulleys. In some embodiments, the receiving surface is articulated to rotate away from parallel with a horizontal plane.
In some embodiments, the extruder assembly is articulated to rotate about one or more axes. In some embodiments, the extruder assembly is articulated to rotate and form a first angle with the receiving surface. In one embodiment, the first angle is between 0 and 90 degrees (e.g., between 0 and 80 degrees, between 0 and 70 degrees, between 0 and 60 degrees, between 0 and 50 degrees, between 0 and 40 degrees, between 0 and 30 degrees, between 0 and 20 degrees, between 0 and 10 degrees, between 10 and 80 degrees, between 10 and 70 degrees, between 10 and 60 degrees, between 10 and 50 degrees, between 10 and 40 degrees, between 10 and 30 degrees, between 10 and 20 degrees, between 20 and 80 degrees, between 30 and 80 degrees, between 40 and 80 degrees, between 50 and 80 degrees, between 10 and 50 degrees, and 0 to 45 degrees). In another embodiment, the first angle is between 0 and −90 degrees (e.g., between 0 and −80 degrees, between 0 and −70 degrees, between 0 and −60 degrees, between 0 and −50 degrees, between 0 and −40 degrees, between 0 and −30 degrees, between 0 and −20 degrees, between 0 and −10 degrees, between −10 and −80 degrees, between −10 and −70 degrees, between −10 and −60 degrees, between −10 and −50 degrees, between −10 and −40 degrees, between −10 and −30 degrees, between −10 and −20 degrees, between −20 and −80 degrees, between −30 and −80 degrees, between −40 and −80 degrees, between −50 and −80 degrees, between −10 and −50 degrees, and 0 to −45 degrees).
In some embodiments, the extruder assembly comprises a nozzle and the nozzle is articulated to rotate about one or more axes. In some embodiments, the nozzle is articulated to rotate and form a second angle with the receiving surface. In one embodiment, the second angle is between 0 and 90 degrees (e.g., between 0 and 80 degrees, between 0 and 70 degrees, between 0 and 60 degrees, between 0 and 50 degrees, between 0 and 40 degrees, between 0 and 30 degrees, between 0 and 20 degrees, between 0 and 10 degrees, between 10 and 80 degrees, between 10 and 70 degrees, between 10 and 60 degrees, between 10 and 50 degrees, between 10 and 40 degrees, between 10 and 30 degrees, between 10 and 20 degrees, between 20 and 80 degrees, between 30 and 80 degrees, between 40 and 80 degrees, between 50 and 80 degrees, between 10 and 50 degrees, and 0 to 45 degrees). In another embodiment, the second angle is between 0 and −90 degrees (e.g., between 0 and −80 degrees, between 0 and −70 degrees, between 0 and −60 degrees, between 0 and −50 degrees, between 0 and −40 degrees, between 0 and −30 degrees, between 0 and −20 degrees, between 0 and −10 degrees, between −10 and −80 degrees, between −10 and −70 degrees, between −10 and −60 degrees, between −10 and −50 degrees, between −10 and −40 degrees, between −10 and −30 degrees, between −10 and −20 degrees, between −20 and −80 degrees, between −30 and −80 degrees, between −40 and −80 degrees, between −50 and −80 degrees, between −10 and −50 degrees, and 0 to −45 degrees).
In some embodiments, the gantry offers a print volume with a first width and first height through which a part that exceeds the print volume is printed by gradually moving the part away from the print volume.
In some embodiments, the printing plane angle relative to the horizontal bed is changed to increase material throughput for a given part geometry and layer cooling rate requirement. In some embodiments, the print angle is changed so that a 3D part with overhangs or hollow sections can be printed without the need for support material, or in some cases, printed with a dramatically reduced amount of support material required (e.g., 25%, 50%, 75%, 90% or less support material required as compared to the same part being printed with traditional 3d printing technologies).
In some embodiments, the extension of the part volume beyond printer volume drives the parallel post-processing of the part by means of a separate working volume into which the part enters and machining operations are executed.
In some embodiments, the receiving surface is a rigid member with a curved surface which includes an angled bar with an internal radius, and a length spanning the width of the 3D printer's build volume in a first direction, wherein the cross-section of the rigid member is consistent along the first direction to increase the surface contact with material deposited by said 3D printer.
In another aspect, the present disclosure describes a method of printing a 3D part using a 3D printer. The method include providing a gantry of the 3D printer; providing an extruder assembly of the 3D printer wherein the extruder assembly is operably attached to the gantry (e.g., via a carriage), and wherein the extruder assembly is configured to print a material in a printing plane and the printing plane forms a first angle with a horizontal plane; rotating the extruder assembly so that the printing plane forms a second angle with the horizontal plane; and depositing a layer of the material on a receiving surface.
In some embodiments, the first angle and second angle are different. In one embodiment, the first angle is between 0 and 90 degrees (e.g., between 0 and 80 degrees, between 0 and 70 degrees, between 0 and 60 degrees, between 0 and 50 degrees, between 0 and 40 degrees, between 0 and 30 degrees, between 0 and 20 degrees, between 0 and 10 degrees, between 10 and 80 degrees, between 10 and 70 degrees, between 10 and 60 degrees, between 10 and 50 degrees, between 10 and 40 degrees, between 10 and 30 degrees, between 10 and 20 degrees, between 20 and 80 degrees, between 30 and 80 degrees, between 40 and 80 degrees, between 50 and 80 degrees, between 10 and 50 degrees, and 0 to 45 degrees). In another embodiment, the first angle is between 0 and −90 degrees (e.g., between 0 and −80 degrees, between 0 and −70 degrees, between 0 and −60 degrees, between 0 and −50 degrees, between 0 and −40 degrees, between 0 and −30 degrees, between 0 and −20 degrees, between 0 and −10 degrees, between −10 and −80 degrees, between −10 and −70 degrees, between −10 and −60 degrees, between −10 and −50 degrees, between −10 and −40 degrees, between −10 and −30 degrees, between −10 and −20 degrees, between −20 and −80 degrees, between −30 and −80 degrees, between −40 and −80 degrees, between −50 and −80 degrees, between −10 and −50 degrees, and 0 to −45 degrees).
In another embodiment, the second angle is between 0 and 90 degrees (e.g., between 0 and 80 degrees, between 0 and 70 degrees, between 0 and 60 degrees, between 0 and 50 degrees, between 0 and 40 degrees, between 0 and 30 degrees, between 0 and 20 degrees, between 0 and 10 degrees, between 10 and 80 degrees, between 10 and 70 degrees, between 10 and 60 degrees, between 10 and 50 degrees, between 10 and 40 degrees, between 10 and 30 degrees, between 10 and 20 degrees, between 20 and 80 degrees, between 30 and 80 degrees, between 40 and 80 degrees, between 50 and 80 degrees, between 10 and 50 degrees, and 0 to 45 degrees). In another embodiment, the second angle is between 0 and −90 degrees (e.g., between 0 and −80 degrees, between 0 and −70 degrees, between 0 and −60 degrees, between 0 and −50 degrees, between 0 and −40 degrees, between 0 and −30 degrees, between 0 and −20 degrees, between 0 and −10 degrees, between −10 and −80 degrees, between −10 and −70 degrees, between −10 and −60 degrees, between −10 and −50 degrees, between −10 and −40 degrees, between −10 and −30 degrees, between −10 and −20 degrees, between −20 and −80 degrees, between −30 and −80 degrees, between −40 and −80 degrees, between −50 and −80 degrees, between −10 and −50 degrees, and 0 to −45 degrees).
In another aspect, the present disclosure describes a 3D printer which includes a receiving surface for accepting the accumulation of material layers, a gantry, and an extruder assembly having a nozzle that is articulated to rotate a printing plane, wherein the extruder assembly is operably attached to the gantry (e.g., via a carriage), and the articulated nozzle is manipulated to rotate the printing plane away from parallel with the receiving surface.
In some embodiments, the receiving surface is movable. In some embodiments, the receiving surface is articulated to rotate away from parallel with a horizontal plane.
In some embodiments, the nozzle is articulated to rotate about one or more axes.
In some embodiments, the gantry offers a print volume with a certain width and height through which a part that exceeds the print volume is printed by gradually moving the part away from the print volume.
In another aspect, the present disclosure describes a method of printing a 3D part using a 3D printer. The method includes providing a gantry of the 3D printer; providing an extruder assembly of the 3D printer wherein the extruder assembly is operably attached to the gantry (e.g., via a carriage), wherein the extruder assembly comprises a nozzle and the nozzle is configured to print a material in a printing plane and the printing plane forms a first angle with a horizontal plane; rotating the nozzle so that the printing plane forms a second angle with the horizontal plane; and depositing a material layer on a receiving surface.
In some embodiments, the first angle and second angle are different. In one embodiment, the first angle is between 0 and 90 degrees (e.g., between 0 and 80 degrees, between 0 and 70 degrees, between 0 and 60 degrees, between 0 and 50 degrees, between 0 and 40 degrees, between 0 and 30 degrees, between 0 and 20 degrees, between 0 and 10 degrees, between 10 and 80 degrees, between 10 and 70 degrees, between 10 and 60 degrees, between 10 and 50 degrees, between 10 and 40 degrees, between 10 and 30 degrees, between 10 and 20 degrees, between 20 and 80 degrees, between 30 and 80 degrees, between 40 and 80 degrees, between 50 and 80 degrees, between 10 and 50 degrees, and 0 to 45 degrees). In another embodiment, the first angle is between 0 and −90 degrees (e.g., between 0 and −80 degrees, between 0 and −70 degrees, between 0 and −60 degrees, between 0 and −50 degrees, between 0 and −40 degrees, between 0 and −30 degrees, between 0 and −20 degrees, between 0 and −10 degrees, between −10 and −80 degrees, between −10 and −70 degrees, between −10 and −60 degrees, between −10 and −50 degrees, between −10 and −40 degrees, between −10 and −30 degrees, between −10 and −20 degrees, between −20 and −80 degrees, between −30 and −80 degrees, between −40 and −80 degrees, between −50 and −80 degrees, between −10 and −50 degrees, and 0 to −45 degrees). In another embodiment, the second angle is between 0 and 90 degrees (e.g., between 0 and 80 degrees, between 0 and 70 degrees, between 0 and 60 degrees, between 0 and 50 degrees, between 0 and 40 degrees, between 0 and 30 degrees, between 0 and 20 degrees, between 0 and 10 degrees, between 10 and 80 degrees, between 10 and 70 degrees, between 10 and 60 degrees, between 10 and 50 degrees, between 10 and 40 degrees, between 10 and 30 degrees, between 10 and 20 degrees, between 20 and 80 degrees, between 30 and 80 degrees, between 40 and 80 degrees, between 50 and 80 degrees, between 10 and 50 degrees, and 0 to 45 degrees). In another embodiment, the second angle is between 0 and −90 degrees (e.g., between 0 and −80 degrees, between 0 and −70 degrees, between 0 and −60 degrees, between 0 and −50 degrees, between 0 and −40 degrees, between 0 and −30 degrees, between 0 and −20 degrees, between 0 and −10 degrees, between −10 and −80 degrees, between −10 and −70 degrees, between −10 and −60 degrees, between −10 and −50 degrees, between −10 and −40 degrees, between −10 and −30 degrees, between −10 and −20 degrees, between −20 and −80 degrees, between −30 and −80 degrees, between −40 and −80 degrees, between −50 and −80 degrees, between −10 and −50 degrees, and 0 to −45 degrees).
In another aspect, the present disclosure describes systems and methods of printing a 3D part. In some embodiments, compared to a conventional 3-axis printer, the systems and methods within the scope of the present disclosure may reduce a material requirement by at least 5%, at least 10%, at least 20%, at least 30%, at least 40%, at least 50%, at least 60%, or at least 70%. In some embodiments, compared to a conventional 3-axis printer, the systems and methods within the scope of the present disclosure may reduce a material requirement by a range of between 0 and 5%, between 0 and 10%, between 0 and 20%, between 0 and 30%, between 0 and 40%, between 0 and 50%, between 0 and 60%, between 0 and 70%, between 10% and 20%, between 10% and 30%, between 10% and 40%, between 10% and 50%, between 10% and 60%, between 10% and 70%.
The foregoing and other objects, aspects, features, and advantages of the present disclosure will become more apparent and better understood by referring to the following description taken in conjunction with the accompanying drawing.
The features and advantages of the present disclosure will become more apparent from the detailed description set forth below when taken in conjunction with the drawing, in which like reference characters identify corresponding elements throughout. In the drawing, like reference numbers generally indicate identical, functionally similar, and/or structurally similar elements. The figures are not drawn to scale since the variation in size of various elements in the Figures is too great to permit depiction to scale.
DETAILED DESCRIPTIONIt is contemplated that systems, architectures, devices, methods, and processes of the claimed invention encompass variations and adaptations developed using information from the embodiments described herein. Adaptation and/or modification of the systems, architectures, devices, methods, and processes described herein may be performed, as contemplated by this description.
Throughout the description, where articles, devices, systems, and architectures are described as having, including, or comprising specific components, or where processes and methods are described as having, including, or comprising specific steps, it is contemplated that, additionally, there are articles, devices, systems, and architectures of the present invention that consist essentially of, or consist of, the recited components, and that there are processes and methods according to the present invention that consist essentially of, or consist of, the recited processing steps.
It should be understood that the order of steps or order for performing certain action is immaterial so long as the invention remains operable. Moreover, two or more steps or actions may be conducted simultaneously.
Elements of embodiments described with respect to a given aspect of the invention may be used in various embodiments of another aspect of the invention. For example, it is contemplated that features of dependent claims depending from one independent claim can be used in apparatus, articles, systems, and/or methods of any of the other independent claims.
The mention herein of any publication, for example, in the Background section, is not an admission that the publication serves as prior art with respect to any of the claims presented herein. The Background section is presented for purposes of clarity and is not meant as a description of prior art with respect to any claim.
As used herein, unless otherwise clear from context, (i) the term “a” may be understood to mean “at least one”; (ii) the term “or” may be understood to mean “and/or”; (iii) the terms “comprising” and “including” may be understood to encompass itemized components or steps whether presented by themselves or together with one or more additional components or steps; and (iv) where ranges are provided, endpoints are included.
As used herein, the terms “about” or “approximately”, when used herein in reference to a value, refers to a value that is similar, in context to a referenced value. In general, those skilled in the art, familiar with the context, will appreciate the relevant degree of variance encompassed by “about” or “approximately” in that context. For example, in some embodiments, the terms “about” or “approximately” may encompass a range of values that within 25%, 20%, 19%, 18%, 17%, 16%, 15%, 14%, 13%, 12%, 11%, 10%, 9%, 8%, 7%, 6%, 5%, 4%, 3%, 2%, 1%, or less of the referred value.
As used herein, the term “substantially” refers to the qualitative condition of exhibiting total or near-total extent or degree of a characteristic or property. For example, a substantially constant value may vary in time by 20%, 15%, 10%, 9%, 8%, 7%, 6%, 5%, 4%, 3%, 2%, 1%, or less of the constant value.
A conventional 3-axis 3D printer shown in
Additional external support structures or infills add to the cost of the 3D part as they consume material which is later removed and discarded. They also increase the total print time because of the extra structures that need to be printed. After printing, the additional support structures have to be removed before the 3D part is ready for use, which adds post processing work and cost. Furthermore, because the support structures need to touch and often stick to the walls of the model, removing them after printing may cause damages the surface of the part or even the entire part accidentally.
In order to solve the above issues, the present disclosure describes, inter alia, a 3D printer that uses a variable print angle (e.g., variable during the printing process) to reduce the need for support material. As shown in
In some embodiments, the print angle is set to a certain value before the printing process begins and fixed during the printing process. In some embodiments, the print angle is variable during the printing process.
The print angle, as used herein, is defined as the angle between a printing plane and a horizontal plane. In some embodiments, the print angle may be greater than or equal to 0 degree, greater than or equal to 10 degrees, greater than or equal to 30 degrees, greater than or equal to 45 degrees, greater than or equal to 60 degrees, or greater than or equal to 90 degrees. In certain embodiments, the print angle may be less than or equal to 90 degrees, less than or equal to 75 degrees, less than or equal to 60 degrees, less than or equal to 45 degrees, less than or equal to 30 degrees, less than or equal to 15 degrees, between 0 and 80 degrees, between 0 and 70 degrees, between 0 and 60 degrees, between 0 and 50 degrees, between 0 and 40 degrees, between 0 and 30 degrees, between 0 and 20 degrees, between 0 and 10 degrees, between 10 and 80 degrees, between 10 and 70 degrees, between 10 and 60 degrees, between 10 and 50 degrees, between 10 and 40 degrees, between 10 and 30 degrees, between 10 and 20 degrees, between 20 and 80 degrees, between 30 and 80 degrees, between 40 and 80 degrees, between 50 and 80 degrees, between 10 and 50 degrees, and 0 to 45 degrees. In another embodiment, the print angle is between 0 and −90 degrees (e.g., between 0 and −80 degrees, between 0 and −70 degrees, between 0 and −60 degrees, between 0 and −50 degrees, between 0 and −40 degrees, between 0 and −30 degrees, between 0 and −20 degrees, between 0 and −10 degrees, between −10 and −80 degrees, between −10 and −70 degrees, between −10 and −60 degrees, between −10 and −50 degrees, between −10 and −40 degrees, between −10 and −30 degrees, between −10 and −20 degrees, between −20 and −80 degrees, between −30 and −80 degrees, between −40 and −80 degrees, between −50 and −80 degrees, between −10 and −50 degrees, and 0 to −45 degrees). Other ranges are also possible.
The print bed 202 can include a receiving surface for accepting a printing material and provide mechanical support for a 3D part during the printing process and it can be fixed or movable. In some embodiments, the print bed 202 includes a fixed receiving surface. In some embodiments, the print bed 202 includes a moving mechanism such as a moving table, a movable belt or a plurality of pulleys. A printing material can be deposited on the print bed directly or indirectly. In some embodiments, a material is directly printed on the print bed 202 to form a layer that adheres to the print bed. In some embodiments, a material is printed on one or more intermediate layers that are directly printed onto the receiving surface of the print bed 202. The print bed 202 can include a temperature control mechanism. In some embodiments, the print bed 202 is heated to an elevated temperature during printing. In one embodiment, the elevated temperature is between 0 and 200° C. (e.g., between 0 and 180° C., between 0 and 160° C., between 0 and 140° C., between 0 and 120° C., between 0 and 100° C., between 0 and 80° C., between 0 and 60° C., between 20° C. and 200° C., between 40° C. and 180° C., between 60° C. and 160° C., between 80° C. and 140° C., and between 100° C. and 120° C.). In some embodiments, the print bed 202 is cooled during printing. In one embodiment, the print bed 202 is cooled by one or more fans.
The gantry 204 can be configured to move in a certain direction over the print bed 202 and provide support for the x-carriage and z-carriage. As shown in
In some embodiments, the printer is a delta printer which comprises one or more arms on rails to move an extruder assembly. In some embodiments, the printer comprises a robotic arm that an extruder assembly is mounted on.
In some embodiments, the print bed 202 is fixed while the gantry 204 moves over the print bed 202 during a printing process. In some embodiments, the gantry 204 is fixed while a receiving surface of the print bed 202 moves in a direction during a printing process. In some embodiments, the gantry 204 and the receiving surface of the print bed 202 are both movable.
The x-carriage 206 and z-carriage 208 can be mounted on the shaft of the gantry 204 and move along the shaft in the x-axis and z-axis, respectively. In the embodiment shown in
The extruder assembly 210 can be mounted on the x-carriage or z-carriage. As shown in
The schematics in
The systems and methods described herein can be employed to convert an existing 3-axis printer into a 5-axis printer. In some embodiments, an extruder assembly of the existing 3-axis printer is replaced with a rotatable extruder assembly. In some embodiments, only a nozzle of the existing 3-axis printer is replaced with a rotatable nozzle.
In some embodiments, varying the nozzle location can be achieved by rotating the nozzle in the one or more planes (e.g., x-z and/or y-z planes). In some embodiments, varying the nozzle location can be achieved by rotating the nozzle in one plane (e.g., x-z or y-z plane) to achieve the desired angle and then rotating the shaft of the nozzle about the z-axis to achieve the desired direction.
One common configuration of a conventional 3D printer (e.g., a 3-axis printer), shown in
In some embodiments, this present disclosure describes a 3D printer that allows parts to be printed through the gantry build envelope and oriented in the y-direction for infinite length printing, uncoupling the part longitudinal size requirements from actual machine volume. An aspect of the invention shown in
In some embodiments, the extruder assembly rotates about two or more axes. For example, similar to the 3D printer shown in
Traditional 3D Printers have a limited range of allowed time between sequentially printed layers, referred to as allowed layer time. If the actual layer time during printing is too short, the previous layer is still hot and soft to print on. On the other hand, if the actual layer time during printing is too long, the previous layer has cooled and gives poor interlayer adhesion. Hence layers with large cross-sections may take too long to print which results in failure to adhere to previous layers, and layers with small cross-sections must be printed slowly which results in a reduction of the machine throughput. Varying the print angle for a given part allows the layer time to be improved for a large range of part geometries and allows for a wider range of part sizes that can be printed closer to the optimal speed settings to increase throughput.
For example,
In general, the layer time t depends on multiple factors including i) the cross sectional area of the 3D part to be printed, ii) the print speed of the 3D printer, and iii) the bead width. With a constant print speed and bead width, a larger cross section will lead to a longer layer time. The cross sectional area can be greatly affected by the print angle θ. As shown in
Similarly, with the cross sectional area and the bead width unchanged, increasing the print speed will shorten the layer time. While decreasing bead width may be needed to print delicate features on a 3D part, it will inevitably lead to more passes for the same print area and therefore a longer layer time.
The allowed maximum and minimum layer time are determined, at least in part, by the bead width and the properties of the print material such as its melting temperature and glass transition temperature Tg. If the layer time is less than the allowed minimum layer time, the previous layer is still hot and soft while the new layer is being printed on top of it, which may cause the deformation of the 3D part. If the layer time is greater than the allowed maximum layer time, the previous layer has cooled substantially and gives poor interlayer adhesion between the layers. Therefore, it is desirable to maintain a layer time between the allowed maximum layer time and the allowed minimum layer time to achieve a satisfactory printing quality.
For example, as shown in
The need for support structures can be mitigated, in part, by reorientation of the part so that the longitudinal axis aligns with the vertical direction, as shown in
In some embodiments, compared to a conventional 3-axis printer, the systems and methods within the scope of the present disclosure may reduce a material requirement by at least 5%, at least 10%, at least 20%, at least 30%, at least 40%, at least 50%, at least 60%, or at least 70%. In some embodiments, compared to a conventional 3-axis printer, the systems and methods within the scope of the present disclosure may reduce a material requirement by a range of between 0 and 5%, between 0 and 10%, between 0 and 20%, between 0 and 30%, between 0 and 40%, between 0 and 50%, between 0 and 60%, between 0 and 70%, between 10% and 20%, between 10% and 30%, between 10% and 40%, between 10% and 50%, between 10% and 60%, between 10% and 70%.
Referring to
When printing a complicated 3D part, the orientation of design features may affect the final accuracy, build time and strength of the final 3D part. A 3-axis printer cannot easily change print angle, and therefore, the entire part is usually printed with a fixed print angle. As in a design 608 shown in
Still referring to
One cost-saving application of 3D printing is the capability to produce parts at near-net shape. The progression toward final part geometry therefore typically requires machining operations to be performed on the part after printing has completed. Machining can be performed on a printed part within one of two logistical schemes: either in-situ operations are performed, where the machining volume coexists with the printing volume, or separate machining and printing volumes exist, and the part is transitioned between them. Both schemes develop serially, where the machining operation cannot begin until the printing operation has completed sufficiently.
Conventional post-processing of parts requires moving the part outside of the printing space into a separate post-processing space or through successive, in-situ print and post-processing operations within a shared space. Post-processing therefore requires greater logistical complexity and associated cost when moving parts out of the printing space and into a separate post-processing space, or increased machine complexity and associated cost for in-situ operations. The present disclosure describes a system and method to create separate process spaces for printing and post-processing at little added logistical or machine complexity.
Referring to
Referring to
It is desirable during the course of a printing process to keep consistent inter-layer adhesion to prevent delamination of material. The adhesion between the first layer and the bed for conventional 3-axis printing is similarly important as delamination tends to propagate through the vertical dimension of the part and lead to failures. As the angle between the printing plane and build surface plane is varied the downward pressure normal to a horizontal build surface reduces. The present disclosure describes a system and method of using a shaped receiver for the first bead which allows a more consistent bead pressure and improves adhesion.
Referring to
Throughout the description, where apparatus and systems are described as having, including, or comprising specific components, or where processes and methods are described as having, including, or comprising specific steps, it is contemplated that, additionally, there are apparatus, and systems of the present invention that consist essentially of, or consist of, the recited components, and that there are processes and methods according to the present invention that consist essentially of, or consist of, the recited processing steps.
It should be understood that the order of steps or order for performing certain action is immaterial so long as the invention remains operable. Moreover, two or more steps or actions may be conducted simultaneously.
While the invention has been particularly shown and described with reference to specific preferred embodiments, it should be understood by those skilled in the art that various changes in form and detail may be made therein without departing from the spirit and scope of the invention as defined by the appended claims.
Claims
1. A 3D printer comprising:
- a receiving surface for accepting the accumulation of material layers; and
- a gantry; and
- an extruder assembly that is articulated to rotate a printing plane;
- wherein the extruder assembly is operably attached to the gantry (e.g., via a carriage), and the articulated extruder assembly is manipulated to rotate the printing plane away from parallel with the receiving surface.
2. The 3D printer of claim 1, wherein the receiving surface is movable.
3. The 3D printer of claim 1, wherein the receiving surface include a flat belt.
4. The 3D printer of claim 1, wherein the receiving surface comprises a plurality of pulleys.
5. The 3D printer of claim 1, wherein the receiving surface is articulated to rotate away from parallel with a horizontal plane.
6. The 3D printer of claim 1, wherein the extruder assembly is articulated to rotate about one or more axes.
7. The 3D printer of claim 1, wherein the extruder assembly is articulated to rotate and form a first angle with the receiving surface.
8. The 3D printer of claim 7, wherein the first angle is between 0 and 90 degrees.
9. The 3D printer of claim 7, wherein the first angle is between 45 and 90 degrees.
10. The 3D printer of claim 1, wherein the extruder assembly comprises a nozzle and the nozzle is articulated to rotate about one or more axes.
11. The 3D printer of claim 10, wherein the nozzle is articulated to rotate and form a second angle with the receiving surface.
12. The 3D printer of claim 11, wherein the second angle is between 0 and 90 degrees.
13. The 3D printer of claim 11, wherein the second angle is between 45 and 90 degrees.
14. The 3D printer of claim 1, wherein the gantry offers a print volume with a first width and first height through which a part that exceeds the print volume is printed by gradually moving the part away from the print area.
15. The 3D printer of claim 1, wherein a printing plane angle relative to the horizontal bed is changed to increase material throughput for a given part geometry and layer cooling rate requirement.
16. The 3D printer of claim 14, wherein the extension of the part volume beyond printer volume drives the parallel post-processing of the part by means of a separate working volume into which the part enters and machining operations are executed.
17. The 3D printer of claim 1, wherein the receiving surface is a rigid member with a curved surface comprising:
- an angled bar with an internal radius; and
- a length spanning the width of the 3D printer's build volume in a first direction;
- wherein the cross-section of the rigid member is consistent along the first direction to increase the surface contact with material deposited by said 3D printer.
18. A method of printing a 3D part using a 3D printer, comprising:
- providing a gantry of the 3D printer;
- providing an extruder assembly of the 3D printer, wherein the extruder assembly is operably attached to the gantry (e.g., via a carriage), and wherein the extruder assembly is configured to print a material in a printing plane and the printing plane forms a first angle with a horizontal plane;
- rotating the extruder assembly so that the printing plane forms a second angle with the horizontal plane; and
- depositing a layer of the material on a receiving surface.
19. The method of claim 18, wherein the first angle and second angle are different.
20. The method of claim 19, wherein the first angle is between 0 and 90 degrees.
21. The method of claim 19, wherein the second angle is between 0 and 90 degrees.
22. A 3D printer comprising:
- a receiving surface for accepting the accumulation of material layers; and
- a gantry; and
- an extruder assembly having a nozzle that is articulated to rotate a printing plane;
- wherein the extruder assembly is operably attached to the gantry (e.g., via a carriage), and the articulated nozzle is manipulated to rotate the printing plane away from parallel with the receiving surface.
23. The 3D printer of claim 22, wherein the receiving surface is movable.
24. The 3D printer of claim 22, wherein the receiving surface is articulated to rotate away from parallel with a horizontal plane.
25. The 3D printer of claim 22, wherein the nozzle is articulated to rotate about one or more axes.
26. The 3D printer of claim 22, wherein the gantry offers a print volume with a certain width and height through which a part that exceeds the print volume is printed by gradually moving the part away from the print volume.
27. A method of printing a 3D part using a 3D printer, comprising:
- providing a gantry of the 3D printer;
- providing an extruder assembly of the 3D printer wherein the extruder assembly is operably attached to the gantry (e.g., via a carriage), wherein the extruder assembly comprises a nozzle and the nozzle is configured to print a material in a printing plane and the printing plane forms a first angle with a horizontal plane;
- rotating the nozzle so that the printing plane forms a second angle with the horizontal plane; and
- depositing a material layer on a receiving surface.
28. The method of claim 27, wherein the first angle and second angle are different.
29. The method of claim 27, wherein the first angle is between 0 and 90 degrees.
30. The method of claim 27, wherein the second angle is between 0 and 90 degrees.
Type: Application
Filed: Aug 6, 2019
Publication Date: Sep 2, 2021
Inventors: James M. Anderson (Hampden, ME), Matthew J. Ireland (Old Town, ME)
Application Number: 17/262,275