Apparatus and method for conditioning a polishing pad used for mechanical and/or chemical-mechanical planarization
Conditioning apparatuses and methods for conditioning polishing pads used for mechanical and/or chemical-mechanical planarization of micro-device workpieces are disclosed herein. In one embodiment, a method for conditioning a polishing pad used for polishing a micro-device workpiece includes monitoring surface condition in a first region of the polishing pad and adjusting at least one of a rotational velocity of the polishing pad, a downforce on the polishing pad, and a sweep velocity of the end effector in response to the monitored surface condition to provide a desired texture in the first region. In another embodiment, an apparatus for conditioning the polishing pad includes an end effector, a monitoring device, and a controller operatively coupled to the end effector and the monitoring device. The controller has a computer-readable medium containing instructions to perform a conditioning method, such as the above-mentioned method.
Latest Micron Technology, Inc. Patents:
- ITERATIVE DECODING TECHNIQUE FOR CORRECTING DRAM DEVICE FAILURES
- ITERATIVE ERROR CORRECTION IN MEMORY SYSTEMS
- Integrated Assemblies Comprising Hydrogen Diffused Within Two or More Different Semiconductor Materials, and Methods of Forming Integrated Assemblies
- APPARATUSES AND METHODS FOR ECC PARITY BIT REDUCTION
- NONLINEAR DRAM DIGITAL EQUALIZATION
The present invention relates to an apparatus and method for conditioning a polishing pad used for mechanical and/or chemical-mechanical planarization of micro-device workpieces.
BACKGROUND Mechanical and chemical-mechanical planarization processes (collectively “CMP”) remove material from the surface of micro-device workpieces in the production of microelectronic devices and other products.
The carrier head 30 has a lower surface 32 to which a micro-device workpiece 12 may be attached, or the workpiece 12 may be attached to a resilient pad 34 under the lower surface 32. The carrier head 30 may be a weighted, free-floating wafer carrier, or an actuator assembly 36 may be attached to the carrier head 30 to impart rotational motion to the micro-device workpiece 12 (indicated by arrow J) and/or reciprocate the workpiece 12 back and forth (indicated by arrow 1).
The planarizing pad 40 and a planarizing solution 44 define a planarizing medium that mechanically and/or chemically-mechanically removes material from the surface of the micro-device workpiece 12. The planarizing solution 44 may be a conventional CMP slurry with abrasive particles and chemicals that etch and/or oxidize the surface of the micro-device workpiece 12, or the planarizing solution 44 may be a “clean” nonabrasive planarizing solution without abrasive particles. In most CMP applications, abrasive slurries with abrasive particles are used on nonabrasive polishing pads, and clean nonabrasive solutions without abrasive particles are used on fixed-abrasive polishing pads.
To planarize the micro-device workpiece 12 with the CMP machine 10, the carrier head 30 presses the workpiece 12 face-down against the planarizing pad 40. More specifically, the carrier head 30 generally presses the micro-device workpiece 12 against the planarizing solution 44 on a planarizing surface 42 of the planarizing pad 40, and the platen 20 and/or the carrier head 30 moves to rub the workpiece 12 against the planarizing surface 42. As the micro-device workpiece 12 rubs against the planarizing surface 42, the planarizing medium removes material from the face of the workpiece 12.
The CMP process must consistently and accurately produce a uniformly planar surface on the micro-device workpiece 12 to enable precise fabrication of circuits and photo-patterns. One problem with conventional CMP methods is that the planarizing surface 42 of the planarizing pad 40 can wear unevenly or become glazed with accumulations of planarizing solution 44 and/or material removed from the micro-device workpiece 12 and/or planarizing pad 40. To restore the planarizing characteristics of the planarizing pad 40, the pad 40 is typically conditioned by removing the accumulations of waste matter with an abrasive conditioning disk 50. The conventional abrasive conditioning disk 50 is generally embedded with diamond particles and mounted to a separate actuator 55 that moves the conditioning disk 50 rotationally, laterally, and/or axially, as indicated by arrows A, B, and C, respectively. The typical conditioning disk 50 removes a thin layer of the planarizing pad material in addition to the waste matter to form a new, clean planarizing surface 42 on the planarizing pad 40.
During the conditioning process, the conditioning disk 50 imparts texture to the planarizing pad 40. One problem with conventional conditioning methods is that even if the conditioning disk 50 uniformly removes the planarizing pad material, different textures are formed across the planarizing pad 40. Differences in texture across the planarizing pad 40 can cause the pad 40 to remove material at different rates across the micro-device workpiece 12 during the CMP process. Differences in texture can also produce defects on the micro-device workpiece 12. Consequently, the CMP process may not produce a uniformly planar surface on the micro-device workpiece 12.
SUMMARYThe present invention is directed toward conditioning apparatuses and methods for conditioning polishing pads used for mechanical and/or chemical-mechanical planarization of micro-device workpieces. In one embodiment, a method for conditioning a polishing pad includes determining surface condition in a first region of the polishing pad, determining surface condition in a second region of the polishing pad, and adjusting at least one of a relative velocity between the polishing pad and an end effector, an existing downforce on the polishing pad, and a sweep velocity of the end effector in response to the determined surface condition of the first region to provide a desired first surface texture in the first region. The method further includes adjusting at least one of the relative velocity between the polishing pad and the end effector, the existing downforce on the polishing pad, and the sweep velocity of the end effector in response to the determined surface condition of the second region to provide a desired second surface texture in the second region. In a further aspect of this embodiment, determining surface condition can include sensing surface texture, roughness, and/or asperities. In another aspect of this embodiment, determining surface condition can occur while the polishing pad is in-situ, rotating, and/or stationary.
In another embodiment of the invention, a method for conditioning the polishing pad includes monitoring surface condition in the first region of the polishing pad and adjusting at least one of a rotational velocity of the polishing pad, the downforce on the polishing pad, and the sweep velocity of the end effector in response to the monitored surface condition to provide the desired texture in the first region.
In another embodiment of the invention, an apparatus for conditioning the polishing pad includes an end effector, a monitoring device, and a controller operatively coupled to the end effector and the monitoring device. In one aspect of this embodiment, the controller has a computer-readable medium containing instructions to perform a method including determining surface condition in the first region of the polishing pad, determining surface condition in the second region of the polishing pad, and adjusting at least one of the relative velocity between the polishing pad and the end effector, the existing downforce on the polishing pad, and the sweep velocity of the end effector in response to the determined surface condition of the first region to provide the desired first surface texture in the first region. The method further includes adjusting at least one of the relative velocity between the polishing pad and the end effector, the existing downforce on the polishing pad, and the sweep velocity of the end effector in response to the determined surface condition of the second region to provide a desired second surface texture in the second region.
In another aspect of this embodiment, the controller has a computer-readable medium containing instructions to perform a method including monitoring surface condition in the first region of the polishing pad, and adjusting at least one of the rotational velocity of the polishing pad, the downforce on the polishing pad, and the sweep velocity of the end effector in response to the monitored surface condition to provide the desired texture in the first region.
BRIEF DESCRIPTION OF THE DRAWINGS
The present invention is directed to apparatuses and methods for conditioning polishing pads used for mechanical and/or chemical-mechanical planarization of micro-device workpieces. The term “micro-device workpiece” is used throughout to include substrates in and/or on which micro-electronic devices, micro-mechanical devices, data storage elements, and other features are fabricated. For example, micro-device workpieces can be semi-conductor wafers, glass substrates, insulated substrates, or many other types of substrates. Furthermore, the terms “planarization” and “planarizing” mean either forming a planar surface and/or forming a smooth surface (e.g., “polishing”). Several specific details of the invention are set forth in the following description and in
In the illustrated embodiment, the conditioning system 100 includes a monitoring device 160, a controller 170, and an end effector 180. The end effector 180 can include an arm 182 and a conditioning disk 150 coupled to the arm 182 to exert a downforce FD against the planarizing pad 140. The conditioning disk 150 is generally imbedded with diamond particles to remove waste matter and a thin layer of the planarizing pad 140. The conditioning disk 150 forms a new clean planarizing surface 142 on the planarizing pad 140. The conditioning disk 150 rotates (indicated by arrow A) with a rotational velocity ω1 to abrade the planarizing pad 140 with the diamond particles. In the illustrated embodiment, the arm 182 can sweep the conditioning disk 150 across the planarizing surface 142 in a direction S with a sweep velocity SV. The sweep velocity SV can change as the conditioning disk 150 moves across the planarizing surface 142 so that the disk 150 contacts different areas on the planarizing surface 142 for different dwell times. In the illustrated embodiment, the conditioning disk 150 conditions the planarizing pad 140 in-situ and in real-time with the planarization process. In other embodiments, conditioning and planarization may not occur concurrently.
The monitoring device 160 monitors the surface condition of the planarizing surface 142. For example, the monitoring device 160 can determine the surface texture, roughness, and/or asperities of the planarizing surface 142. The monitoring device 160 can be stationary or movable relative to the CMP machine 110 to monitor the entire planarizing surface 142 of the planarizing pad 140 when the pad 140 is stationary or while it rotates. In one embodiment, the monitoring device 160 can include an optical analyzer, such as an interferometer or a device that measures the scatter of light. In other embodiments, the monitoring device 160 can use contact methods, such as frictional forces, or profilometry to monitor the surface condition. In any of these embodiments, the monitoring device 160 can monitor a single region or a plurality of monitoring devices can monitor multiple regions on the planarizing pad 140 concurrently. For example, the planarizing surface 142 of the planarizing pad 140 can be analyzed by organizing the pad 140 into known regions, such as a first region R1, a second region R2, and a third region R3. The monitoring device 160 can monitor the surface condition in the first, second, and third regions R1, R2, and R3 simultaneously. In other embodiments, the monitoring device 160 may monitor only one region at a time. In still other embodiments, a single monitoring device could be movable to monitor more than one region.
The controller 170 is operatively coupled to a platen 120, the actuator assembly 136, the monitoring device 160, and the end effector 180 to control the conditioning process. The controller 170 controls the conditioning process by adjusting certain process variables to provide a desired surface texture across the planarizing pad 140. For example, the controller 170 can adjust the relative velocity between the planarizing pad 140 and the end effector 180, the downforce FD of the end effector 180 on the planarizing pad 140, and/or the sweep velocity SV of the end effector 180 to provide the desired texture on the planarizing surface 142. The controller 170 can adjust the relative velocity between the planarizing pad 140 and the end effector 180 by changing the speed at which the platen 120 rotates. Accordingly, the controller 170 regulates the conditioning process to provide a desired surface condition. In one embodiment, the controller 170 can include a computer; in other embodiments, the controller 170 can include a hardwired circuit board.
Referring to
In one embodiment, for example, the controller 170 can vary the dwell time Dt of the conditioning disk 150 and the platen's rotational velocity Ω to maintain a constant relative velocity Vr between the planarizing pad 140 and the conditioning disk 150 to provide a uniform surface texture across the pad 140. If the required relative velocity Vr is known, the platen's rotational velocity ΩR at a radius R can be determined by the following formula:
The dwell time Dt(R) of the conditioning disk 150 at the radius R can be determined by the following formula:
where Cl is the length of conditioning and rc is the radius of the conditioning disk 150, assuming the required length of conditioning Cl is known. In other embodiments, the downforce FD can be adjusted, such as when the conditioning disk 150 conditions the edge of the planarizing pad 140 and a portion of the disk 150 hangs over the pad 140.
One advantage of the conditioning systems in the illustrated embodiments is the ability to control both the surface texture and the surface contour in real-time throughout the conditioning cycle. For example, the conditioning systems can provide a first desired surface texture in a first region of the planarizing pad and a second desired surface texture in a second region of the pad. The conditioning systems can also provide a uniform surface texture across the planarizing pad so that material can be removed from a micro-device workpiece uniformly across the workpiece during the CMP process. A uniform surface texture can also reduce defects on the micro-device workpiece.
From the foregoing, it will be appreciated that specific embodiments of the invention have been described herein for purposes of illustration, but that various modifications may be made without deviating from the spirit and scope of the invention. Accordingly, the invention is not limited except as by the appended claims.
Claims
1-53. (canceled)
54. An apparatus for conditioning a polishing pad used for polishing a micro-device workpiece, comprising:
- an end effector;
- a monitoring device; and
- a controller operatively coupled to the end effector and the monitoring device, the controller having a computer-readable medium containing instructions to perform a method comprising: determining surface condition in a first region of the polishing pad; determining surface condition in a second region of the polishing pad; adjusting at least one of a relative velocity between the polishing pad and the end effector, an existing downforce on the polishing pad, and a sweep velocity of the end effector in response to the determined surface condition of the first region to provide a desired first surface texture in the first region; and adjusting at least one of the relative velocity between the polishing pad and the end effector, the existing downforce on the polishing pad, and the sweep velocity of the end effector in response to the determined surface condition of the second region to provide a desired second surface texture in the second region.
55. The apparatus of claim 54 wherein the monitoring device comprises an optical analyzer.
56. The apparatus of claim 54 wherein the monitoring device comprises a load cell configured to measure a frictional force in a plane defined by the polishing pad.
57. The apparatus of claim 54 wherein the end effector comprises abrasive elements for abrading the polishing pad.
58. The apparatus of claim 54 wherein the monitoring device is configured to sense the surface condition of the polishing pad.
59. An apparatus for conditioning a polishing pad used for polishing a micro-device workpiece, comprising:
- an end effector;
- a sensor; and
- a controller operatively coupled to the end effector and the sensor, the controller having a computer-readable medium containing instructions to perform a method comprising: monitoring surface condition in a first region of the polishing pad; and adjusting at least one of a rotational velocity of the polishing pad, a downforce on the polishing pad, and a sweep velocity of the end effector in response to the monitored surface condition to provide a desired texture in the first region.
60. The apparatus of claim 59 wherein the sensor comprises an optical sensor.
61. The apparatus of claim 59 wherein the sensor comprises a load cell configured to measure a frictional force in a plane defined by the polishing pad.
62. The apparatus of claim 59 wherein the sensor is configured to detect the surface condition of the polishing pad.
63. The apparatus of claim 59 wherein the sensor is configured to continuously monitor the surface condition of the polishing pad.
64. An apparatus for conditioning a polishing pad used for polishing a micro-device workpiece, comprising:
- an end effector;
- a means for sensing surface condition; and
- a controller operatively coupled to the end effector and the means for sensing, the controller having a computer-readable medium containing instructions to perform a method comprising: determining roughness of surface texture in a first region of the polishing pad; and controlling at least one of a rotational velocity of the polishing pad, a downforce on the polishing pad and a sweep velocity of the end effector in response to the determined roughness to provide a desired texture in the first region.
65. The apparatus of claim 64 wherein the means for sensing comprises an optical analyzer.
66. The apparatus of claim 64 wherein the means for sensing comprises a load cell configured to measure a frictional force in a plane defined by the polishing pad.
67. An apparatus for conditioning a polishing pad used for polishing a micro-device workpiece, comprising:
- an end effector;
- a monitoring device; and
- a controller operatively coupled to the end effector and the monitoring device, the controller having a computer-readable medium containing instructions to perform a method comprising: engaging an end effector with the polishing pad and moving at least one of the end effector and the polishing pad relative to the other; monitoring surface condition in a first region of the polishing pad; and providing a desired texture in the first region of the polishing pad by regulating at least one of a relative velocity between the polishing pad and the end effector, a downforce on the polishing pad, and a sweep velocity of the end effector in response to the monitored surface condition of the first region.
68. The apparatus of claim 67 wherein the monitoring device comprises an optical analyzer.
69. The apparatus of claim 67 wherein the monitoring device comprises a load cell configured to measure a frictional force in a plane defined by the polishing pad.
Type: Application
Filed: May 3, 2006
Publication Date: Sep 7, 2006
Applicant: Micron Technology, Inc. (Boise, ID)
Inventor: Theodore Taylor (Boise, ID)
Application Number: 11/416,867
International Classification: B24B 51/00 (20060101); B24B 49/00 (20060101);