Patents Assigned to Mitsui
-
Patent number: 6579568Abstract: This invention provides a copper foil for a printed wiring board, which comprises a copper foil, an alloy layer (A) comprising copper, zinc, tin and nickel which is formed on a surface of the copper foil, said surface to be brought into contact with a substrate for a printed wiring board, and a chromate layer which is formed on a surface of the alloy layer (A). The copper foil for a printed wiring board has the following features: even if a printed wiring board is produced using a long-term stored copper foil, the interface between the copper foil and the substrate is only slightly corroded with chemicals; even if the copper foil contacts a varnish containing an organic acid, e.g., a varnish for an acrylic resin, in the formation of a copper-clad laminate, the bond strength is sufficient.Type: GrantFiled: October 26, 2001Date of Patent: June 17, 2003Assignee: Mitsui Mining & Smelting Co., Ltd.Inventors: Kazuhisa Fujiwara, Hiroshi Tan, Mitsuo Fujii, Masanobu Tsushima
-
Patent number: 6576321Abstract: An optical recording medium comprising a recording and a metal reflective layers on a transparent substrate having a groove, wherein the recording layer comprises an azaporphyrin metal complex dye with 1 to 4 meso-nitrogen atoms as a main component; recording and/or reproduction can be conducted using laser beams with wavelengths of &lgr;1 and &lgr;2 which is shorter than &lgr;1; a refractive index n of the recording layer is 2.0 or more at &lgr;1 and 1.8 or more at &lgr;2 as well as an attenuation coefficient k of the layer is 0.04 to 0.20 at &lgr;1 and 0.30 or less at &lgr;2; and the groove has a pitch of 0.70 to 0.85 &mgr;m, a half-value width of 0.20 to 0.Type: GrantFiled: September 19, 2001Date of Patent: June 10, 2003Assignee: Mitsui Chemicals, Inc.Inventors: Norihiko Mihara, Tadashi Koike
-
Patent number: 6576215Abstract: The process for preparing spinel-type lithium manganate according to the present invention is constituted by a process to admix the electrolyzed manganese dioxide, which is obtained by neutralizing manganese dioxide precipitated by means of electrolysis with any of potassium hydroxide, potassium carbonate and lithium hydroxide, and a lithium material and a process to subject the resulting mixture to a sintering process.Type: GrantFiled: November 29, 2000Date of Patent: June 10, 2003Assignees: Mitsui Mining & Smelting Co., Ltd., Matsushita Electric Industrial Co, Ltd.Inventors: Koichi Numata, Tsuneyoshi Kamada, Takuya Nakashima, Shinji Arimoto
-
Patent number: 6569936Abstract: According to the present invention, there is provided a rubber composition for a conveyor belt comprising (A) 100 parts by weight of an ethylene/&agr;-olefin containing 3 to 20 carbon atoms/non-conjugated polyene copolymer rubber containing a diene unit derived from special non-conjugated dienes, (B) 0.5 to 15 parts by weight of an organic peroxide, (C) 30 to 80 parts by weight of a carbon black and (D) 5 to 25 parts by weight of a softening agent. This rubber composition provides excellent mechanical strength, heat resistance (including heat aging resistance), abrasion resistance and roll processability. It is especially preferred to convey a sintered product, a coke, a cement, clinker and quicklime.Type: GrantFiled: November 22, 2000Date of Patent: May 27, 2003Assignee: Mitsui Chemicals, Inc.Inventors: Masaaki Kawasaki, Takashi Hakuta, Hidenari Nakahama, Tetsuo Tojo
-
Patent number: 6569533Abstract: A polyurethane resin having a total concentration of the urethane group and the urea group of not less than 15% by weight is prepared by reacting a diisocyanate component (e.g., an aromatic diisocyanate) with a diol component (e.g., a C2-8alkylene glycol). The repeating unit of the polyurethane resin may contain a constitutive unit of an aromatic or alicyclic compound. The polyurethane resin may be shaped into a film for use as a gas barrier film. The film may be a gas barrier composite film composed of a base film layer and a resin layer at least comprising the polyurethane resin. The present invention provides a polyurethane resin excellent in gas barrier properties against water vapor, oxygen, aromatics, and others, and a film containing the same.Type: GrantFiled: July 19, 2000Date of Patent: May 27, 2003Assignee: Mitsui Takeda Chemicals Inc.Inventors: Takashi Uchida, Tsutomu Tawa, Hiroyuki Shiraki
-
Patent number: 6569572Abstract: In a lithium battery comprising a positive electrode, a negative electrode and a gel electrolyte; the gel electrolyte is composed of at least an ester-group or ether-group aprotic polar solvent, a lithium salt and a polymeric compound, and the polymeric compound comprises a polymer of at least one compound among those expressed by an equation (I) and an equation (II). (k: zero or number of 1 or more, m: number of 1 or more, R1:CpH2p, R2:CqH2q, p≠q, p & q: integer of 1 or more, A: CH2═CH—CO— or CH2═C(CH3)—CO—, X: n-valent combination group (n: integer ranging from 1 to 4), r: zero or number of 1 or more, s: number of 1 or more, R3: CtH2t, R4: CuH2u, t≠u, t & u: integer of 1 or more).Type: GrantFiled: April 11, 2000Date of Patent: May 27, 2003Assignees: Yuasa Corporation, Mitsui Chemicals, Inc.Inventors: Seijiro Ochiai, Syuichi Izuchi, Takeshi Ishitoku, Masaharu Shindo, Hidenobu Nogi
-
Patent number: 6570025Abstract: This invention provides sulfur-containing (meth)acrylic ester compounds each of which is represented by the following formula (1); wherein R1 and R2 each independently represent a hydrogen atom or an alkyl group or may be fused together to form a ring, R3 represents a hydrogen atom or a methyl group, X1 represents an oxygen atom or a sulfur atom, m stands for an integer of from 0 to 3, and n stands for an integer of from 1 to 4, polymerizable compositions comprising the sulfur-containing (meth)acrylic acids, and cured products and optical parts obtained by polymerizing the polymerizable compositions. The sulfur-containing (meth)acrylic ester compounds according to the present invention are very useful, as monomers for photocurable, polymerizable compositions, in applications such as optical materials and dental materials.Type: GrantFiled: January 25, 2002Date of Patent: May 27, 2003Assignee: Mitsui Chemicals, Inc.Inventors: Kenichi Fujii, Atsuo Otsuji, Masao Imai, Kenichi Sugimoto, Tadashi Okuma, Rihoko Suzuki, Keisuke Takuma
-
Publication number: 20030096456Abstract: A method of manufacturing a semiconductor device. The method includes the steps of: providing a lead frame assembly with joined first and second unit lead frames, with the first unit lead frame having a first support and a plurality of leads and the second unit lead frame having a second support and a plurality of leads; mounting operating components on the first and second unit lead frames; applying a sealing composition over the lead frame assembly and the operating components to define a semiconductor preassembly; cutting the semiconductor preassembly so as to define first and second semiconductor devices, with the first and second semiconductor devices having first and second exposed edges respectively defined by cutting of the semiconductor preassembly; and moving at least the first semiconductor device against another element to break loose flash on the first exposed edge.Type: ApplicationFiled: November 8, 2002Publication date: May 22, 2003Applicant: Mitsui High-tec Inc.Inventors: Shoshi Yasunaga, Hiroaki Narimatsu, Atsushi Fukui
-
Patent number: 6565986Abstract: An olefinic thermoplastic elastomer capable of producing a sheet applicable for preparing a covering skin sheet for interior furnishings in automobile superior in the formability, heat resistance, mechnical properties, tensile characteristics, strain restorability and repulsive elasticity together with superior grain retention performance upon a male vacuum forming of the sheet, the said olefinic thermoplastic elastomer comprising an olefinic resin and an olefinic copolymer rubber and having a characteristic feature that it satisfies, when a grained sheet made of the said elatomer is subjected to a male vacuum forming at least at a point of sheet temperature within the range of 130-150° C., the condition that the grain retention rate expressed by the proportion of the grain depth of the sheet retained after the male vacuum forming relative to the grain depth before the male vacuum forming represented by percent meets the relation defined by the following equation (1) % retention of grain≧100−2.Type: GrantFiled: October 16, 2002Date of Patent: May 20, 2003Assignee: Mitsui Chemicals, Inc.Inventor: Yuichi Itoh
-
Patent number: 6566740Abstract: A lead frame for a semiconductor device. The lead frame has a layer defining a first unit lead frame including a first support for a semiconductor chip and a plurality of leads spaced around the first support. The first support has a peripheral edge. The layer further defines a guide rail extending along at least a portion of the peripheral edge and connected to at least one of the leads. At least one notch is formed in the layer between the at least one lead and a part of the guide rail so as to define a first tie bar.Type: GrantFiled: March 20, 2001Date of Patent: May 20, 2003Assignee: Mitsui High-tec, Inc.Inventors: Shoshi Yasunaga, Jun Sugimoto
-
Publication number: 20030090415Abstract: A GPS positioning system comprises a fixed station and a mobile station. The mobile station has: positional positioning means; imaging means; direction detecting means; and arithmetic processing means. The positional positioning means measures positional coordinates by receiving radio wave from a satellite. The imaging means is arranged in a predetermined position for the GPS positional positioning means. The direction detecting means detects a photographing direction during photographing by the imaging means. The arithmetic processing means forms landscape data in which imaging data that is an output from the imaging means is associated with orientation data that is an output from the direction detecting means.Type: ApplicationFiled: October 24, 2002Publication date: May 15, 2003Applicant: MITSUI & CO., LTD.Inventors: Koji Miyasaka, Masakazu Mori, Yuji Kobayashi, Kazuyuki Sakaki, Kenichi Takasu
-
Publication number: 20030092870Abstract: The aromatic diamine compound of the present invention is represented by the following formula (1), and from the aromatic diamine compound a polyimide having a repeating unit represented by the following formula (4), which has low-temperature adherability, can be obtained.Type: ApplicationFiled: September 3, 2002Publication date: May 15, 2003Applicant: Mitsui Chemicals, Inc.Inventors: Yoichi Kodama, Minehiro Mori, Naoshi Nagai, Masaru Kawaguchi
-
Patent number: 6562092Abstract: The present invention provides a stock material for cerium-based abrasives which can be sintered at a relatively low roasting temperature without causing abnormal growth of the particles. More concretely, the stock material for cerium-based abrasives is produced by calcinating the carbonate of rare earth at a given temperature level to partly convert it into the oxide of rare earth in such a way to produce the mixed stock material having a loss on ignition of 0.5 to 25% on a dry basis, determined by heating at 1000° C. for 1 hour.Type: GrantFiled: November 30, 2001Date of Patent: May 13, 2003Assignee: Mitsui Mining & Smelting Co., Ltd.Inventors: Terunori Ito, Hidehiko Yamasaki, Yoshitsugu Uchino
-
Patent number: 6562901Abstract: Present invention is a resin composition obtained by reacting polyolefin (A) with a (co)polymer (B) prepared from a copolymerizable monomer mixture (C) comprising an &agr;,&bgr;-monoethylenically unsaturated monomer and other copolymerizable monomers in a weight ratio (A)/(B)=1/9-9/1 under radical generation in an organic solvent, or by polymerizing a copolymerizable monomer mixture (C) comprising an &agr;,&bgr;-monoethylenically unsaturated monomer and other copolymerizable monomers in the presence of polyolefin (A) in a weight ratio (A)/(C)=1/9-9/1 in an organic solvent and successively by reacting the obtained reaction mass under radical generation; and the resin composition has good solution stability, does not cause liquid phase separation or solid precipitation, can be used as intact, is excellent in sprayability at high concentration, and, specifically, has novel function and effect that adhesion to polyolefin molded articles is excellent; and the resin composition can be favorably used fType: GrantFiled: February 23, 2001Date of Patent: May 13, 2003Assignee: Mitsui Chemicals, Inc.Inventors: Keiichi Asami, Taisaku Kano, Koichi Machida, Tsukasa Murakami
-
Patent number: 6563199Abstract: A semiconductor device having a unit lead frame defining a support with a peripheral edge and a first lead spaced from the peripheral edge. The first lead has a recess formed therein. A semiconductor chip is provided on the support. A conductive element electrically connects between the semiconductor chip and the first lead. The resin layer on the semiconductor chip and the first lead extends into the recess. The invention is also directed to a unit lead frame that is part of the semiconductor device, a lead frame incorporating a plurality of unit lead frames, and a method of manufacturing semiconductor devices.Type: GrantFiled: March 20, 2001Date of Patent: May 13, 2003Assignee: Mitsui High-tec Inc.Inventors: Shoshi Yasunaga, Takahiro Ishibashi
-
Patent number: 6563579Abstract: The present invention relates to an internal quality measuring apparatus for measuring an internal quality of an object, and the apparatus has a conveying device, a detecting device, a light projecting device, a light receiving device, an analyzing device and a pseudo-object member interposing device, and the analyzing device compares light received with a pseudo-object member, with reference data preliminarily stored, and correct a result of the analysis, based thereon.Type: GrantFiled: June 1, 2000Date of Patent: May 13, 2003Assignee: Mitsui Mining & Smelting Co., Ltd.Inventors: Mikio Kimura, Toyohiko Aoki, Hirotsugu Hashimoto, Takeshi Ota, Akihiko Fujita
-
Patent number: 6562155Abstract: A process for producing an aluminum alloy semi-molten billet for use as a transporation unit, including the steps of: producing an aluminum alloy having a composition consisting essentially of, in weight %, 0.5 or less Cu, 5.0 to 10.0 Si, 0.2 to 0.7 Mg, 0.35 or less Zn, 0.55 or less Fe, 0.5 or less Mn, 0.005 to 0.5 Ti, and the balance aluminum; introducing working strain into a melt of the aluminum alloy by means of molding flask-assisted cold forging at a distortion rate of 10 to 40%, at a working introduction velocity of 10 mm or less per second, and at a temperature of 200° C. or lower; and, thereafter heat-treating such a strain introduced melt at temperatures in a range of 576 to 585° C.Type: GrantFiled: September 18, 2000Date of Patent: May 13, 2003Assignee: Kyusyu Mitsui, Aluminum Co., Ltd.Inventors: Shigeru Mikubo, Masafumi Mizouti, Yasuyuki Murayama, Tsunaki Iwashita, Akihiko Kamio, Tatsuo Sato
-
Publication number: 20030088125Abstract: An amide composition containing an unsaturated amide, a sulfur-containing compound, and a weak acid salt. The composition can include an amide in crystalline form or the composition can be in form of aqueous solution. The composition can exhibit improved stability whereby polymerization of the amide is inhibited.Type: ApplicationFiled: November 4, 2002Publication date: May 8, 2003Applicant: Mitsui Chemicals, Inc.Inventors: Takeya Abe, Kenju Sasaki
-
Patent number: 6555187Abstract: Provided is a liquid crystal sealant composition in which an aqueous solution obtained by admixing the epoxy resin composition with purified water has an ionic conductivity of 1 mS/m or less; the B stage-reduced product has a viscosity of 50 to 10000 Pa·s at 80 to 100° C.; the cured matter of the above composition has a linear expansion coefficient of 10×10−5 mm/mm/° C. or less and a glass transition temperature Tg of 100° C. or higher; and the above cured matter has a moisture permeability of 200 g/m2·24 hours or less at 80° C. and which can meet a liquid crystal display element (cell) produced by a single layer press hot bonding system and exhibits high adhesion reliability and makes it possible to produce a homogeneous liquid crystal display element having a high quality.Type: GrantFiled: November 30, 2000Date of Patent: April 29, 2003Assignee: Mitsui Chemicals, Inc.Inventor: Tadashi Kitamura
-
Patent number: 6555645Abstract: The invention is a degradable polyurethane resin obtained by reacting 2,5-/2,6-diisocyanatomethylbicyclo[2.2.1]heptane and/or a modified compound thereof with polyol comprising a single compound, mixture or copolycondensate selected from the group consisting of (A) polyhydroxycarboxylate polyol, (B) aliphatic polyester polyol and (C) saccharides, or (D) straight or branched polyol formed by condensation of (A) and/or (B) with aliphatic polyhydric alcohol having functionality of three or more, and the polyurethane resin has hydralyzability and biodegradability, is excellent in rigidity and elasticity in combination with flexibility as compared with conventionally known biodegradable resin, and can provide formed articles having outstandingly high elasticity and elongation and other unprecedented properties.Type: GrantFiled: May 9, 2001Date of Patent: April 29, 2003Assignee: Mitsui Chemicals, Inc.Inventors: Kan Ikeda, Hiroaki Matsuno, Naoki Sato