Abstract: A polyurethane foam may include a base polyol component, a phosphorous polyol component, an expandable graphite, and melamine. The polyurethane foam may have a VO rating based on a UL94 flame retardancy test performed at a polyurethane foam thickness of 3.5 mm and a polyurethane foam density of 380 kg/m3.
Abstract: A base polyamide composition comprising a nylon mixture having caprolactam units from 1 wppb to 50 wppm catalyst composition; and greater than 0.75 wt % residual caprolactam, wherein the base polyamide composition has a delta end group level ranging from 30 ?eq/gram to 90 ?eq/gram.
Abstract: A liquefier tube for an additive manufacturing system, the liquefier tube including a body provided with a feed channel including a feeding portion having a first diameter, an outlet portion having a second diameter, the first diameter being larger than the second diameter, a transitional portion interconnecting the feeding portion and the outlet portion. The transitional portion has a monotonically decreasing third diameter from the feeding portion to the outlet portion and the third diameter as function of a longitudinal position of the feed channel in the transitional portion between the feeding portion and the outlet portion and at a transition between the transitional portion and the outlet portion is differentiable. Methods of manufacturing the liquefier tube.
Type:
Grant
Filed:
October 2, 2019
Date of Patent:
December 26, 2023
Assignee:
BOND HIGH PERFORMANCE 3D TECHNOLOGY B.V.
Inventors:
Adrianus Bruggeman, Marald Speelman, Klaas Groen, Martijn Johannes Wolbers, Koendert Hendrik Kuit, Antonie Everhard Ekkelenkamp
Abstract: The present disclosure relates to a low friction bearing liner for a solenoid may include a low friction layer. The low friction layer may include a first fluoropolymer matrix component and a first thermoplastic filler component distributed throughout the first fluoropolymer matrix component. The content of the first fluoropolymer matrix component may be at least about 1 wt. % and not greater than about 99 wt. % for a total weight of the first low friction layer. The content of the first thermoplastic filler component may be at least about 1 wt. % and not greater than about 99 wt. % for a total weight of the first low friction layer.
Abstract: An erosion control system is disclosed for preventing erosion of embankments including a three-dimensional material, the three-dimensional material including void volumes, and a mixture including a particulate material and a binder material included in the void volumes, wherein the binder material includes an organic binder material derived from living matter.
Type:
Application
Filed:
October 27, 2021
Publication date:
December 21, 2023
Applicant:
FREUDENBERG PERFORMANCE MATERIALS B.V.
Inventors:
Rijk GERRITSEN, Kennard VAN MALENSTEIN, Erik-Jan KOLLEN, Lucas BROUWERS
Abstract: An antistripping composition, comprising a first triamine compound or a second amine compound, and less than 1 wt % of a nitrile compound. When the antistripping composition is used in a bitumen composition, the bitumen composition demonstrates 50% or more retained coating as measured according to AASHTO T 283 (2022), and a tensile strength ratio of at least 80% when measured according to ASTM D 3625 (2020).
Abstract: A tunnel tube cooking pot that substantially improves thermal absorption of an aluminum boiling pot by welding specially designed and tuned pieces of aluminum channel or tubing on the bottom of the pot.
Abstract: A connection includes: a first profile having a first end, the first profile including a first polymeric material comprising a thermoset material; and a second profile having a second end, the second profile including a second polymeric material, a metal, or combination thereof, wherein the first end and the second end are coincidently bonded without a bonding material at an interface of the first end and the second end.
Abstract: A composite film may include a first transparent substrate and a first anti-reflective coating overlying a first surface of the first transparent substrate. The first anti-reflective coating may include a first UV curable acrylate binder, a photo initiator component, and silica nanoparticles dispersed within the first anti-reflective coating. The first anti-reflective coating may further include a ratio AC1SiO2/AC1B of at least about 0.01 and not greater than about 1.3. The composite film may further have a VLT of at least about 93.0% and a haze value of not greater than about 3%.
Abstract: A multi-purpose case that holds a portable computing device and an interchangeable thermoregulation element such that the thermoregulation element can be replaced without removing (or moving) the portable computing device. The case has modular components and can be attached to a light shield and or a document holder.
Abstract: A joint assembly including a housing including an inner diameter portion having a tapered surface; and at least one shaft having an outer diameter portion having a tapered surface that is complementary in shape to the inner diameter portion of the housing, where the shaft is adapted to rotate relative to the housing, and where the frictional fit is adjustable by modifying the axial position of the shaft relative to the housing.
Abstract: The present disclosure relates to a multilayer tube that may include an inner layer and an outer layer. The inner layer may include a fluoroether elastomer and the outer layer may include a non-fluoroether based elastomer. The multilayer tube may further include an adhesion force between the inner layer and the outer layer of at least about 1 ppi.
Abstract: The present invention is directed to tack solutions comprising formic acid, and their use in applying adhesive-coated films to substrates. In particular, paint protection films (PPFs) can be applied to vehicle bodies using the solutions of the present invention.
Abstract: A bearing including a substrate layer including an aluminum alloy including a thickness, TS, where TS?0.6 mm; an adhesive layer; and a low friction material layer overlying the adhesive layer, where the bearing includes an elongation at break, A50, of ?23%.
Abstract: The disclosure concerns a coupling assembly comprising at least first coupler, a second coupler, locators which assist in properly aligning the couplers, and hardware to hold the two couplers together. The coupling assembly may have more than one coupler. One end of each coupler is configured to attach to an assembly member. Another end of each coupler is configured with a coupling mechanism such that it may be coupled to the coupling mechanism of another coupler. The interior side of each coupling mechanism may have one or more recesses called locator pockets. The locator pockets on one coupler are configured to line up with the locator pockets on another coupler. As the first and second couplers are brought into an aligned position, a locator may be placed into the void created by each aligned locator pocket pair. After the locators are inserted and the couplers are brought into approximate alignment, the user may insert bolts through the couplers and apply nuts to the bolts.