CHIP ON FILM PACKAGE

A chip on film package includes a base film, a patterned circuit layer, a solder resist layer, a chip and a graphite sheet. The base film includes a first surface and a mounting region located on the first surface. The patterned circuit layer is disposed on the first surface. The solder resist layer partially covers the patterned circuit layer. The chip is disposed on the mounting region and electrically connected to the patterned circuit layer. The graphite sheet covers at least a part of the solder resist layer, wherein an outer edge of the graphite sheet is substantially aligned with an outer edge of the solder resist layer.

Skip to: Description  ·  Claims  · Patent History  ·  Patent History
Description
CROSS-REFERENCE TO RELATED APPLICATION

This application claims the priority benefit of U.S. provisional application Ser. No. 62/468,340, filed on Mar. 7, 2017. The entirety of the above-mentioned patent application is hereby incorporated by reference herein and made a part of this specification.

BACKGROUND Technical Field

The present disclosure generally relates to a chip package. More particularly, the present disclosure relates to a chip on film package.

Description of Related Art

In semiconductor production, the manufacturing of integrated circuits (IC) can be divided into three different stages, namely, a wafer fabrication stage, an integrated circuit fabrication stage and an IC packaging stage such as applying a chip-on-film (COF) package.

To increase the dissipation of heat from a chip of a COF package, a heat dissipation sheet is normally attached to a top surface of the base film to cover the whole chip or attached to a bottom surface of the base film opposite to the chip using thermal conductive glue after the chip is electrically connected to the film via bumps. Conventionally, during the process of attaching the heat dissipation sheet on the film for covering the chip, it is hard to make the heat dissipation sheet and the chip tightly attached together, so air gap usually exists between the chip and the heat dissipation sheet. As such, the air trapped between the chip and the heat dissipation sheet would expand during the subsequent thermal process, which may cause the heat dissipation sheet separating from the chip and reduce the reliability of the chip package. Moreover, since the heat conductivity of air is rather low, the air trapped in the space between the chip and the heat dissipation sheet would also affect the efficiency for heat generated from the chip to be conducted to the heat dissipation sheet.

SUMMARY

Accordingly, the present disclosure is directed to a chip on film package with favourable heat dissipation efficiency.

The present disclosure provides a chip on film package includes a base film, a patterned circuit layer, a solder resist layer, a chip and a graphite sheet. The base film includes a first surface and a mounting region located on the first surface. The patterned circuit layer is disposed on the first surface. The solder resist layer partially covers the patterned circuit layer. The chip is disposed on the mounting region and electrically connected to the patterned circuit layer. The graphite sheet covers at least a part of the solder resist layer, wherein an outer edge of the graphite sheet is substantially aligned with an outer edge of the solder resist layer.

According to an embodiment of the present disclosure, the graphite sheet further includes an opening exposing at least a part of the chip.

According to an embodiment of the present disclosure, the opening completely exposes an upper surface and four side surfaces of the chip.

According to an embodiment of the present disclosure, the graphite sheet covers at least part of an upper surface of the chip and the opening completely exposes two side surfaces of the chip.

According to an embodiment of the present disclosure, the opening exposes at least a part of a plurality of side surfaces of the chip.

According to an embodiment of the present disclosure, the opening exposes at least a part of two short side surfaces of the chip.

According to an embodiment of the present disclosure, the opening completely exposes two short side surfaces of the chip.

According to an embodiment of the present disclosure, the opening exposes at least a part of two long side surfaces of the chip.

According to an embodiment of the present disclosure, the opening completely exposes two long side surfaces of the chip.

According to an embodiment of the present disclosure, the opening exposes a part of an upper surface of the chip.

According to an embodiment of the present disclosure, the graphite sheet layer completely covers an upper surface of the chip.

According to an embodiment of the present disclosure, the opening completely exposes an upper surface of the chip.

According to an embodiment of the present disclosure, a distance between the outer edge of the graphite sheet and the outer edge of the solder resist layer is equal to or smaller than 1 mm.

According to an embodiment of the present disclosure, the patterned circuit layer is extended to the mounting region and the solder resist layer exposes a part of the patterned circuit layer extended to the mounting region.

According to an embodiment of the present disclosure, the chip is mounted on the part of the patterned circuit layer extended to the mounting region.

According to an embodiment of the present disclosure, the opening of the graphite sheet exposes the part of the patterned circuit layer extended to the mounting region.

According to an embodiment of the present disclosure, the chip on film package further including an underfill filled between the chip and the base film, and the opening exposing the underfill.

According to an embodiment of the present disclosure, the opening exposes a whole of the upper surface of the chip and a gap exists between the opening and a side surface of the chip.

According to an embodiment of the present disclosure, a width of the gap is equal to or longer than 2 mm.

According to an embodiment of the present disclosure, a thickness of the graphite sheet substantially ranges from 17 μm to 20 μm.

According to an embodiment of the present disclosure, the chip on film package further includes an adhesive layer disposed on an attaching surface of the graphite sheet, and the attaching surface is a surface attached to the solder resist layer by the adhesive layer.

According to an embodiment of the present disclosure, the chip on film package further including a back graphite sheet disposed on a second surface of the base film opposite to the first surface of the base film.

According to an embodiment of the present disclosure, the back graphite sheet is overlapped with at least the mounting region along a normal direction of the base film.

According to an embodiment of the present disclosure, an outer edge of the back graphite sheet is substantially aligned with the outer edge of the solder resist layer.

The present disclosure provides a manufacturing method of a chip on film package including the following steps. A graphite roll is provided, wherein the graphite roll includes a plurality of graphite sheets and a release film, the graphite sheets attached on the release film and each of the graphite sheets includes an opening. The graphite roll is unwound and one of graphite sheets on an unwounded part of the graphite roll is picked up from the release film. The one of the graphite sheets is placed and laminated on a base film, wherein the base film includes a chip mounted thereon and the opening of the one of the graphite sheets exposes the chip.

According to an embodiment of the present disclosure, the one of the graphite sheets is laminated on the base film by a laminating head.

According to an embodiment of the present disclosure, the laminating head is a flexible laminating head.

According to an embodiment of the present disclosure, the laminating head includes a cavity, when the laminating head presses the one of the graphite sheets onto the base film, the chip is located in the cavity.

According to an embodiment of the present disclosure, a gap maintains between the cavity and a side surface of the chip.

According to an embodiment of the present disclosure, a shortest distance from the cavity to a side surface of the chip is substantially 1 mm to 3 mm.

According to an embodiment of the present disclosure, each of the graphite sheets further includes an adhesive layer disposed on an attaching surface of the graphite sheet, and the release film covers the adhesive layer.

In light of the foregoing, the graphite sheet is attached to the chip on film package of the disclosure, wherein the graphite sheet exposes at least a part of the chip and an outer edge of the graphite sheet is aligned with an outer edge of the solder resist layer of the chip on film package. With such configuration, the contact area between the graphite sheet and the solder resist layer/the chip can be maximizing, so as to improve the heat dissipation of the chip on film package 100. Also, the air and/or moisture trapped between the chip and the graphite sheet can be easily discharged since the graphite sheet does not completely covers the chip, so the graphite sheet would not be deformed or even separated from the chip under high temperature and/or high humidity condition, so as to improve the reliability of the chip on film package.

In addition, a plurality of graphite sheets may be connected to one another via a release film to form a graphite roll. Accordingly, the graphite sheets with poor flexibility can be applied to a roll to roll manufacturing process, such that graphite sheets can be applied to chip on film packages for mass production. Therefore, heat dissipation of the chip on film package in the disclosure can be improved.

BRIEF DESCRIPTION OF THE DRAWINGS

The accompanying drawings are included to provide a further understanding of the disclosure, and are incorporated in and constitute a part of this specification. The drawings illustrate embodiments of the disclosure and, together with the description, serve to explain the principles of the disclosure.

FIG. 1 illustrates a cross-sectional view of a chip on film package according to an embodiment of the disclosure.

FIG. 2 illustrates a top view of a chip on film package according to an embodiment of the disclosure.

FIG. 3 illustrates a cross-sectional view of a graphite sheet according to an embodiment of the disclosure.

FIG. 4 illustrates a top view of a chip on film package according to an embodiment of the disclosure.

FIG. 5 illustrates a cross-sectional view of a chip on film package according to an embodiment of the disclosure.

FIG. 6 illustrates a schematic view of a chip on film package according to an embodiment of the disclosure.

FIG. 7A to FIG. 7C illustrate a part of a manufacturing process of a chip on film packages according to embodiments of the disclosure.

FIG. 8 illustrates an elevation view of a fixture attaching a graphite sheet onto a chip on film package according to an embodiment of the disclosure.

DESCRIPTION OF THE EMBODIMENTS

Reference will now be made in detail to the present preferred embodiments of the disclosure, examples of which are illustrated in the accompanying drawings. Wherever possible, the same reference numbers are used in the drawings and the description to refer to the same or like parts.

FIG. 1 illustrates a cross-sectional view of a chip on film package according to an embodiment of the disclosure. FIG. 2 illustrates a top view of a chip on film package according to an embodiment of the disclosure. It is noted that FIG. 1 is the cross-sectional view of FIG. 2 along line A-A′. Referring to FIG. 1 and FIG. 2, in the present embodiment, a chip on film package 100 includes a base film 110, a patterned circuit layer 118, a solder resist layer 119, a chip 120 and a graphite sheet 130. The base film 110 includes a first surface 112. A mounting region R1 is where the chip 120 is mounted and is located on the first surface 112. The patterned circuit layer 118 is disposed on the first surface 112 of the base film 110. The solder resist layer 119 partially covers the patterned circuit layer 118. The chip 120 is disposed in the mounting region R1 and electrically connected to the patterned circuit layer 118.

In more detail, for example, as shown in the present embodiment, the solder resist layer 119 covers the patterned circuit layer 118 and exposes a part of the patterned circuit layer 118, such that the chip 120 is electrically connected to the part of the patterned circuit layer 118 exposed by the solder resist layer 119. In the present embodiment, the patterned circuit layer 118 is extended to the mounting region R1 and the solder resist layer 119 exposes a part of the patterned circuit layer 118 extended to the mounting region R1 as shown in FIG. 1. The chip 120 is mounted on the part of the patterned circuit layer 118 extended to the mounting region R1.

Moreover, the graphite sheet 130 covers at least a part of the solder resist layer 119. Advantageously, the graphite sheet 130 may have a soft texture and good thermal conductivity, allowing the area of heat dissipation to be increased and therefore leading to an improved heat dissipation effect. Preferably but not limitedly, an outer edge E1/E2 of the graphite sheet 130 can be arranged to be substantially aligned with an outer edge of the solder resist layer 119. For example, a distance between the outer edge E1/E2 of the graphite sheet 130 and the outer edge of the solder resist layer 119 is equal to or smaller than 1 mm.

In some implementations as shown in the present embodiment, the graphite sheet 130 may include a plurality of alignment holes H1 for aligning the outer edge E1/E2 of the graphite sheet 130 with the outer edge of the solder resist layer 119. The alignment holes H1 can be any shape according to desired or required of designs. Preferably but not limitedly, the sizes of the holes H1 may be arranged to be smaller than 3 mm to maximize the heat dissipation effect of the graphite sheet 130.

In the present embodiment, after the packaging process is done, the package structure may be cut along a plurality of cutting lines, which may be aligned with the outer edge E1/E2 of the solder resist layer 119, to form a plurality of chip on film packages 100. With the arrangement of the outer edge E1/E2 of the graphite sheet 130 being aligned with the outer edge of the solder resist layer 119, the contact area between the graphite sheet 130 and the solder resist layer 119/the chip 120 can be maximized, which can improve the heat dissipation of the chip on film package 100.

In general, if the heat-dissipation layer covers the chip completely, the heat-dissipation layer might deform or even separate from the chip under high temperature and/or high humidity condition due to the expansion of the air and/or moisture trapped between the chip and the heat-dissipation layer. As such, in some implementations as shown in the present embodiment, the graphite sheet 130 may further include one or more openings OP1 exposing at least a part of the chip 120 and the part of the patterned circuit layer 118 extended to the mounting region R1. With such a configuration, the air and/or moisture trapped between the chip 120 and the graphite sheet 130 may be more easily discharged through the opening OP1, so as to avoid unwanted deformation or separation of the graphite sheet 130. Thereby, the reliability of the chip on film package 100 can be improved.

In the present embodiment, the opening OP1 may completely expose an upper surface and a plurality of side surfaces of the chip 120 as shown in FIG. 1 and FIG. 2, but the disclosure is not limited thereto. In addition, the chip on film package 100 may further include an underfill 150 filled between the chip 120 and the base film 110. The underfill 150 may be further filled between a side surface of the chip 120 and a side surface of the graphite sheet 130 exposed by the opening OP1 as shown in FIG. 1. In the present embodiment, one or more gap G1/G2 exist between a side surface of the graphite sheet 130/the opening OP1 and a side surface of the chip 120. For example, the gap G1 may exist between a side surface of the graphite sheet 130/the opening OP1 and a short side surface of the chip 120, and the gap G2 may exist between another side surface of the graphite sheet 130/the opening OP1 and a long side surface of the chip 120 as shown in FIG. 2. Preferably but not limitedly, a width of the gap G1/G2 can be arranged to be substantially equal to or longer than 2 mm. Moreover, it is noted that the width of the gap G1 may be substantially the same as or different from the width of the gap G2.

It is noted that in the present embodiment, the graphite sheet 130 exposes an upper surface and a plurality of side surfaces (e.g. four side surfaces)_of the chip 120, which means that none of the upper surface and the side surfaces of the chip 120 is completely covered, but the disclosure is not limited thereto. For example, in some other embodiments, the graphite sheet 130 partially or completely covers the upper surface of the chip, while completely exposes the side surfaces of the chip 120. Moreover, in some other embodiments, the graphite sheet 130 partially or completely covers the upper surface of the chip and two short/long side surfaces, while completely exposes two long/short side surfaces of the chip 120. Furthermore, in some yet other embodiments, the graphite sheet 130 completely or partially covers each of an upper surface and the side surfaces of the chip 120, which means that none of the upper surface and the side surfaces of the chip 120 is completely exposed. More other different combinations of exposure or coverage of the graphite sheet on the upper surface and side surfaces of the chip 120 can be implemented as required and is not limited in the disclosure.

In some embodiments, the chip on film package 100 further includes an adhesive layer 138 disposed on an attaching surface of the graphite sheet 130, wherein the attaching surface is a surface of the graphite sheet 130 attached to the solder resist layer 119 by the adhesive layer 138. FIG. 3 illustrates a cross-sectional view of a graphite sheet according to such an embodiment of the disclosure. In detail, the graphite sheet 130 may include a graphite layer 132, a first adhesive layer 134, a second adhesive layer 138 and a protection layer 136 as shown in FIG. 3. In addition, the structure shown in FIG. 3 can be applied to FIG. 1 or other embodiments in the disclosure but not limited thereto. The graphite layer 132 is attached to the base film 110 and the chip 120 by the first adhesive layer 134. The protection layer 136 is attached to the graphite layer 132 by the second adhesive layer 138. Preferably but not limitedly, the first adhesive layer 134 may be an organic double coated tape, the second adhesive layer 138 may be an inorganic double coated tape, the protection layer 136 may include an insulating film such as a polyimide (PI) film, but the embodiment is merely for illustration and the disclosure does not limit the materials of the the first adhesive layer 134, the second adhesive layer 138 and the protection layer 136. In some implementations, a thickness T1 of the graphite sheet 130 may substantially range from 17 μm to 20 μm but not limited thereto.

In some implementations as exemplarily shown in the embodiment of FIG. 1, the chip on film package 100 further includes a back graphite sheet 140 disposed on a second surface 114 of the base film 110 opposite to the first surface 112 of the base film 110. The back graphite sheet 140 is overlapped with at least the mounting region R1 along a normal direction of the base film 110. The back graphite sheet 140 may also include a graphite layer 142, a first adhesive layer 144, a second adhesive layer 148 and a protection layer 146 as shown in FIG. 1. The graphite layer 142 is attached to the second surface 114 of the base film 110 by the first adhesive layer 144. The protection layer 146 is attached to the graphite layer 142 by the second adhesive layer 148. Advantageously, an outer edge of the back graphite sheet 140 can be arranged to be substantially aligned with the outer edge of the solder resist layer 119, so as to maximizing the contact area between the back graphite sheet 140 and the base film 110, and further enhance the heat dissipation of the chip on film package 100.

FIG. 4 illustrates a top view of a chip on film package according to an embodiment of the disclosure. FIG. 5 illustrates a cross-sectional view of a chip on film package according to an embodiment of the disclosure. It is noted that FIG. 4 is the cross-sectional view of FIG. 5 along line B-B′, and the chip on film package shown in FIG. 4 and FIG. 5 contains many features same as or similar to the chip on film package 100 disclosed earlier with FIG. 1 to FIG. 3. For purpose of clarity and simplicity, detail description of same or similar features may be omitted, and the same or similar reference numbers denote the same or like components. The main differences between the chip on film package shown in FIG. 4 and FIG. 5 and the chip on film package 100 shown in FIG. 1 to FIG. 3 are described as follows.

Referring to FIG. 4 and FIG. 5, the graphite sheet 130 covers at least part of an upper surface of the chip 120 and the opening OP1 exposes at least a part of the side surfaces of the chip 120. In detail, the opening OP1 may expose at least a part of two short side surfaces of the chip 120. In the present embodiment, the opening OP1 completely exposes the two short side surfaces of the chip 120. It is noted that the so-called “short side surfaces of the chip 120” means the two side surfaces parallel to the short axis (e.g. axis A2 in FIG. 4) of the chip 120.

In detail, the chip 120 has a chip length L1 along a first axis A1 of the chip 120. A part of the graphite sheet 130 with the opening OP1 has a length L2 along the first axis A1, and another part of the graphite sheet 130 without the opening OP1 has a length L3 along the first axis A1. As such, the length L3 is substantially longer than the length L2, and the length L2 is substantially longer than the length L1. Accordingly, the opening OP1 exposes a part of an upper surface of the chip 120 and the opening OP1 exposes the two short side surfaces of the chip 120 as shown in FIG. 4.

FIG. 6 illustrates a schematic view of a chip on film package according to an embodiment of the disclosure. It is noted that the chip on film package shown in FIG. 6 contains many features same as or similar to the chip on film package 100 in the previous embodiments. For purpose of clarity and simplicity, detail description of same or similar features may be omitted, and the same or similar reference numbers denote the same or like components. The main differences between the chip on film package shown in FIG. 6 and the chip on film package 100 in the previous embodiments are described as follows.

Referring to FIG. 6, the graphite sheet 130 may completely cover the upper surface of the chip 120 and the opening OP1 exposes at least a part of the side surfaces of the chip 120. In detail, the opening OP1 may expose at least a part of two long side surfaces of the chip 120. In the present embodiment, the opening OP1 completely exposes the two long side surfaces of the chip 120. It is noted that the so-called “long side surfaces of the chip 120” means the two side surfaces parallel to the long axis (e.g. axis A1 in FIG. 4) of the chip 120.

FIG. 7A to FIG. 7C illustrate a part of a manufacturing process of a chip on film packages according to embodiments of the disclosure. FIG. 8 illustrates an elevation view of a fixture attaching a graphite sheet onto a chip on film package according to an embodiment of the disclosure. In the present embodiment, the chip on film package 100 may be formed by a manufacturing method including the following steps. First of all, a graphite roll 130a as shown in FIG. 7A and FIG. 7B is provided. The graphite roll 130a includes a plurality of graphite sheets 130 and a release film 131. The graphite sheets 130 are attached on the release film 131 and each of the graphite sheets 130 includes the opening OP1. In detail, each of the graphite sheets 130 may be similar to the graphite sheet 130 shown in FIG. 3 and further include an adhesive layer (e.g. the second adhesive layer 138 shown in FIG. 3) disposed on the attaching surface of the graphite sheet 130. The release film 131 covers the adhesive layer of the graphite sheets 130.

With such a configuration, the graphite sheets 130 can be connected to each other via the release film 131 to form a graphite sheet belt and the graphite sheet belt can be rolled up to form the graphite roll 130a. Accordingly, the graphite sheets 130 with poor flexibility can be applied to a roll to roll process, so as to be suitable for mass production. Then, the graphite roll 130a is unwound as shown in FIG. 7B, and one of graphite sheets 130 on an unwounded part of the graphite roll 130a may be picked up from the release film 131.

Then, referring to FIG. 7C and FIG. 8, the picked graphite sheet 130 is placed and laminated on a base film 110 by a laminating head 700. In some implementations, a plurality of base films 110 with chips 120 mounted thereon may also be connected to one another and rolled up as a base film roll. The base film roll is then unwound and transmitted along a first direction D1, and the graphite roll 130a with a plurality of graphite sheets 130 is unwound and transmitted along a second direction D2. The first direction D1 and the second direction D2 may be intersected with each other. Accordingly, one of the graphite sheet 130 is placed and laminated on the corresponding base film 110 by the laminating head 700, and the opening (e.g. the opening OPI shown in FIG. 2) of the corresponding graphite sheet 130 exposes the chip 120 on the corresponding base film 110.

In the present embodiment, the laminating head 700 is a flexible laminating head to avoid unwanted damages to the chip on film package 100. In detail, the laminating head 700 may include a cavity as shown in FIG. 8. Accordingly, when the laminating head 700 presses the graphite sheet 130 onto the base film 110, the chip 120 is located in the cavity without being pressed and damaged. A gap may maintain between the cavity and a side surface of the chip 120 to further prevent the laminating head 700 from damaging the chip 120, and a shortest distance from the cavity to a side surface of the chip 120 is substantially 1 mm to 3 mm.

In sum, in the embodiments of the disclosure, a graphite sheet can be utilized for heat dissipation. The graphite sheet can have good thermal conductivity and hence leads to an enhanced heat dissipation effect. In addition, an outer edge of the graphite sheet can be aligned with an outer edge of the solder resist layer of the chip on film package to maximize coverage of the graphite sheet and hence heat dissipation effect. With such an arrangement, the contact area between the graphite sheet and the solder resist layer/the chip can be maximized, so as to improve the heat dissipation of the chip on film package. Moreover, the graphite sheet can include an opening for exposing at least a part of the chip. The air and/or moisture trapped between the chip and the graphite sheet can be easily discharged through the opening, so the graphite sheet would not be deformed or even separated from the chip under high temperature and/or high humidity condition, so as to improve the reliability of the chip on film package.

Furthermore, in manufacturing processes, a plurality of graphite sheets may be connected to one another via a release film to form a graphite roll. Accordingly, the graphite sheets with poor flexibility can be applied to a roll to roll manufacturing process, such that graphite sheets can be applied to chip on film packages for mass production. Therefore, heat dissipation of the chip on film package in the disclosure can be improved.

It will be apparent to those skilled in the art that various modifications and variations can be made to the structure of the present disclosure without departing from the scope or spirit of the disclosure. In view of the foregoing, it is intended that the present disclosure cover modifications and variations of this disclosure provided they fall within the scope of the following claims and their equivalents.

Claims

1. A chip on film package, comprising:

a base film comprising a first surface and a mounting region located on the first surface;
a patterned circuit layer disposed on the first surface;
a solder resist layer partially covering the patterned circuit layer;
a chip disposed on the mounting region and electrically connected to the patterned circuit layer; and
a graphite sheet covering at least a part of the solder resist layer and comprising an opening exposing at least a part of the chip, wherein an outer edge of the graphite sheet is substantially aligned with an outer edge of the solder resist layer.

2. (canceled)

3. The chip on film package as claimed in claim 1, wherein the opening completely exposes an upper surface and a plurality of side surfaces of the chip.

4. The chip on film package as claimed in claim 1, wherein the graphite sheet covers at least a part of an upper surface of the chip and the opening completely exposes two side surfaces of the chip.

5. The chip on film package as claimed in claim 1, wherein the opening exposes at least a part of a plurality of side surfaces of the chip.

6. The chip on film package as claimed in claim 5, wherein the opening exposes at least a part of two short side surfaces of the chip.

7. The chip on film package as claimed in claim 5, wherein the opening completely exposes two short side surfaces of the chip.

8. The chip on film package as claimed in claim 5, wherein the opening exposes at least a part of two long side surfaces of the chip.

9. The chip on film package as claimed in claim 5, wherein the opening completely exposes two long side surfaces of the chip.

10. The chip on film package as claimed in claim 1, wherein the opening exposes a part of an upper surface of the chip.

11. The chip on film package as claimed in claim 1, wherein the graphite sheet layer completely covers an upper surface of the chip.

12. The chip on film package as claimed in claim 1, wherein the opening completely exposes an upper surface of the chip.

13. The chip on film package as claimed in claim 1, wherein a distance between the outer edge of the graphite sheet and the outer edge of the solder resist layer is equal to or smaller than 1 mm.

14. The chip on film package as claimed in claim 1, wherein the patterned circuit layer is extended to the mounting region and the solder resist layer exposes a part of the patterned circuit layer extended to the mounting region.

15. The chip on film package as claimed in claim 14, wherein the chip is mounted on the part of the patterned circuit layer extended to the mounting region.

16. The chip on film package as claimed in claim 14, wherein the opening of the graphite sheet exposes the part of the patterned circuit layer extended to the mounting region.

17. The chip on film package as claimed in claim 1, further comprising an underfill filled between the chip and the base film, and the opening exposing the underfill.

18. The chip on film package as claimed in claim 1, wherein the opening exposes a whole of the upper surface of the chip and a gap exists between the opening and a side surface of the chip.

19. The chip on film package as claimed in claim 18, wherein a width of the gap is equal to or longer than 2 mm.

20. The chip on film package as claimed in claim 1, wherein a thickness of the graphite sheet substantially ranges from 17 μm to 20 μm.

21. The chip on film package as claimed in claim 1, further comprises an adhesive layer disposed on an attaching surface of the graphite sheet, and the attaching surface is a surface attached to the solder resist layer by the adhesive layer.

22. The chip on film package as claimed in claim 1, further comprising a back graphite sheet disposed on a second surface of the base film opposite to the first surface of the base film.

23. The chip on film package as claimed in claim 22, wherein the back graphite sheet is overlapped with at least the mounting region along a normal direction of the base film.

24. The chip on film package as claimed in claim 22, wherein an outer edge of the back graphite sheet is substantially aligned with the outer edge of the solder resist layer.

25. A manufacturing method of a chip on film package, comprising:

providing a graphite roll, wherein the graphite roll comprises a plurality of graphite sheets and a release film, the graphite sheets attached on the release film and each of the graphite sheets comprises an opening;
unwinding the graphite roll and picking up one of graphite sheets on an unwounded part of the graphite roll from the release film; and
placing and laminating the one of the graphite sheets on a base film, wherein the base film comprises a chip mounted thereon and the opening of the one of the graphite sheets exposes the chip.

26. The manufacturing method of a chip on film package as claimed in claim 25, wherein the one of the graphite sheets is laminated on the base film by a laminating head.

27. The manufacturing method of a chip on film package as claimed in claim 26, wherein the laminating head is a flexible laminating head.

28. The manufacturing method of a chip on film package as claimed in claim 26, wherein the laminating head comprises a cavity, when the laminating head presses the one of the graphite sheets onto the base film, the chip is located in the cavity.

29. The manufacturing method of a chip on film package as claimed in claim 28, wherein a gap maintains between the cavity and a side surface of the chip.

30. The manufacturing method of a chip on film package as claimed in claim 28, wherein a shortest distance from the cavity to a side surface of the chip is substantially 1 mm to 3 mm.

31. The manufacturing method of a chip on film package as claimed in claim 25, wherein each of the graphite sheets further comprises an adhesive layer disposed on an attaching surface of the graphite sheet, and the release film covers the adhesive layer.

32. A chip on film package, comprising:

a base film comprising a first surface and a mounting region located on the first surface;
a patterned circuit layer disposed on the first surface, wherein the patterned circuit layer is extended to the mounting region;
a solder resist layer partially covering the patterned circuit layer and exposing a part of the patterned circuit layer extended to the mounting region;
a chip disposed on the mounting region and electrically connected to the patterned circuit layer; and
a graphite sheet covering at least a part of the solder resist layer, wherein an outer edge of the graphite sheet is substantially aligned with an outer edge of the solder resist layer.

33. A chip on film package, comprising:

a base film comprising a first surface and a mounting region located on the first surface;
a patterned circuit layer disposed on the first surface;
a solder resist layer partially covering the patterned circuit layer;
a chip disposed on the mounting region and electrically connected to the patterned circuit layer;
a graphite sheet covering at least a part of the solder resist layer, wherein an outer edge of the graphite sheet is substantially aligned with an outer edge of the solder resist layer; and
an underfill filled between the chip and the base film, wherein the opening exposes the underfill.
Patent History
Publication number: 20180261523
Type: Application
Filed: Jun 5, 2017
Publication Date: Sep 13, 2018
Applicant: Novatek Microelectronics Corp. (Hsinchu)
Inventors: Wen-Ching Huang (Hsinchu City), Chien-Chen Ko (Hsinchu City)
Application Number: 15/613,275
Classifications
International Classification: H01L 23/373 (20060101); H01L 23/498 (20060101); H01L 23/31 (20060101); H01L 23/00 (20060101); H01L 23/367 (20060101); H01L 21/48 (20060101); B32B 9/00 (20060101); B32B 7/12 (20060101); B32B 37/14 (20060101); B32B 37/12 (20060101);